Technology of the high temperature diffusive brazing of a bimetallic «blisk» design

Ospennikova O.G., Lukin V.I., Afanasiev-Khodykin A.N., Galushka I.A.
Ospennikova O.G., Lukin V.I., Afanasiev-Khodykin A.N., Galushka I.A. Technology of the high temperature diffusive brazing of a bimetallic «blisk» design // Proceedings of VIAM. 2019. No. 9. DOI: 10.18577/2307-6046-2019-0-9-26-37. URL: https://www.viam-works.ru/en/journal/2019/9/3
Keywords
brazing, a high-temperature diffusion brazing, nickel-based superalloys
Abstract

The article presents the results of the development a manufacturing technology for the construction type «blisk» design constructed with a permanent joint with the method of a high-temperature diffusion brazing. The brazing alloy for brazing nickel-based superalloys in bimetallic combinations, that provide a long-term strength of the brazing joint at the level of strength 0,8–0,9 from the least durable of the materials was developed. The influence of heat treatment on microstructure and strength of the brazing joint was investigated. The technology of brazing bimetallic nickel-based superalloys for «blisk» design was developed. Test of a bimetallic specimen of a «blisk» design demonstrator was carried out.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Inozemtsev A.A., Nikhamkin M.A., Sandratskiy V.L. Gazoturbinnyye dvigateli. Osnovy konstruirovaniya aviatsionnykh dvigateley i energeticheskikh ustanovok [Gas turbine engines. Fundamentals of designing aircraft engines and power plants]. M.: Mashinostroyeniye, 2007. T. 1: Obshchiye svedeniya. Osnovnyye parametry i trebovaniya. Konstruktivnyye i silovyye skhemy. S. 7–17.
  3. Babkin V.I., Tskhovrebov M.M., Solonin V.I., Lanshin A.I. Razvitiye aviatsionnykh GTD i sozdaniye unikal'nykh tekhnologiy [The development of aviation gas turbine engines and the creation of unique technologies] // Dvigatel. 2013. №2 (86). S. 2–7.
  4. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of a new generation – the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  5. Inozemtsev A.A., Nikhamkin M.A., Sandratskiy V.L. Gazoturbinnyye dvigateli. Osnovy konstruirovaniya aviatsionnykh dvigateley i energeticheskikh ustanovok [Gas turbine engines. Fundamentals of designing aircraft engines and power plants]. M.: Mashinostroyeniye, 2007. T. 2: Kompressory. Kamery sgoraniya. Forsazhnyye kamery. Turbiny. Vykhodnyye ustroystva. S. 259–272.
  6. Lunev A.N., Kurylev D.V. Obzor progressivnykh metodov izgotovleniya osevykh monokoles aviatsionnykh gazoturbinnykh dvigateley [A review of progressive manufacturing methods for axial monowheels of aircraft gas turbine engines] // Fundamentalnye issledovaniya. 2016. №6–1. S. 78–82. Available at: http://www.fundamental-research.ru/ru/article/view?id=40375 (accessed: June 18, 2019).
  7. Magerramova L.A., Vasilev B.E. Bimetallicheskiye bliski turbin s bandazhirovannymi lopatkami dlya gazoturbinnykh dvigateley [Bimetallic glare of turbines with bandaged blades for gas turbine engines] // Nauka i obrazovaniye: nauchnoye izdaniye MGTU im. N.E. Baumana. 2015. №6. S. 143–156.
  8. Yuan J., Scarpa F., Titurus B. et al. Efficient computational techniques for mistuning analysis of bladed discs: a review // Mechanical Systems and Signal Processing. 2017. Vol. 87. Part A. P. 71–90.
  9. Magerramova L., Zakharova T., Gromov M., Samarov V. Turbiny: s «blisk»om i bez [Turbines: with and without «blisk»]. Available at: http://engine.aviaport.ru/02page32.html (accessed: Septamber 05, 2019).
  10. Kablov E.N., Petrushin N.V., Elyutin E.S. Monokristallicheskiye zharoprochnyye splavy dlya gazoturbinnykh dvigateley [Monocrystalline heat-resistant alloys for gas turbine engines] // Vestnik MGTU im. N.E. Baumana. 2011. Spetsvypusk: Perspektivnyye konstruktsionnyye materialy i tekhnologii. S. 38–52.
  11. Povarova K.B., Valitov V.A., Ovsepyan S.V., Drozdov A.A., Bazyleva O.A., Valitova E.V. Izucheniye svoystv i vybor splavov dlya diskov s lopatkami («bliskov») i sposoba ikh soyedineniya [Studying the properties and selection of alloys for blades with blades («blisk») and the method of their connection] // Metally. 2014. №35. S. 61–70.
  12. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  13. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallidnyye splavy na osnove titana i nikelya / pod obshch. red. E.N. Kablova [Intermetallic alloys based on titanium and nickel / gen. ed. E.N. Kablov]. M.: VIAM, 2018. 308 s.
  14. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Liteynyye zharoprochnyye splavy novogo pokoleniya [Heat-resistant foundry alloys of a new generation] // 75 let. Aviatsionnyye materialy. M.: VIAM, 2007. S. 27–44.
  15. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. Primenenie novyh deformiruemyh nikelevyh splavov dlja perspektivnyh gazoturbinnyh dvigatelej [The application of new wrought nickel alloys for advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  16. Lukin V.I., Kovalchuk V.G., Ioda E.N. Svarka plavleniyem – osnova svarochnogo proizvodstva [Fusion welding is a core of welding manufacturing] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 130–143. DOI: 10.18577/2071-9140-2017-0-S-130-143.
  17. Ospennikova O.G., Lukin V.I., Afanasev-Khodykin A.N., Galushka I.A. Izgotovleniye konstruktsii tipa «blisk» iz raznoimennogo sochetaniya materialov (obzor) [Manufacturing of design of the «blisk» type from ranoimenny combingtion of materials (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №10 (70). St. 02. Available at: http://www.viam-works.ru (accessed: July 16, 2019). DOI: 10.18577/2307-6046-2018-0-10-10-16.
  18. Magerramova L.A. The advantages of bimetallic blisks manufactured by HIP from powder and cast Ni-base super alloys application to gas turbine with high speed // Proceedings of International Conference on Hot Isostatic Pressing, (HIP02). International Academic Publishers, 2002. P. 59–67.
  19. Ospennikova O.G., Lukin V.I., Afanasyev-Khodykin A.N., Galushka I.A., Shevchenko O.V. Perspektivnyye razrabotki v oblasti vysokotemperaturnoy payki zharoprochnykh splavov [Advanced developments in the field of the high-temperature soldering of heat resisting alloys] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 144–158. DOI: 10.18577/2071-9140-2017-0-S-144-158.
  20. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  21. Kishkin S.T., Kachanov E.B., Bulygin I.P. Aviacionnye materialy: spravochnik v 9 t. / pod red. R.E. Shalina. 6-e izd., pererab. i dop. [Aviation Materials: a handbook of 9 vol. / ed. R.E. Shalin. 6th ed., rev. and add.]. M.: VIAM, 1989. T. 3: Zharoprochnyye stali i splavy. Splavy na osnove tugoplavkikh metallov. Ch. 1 Deformiruyemyye zharoprochnyye stali i splavy. S. 448–452.
  22. Petrunin I.E., Bereznikov Yu.I., Bunkina R.R. i dr. Spravochnik po payke. 3-ye izd. pererab. i dop. [Soldering reference. 3rd ed. rev. and add.]. M.: Mashinostroyeniye-1, 2003. 480 s.
  23. Petrunin I.E., Markova I.Yu., Ekatova A.S. Metallovedeniye payki [Metallurgy soldering]. M.: Metallurgiya, 1976. 264 s.
  24. Khorunov V.F., Maksimova S.V. Payka zharoprochnykh splavov na sovremennom etape [Brazing of heat-resistant alloys at the present stage] // Svarochnoye proizvodstvo. 2010. №10. S. 24–27.