Particulars of the precipitation strengthening γʹ-phase during aging of heat-resistant wrought nickel superalloy VZh175-ID
UDC
544.344:621.762:669.245
DOI
10.18577/2307-6046-2019-0-9-3-14
Article PDF (Russian)
(1.18 MB)
How to cite
Kablov E.N., Letnikov M.N., Ospennikova O.G., Bakradze M.M., Shestakova A.A. Particulars of the precipitation strengthening γʹ-phase during aging of heat-resistant wrought nickel superalloy VZh175-ID // Proceedings of VIAM. 2019. No. 9. DOI: 10.18577/2307-6046-2019-0-9-3-14. URL: https://www.viam-works.ru/en/journal/2019/9/1
Keywords
Ni superalloy, gamma prime, aging, cooling rate, mechanical properties, alloy VZh175-ID.
Abstract
The effect of aging at various temperatures on the size, morphology of the strengthening particles of the γʹ-phase and the mechanical properties of the heat-resistant wrought nickel superalloy VZh175-ID was studied. It is shown that the hardening effect during aging at different temperatures varies and depends on the microstructure which formed in the alloy VZh175-ID superalloy at the quenching stage. The excellent tensile strength and strength to rupture is achieved when small spherical or cuboid secondary γʹ-phase and nanosized tertiary γʹ-phase are formed in the structure.
Reference list
- Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnyye napravleniya razvitiya tekhnologiy proizvodstva zharoprochnykh materialov dlya aviatsionnogo dvigatelestroyeniya [Priority areas for the development of technologies for the production of heat-resistant materials for aircraft engine building] // Problemy chernoy metallurgii i materialovedeniya. 2013. №3. S. 47–54.
- Kablov E.N. Materialy novogo pokoleniya [Generation Materials] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
- Kablov E.N., Alekseyev A.A. Fizika zharoprochnosti geterofaznykh splavov [Physics of heat resistance of heterophase alloys] // Liteynyye zharoprochnyye splavy. Effekt S.T. Kishkina. M.: Nauka, 2006. S. 44–55.
- Reed R.C. The Superalloys fundamentals and applications // Cambridge university press. 2006. P. 73–81.
- Kozar R.W., Suzuki A., Milligan W.W. et al. Strengthening Mechanisms in Polycrystalline Multimodal Nickel-Base Superalloys // Metallurgical and materials transactions A. 2009. Vol. 40. Issue 7. P. 1588–1603.
- Gabb T.P., Backman D.G., Wei D.Y. et al. yʹ formation in nickel-base disk superalloy // Superalloys-2000. The Minerals, Metals & Materials Society, 2000. P. 405–414.
- Jackson M.P., Reed R.C. Heat treatment of UDIMET 720Li: the effect of microstructure on properties // Materials Science and Engineering A. 1999. Vol. 259. P. 85–97.
- Groh J.R. Effect of cooling rate from solution heat treatment on Waspaloy microstructure and properties // Superalloys-1996. The Minerals, Metals & Materials Society, 1996. P. 621–626.
- Mao J., Chang K.M., Yang W. et al. Cooling precipitation and strengthening study in powder metallurgy superalloy Rene 88DT // Materials Science and Engineering. 2002. Vol. A332. P. 318–329.
- Bhowal P.R., Wright E.F., Raymond E.L. Effects of Cooling Rate and Morphology on Creep and Stress-Rupture Properties of a Powder Metallurgy Superalloy // Metallurgical Transactions A. 1990. Vol. 21A. Issue 6. P. 1709–1717.
- Mao J., Chang K.M., Yang W. et al. Cooling precipitation and strengthening study in powder metallurgy superalloy U720LI // Metallurgical and materials transaction A. 2001.Vol. 32. Issue 10. P. 2441–2452.
- Perrut M., Locq D. ʹ precipitation kinetics in the powder metallurgy superalloy N19 and influence of the precipitation latent heat // MATEC Web of Congerences. 2014. Available at: https://www.matec-conferences.org/ (accessed: August 25, 2019). DOI: 10.1051/matecconf/20141409004.
- Letnikov M.N., Lomberg B.S., Ospennikova O.G., Bakradze M.M. Vliyaniye skorosti okhlazhdeniya pri zakalke na mikrostrukturu i svoystva zharoprochnogo deformiruyemogo nikelevogo splava VZH175-ID [influence of quench rate on microstructure and mechanical properties of nickel-based wrought superalloy VZh175-ID] // Aviacionnye materialy i tehnologii. 2019. №2 (55). S. 21–30. DOI: 10.18577/2071-9140-2019-0-2-21-30.
- Baillif P., Lamesle P., Delagnes D. et al. Influence of the quenching rate and step-wise cooling temperatures on microstructural and tensile properties of PER72 Ni-based superalloy. Available at: https://www.matec-conferences.org (accessed: August 25, 2019). DOI: 10.1051/matecconf/20141421002.
- Xu C., Liu F., Huang L., Jiang. L. Dependance of creep performance and microstructure evolution on solution cooling rate in a polycrcystalline superalloy // Metals. 2018. Vol. 8. Issue 1. Available at: www.mdpi.com/jornal/metals (accessed: August 25, 2019). DOI: 10.3390/met8010004.
- Gabb T.P., Garg A., Ellis D.L., OʹConnor K.M. Detailed microstructural characterization of the disk alloy ME3. Available at: https://ntrs.nasa.gov (accessed: August 25, 2019).
- Mitchell R.J., Hardy M., Preuss M., Tin S. Development of ʹ morfology in P/M rotor disc alloys during heat treatment // Superalloys 2004. The Minerals, Metals & Materials Society, 2004. P. 361–370.
- Mitchell R.J., Preuss M. Inter-Relationships between Composition, ʹ Morphology, Hardness, and -ʹ Mismatch in Advanced Polycrystalline Nickel-Base Superalloys during Aging at 800°C // Metallurgical and Materials Transactions A. 2007. Vol. 38A. P. 615–627.
- Mitchell R.J., Preuss M., Tin S., Hardy M. The influence of cooling rate from temperatures above yʹ solvus on morphology, mismatch and hardness in advanced polycrystalline nickel-base superalloys // Materials Science and Engineering A. 2008. Vol. 473. Issues 1–2. P. 158–165.
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M. Novyy zharoprochnyy nikelevyy splav dlya diskov gazoturbinnykh dvigateley (GTD) i gazoturbinnykh ustanovok (GTU) [New heat-resistant nickel alloy for disks of gas turbine engines (GTE) and gas turbine units (GTU)] // Materialovedeniye. 2010. №7. S. 24–28.
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
- Kablov E.N. VIAM: materialy novogo pokoleniya dlya PD-14 [VIAM: new generation materials for PD-14] // Krylya Rodiny. 2019. №7–8. S. 54–58.
- Belyaev M.S., Terentev V.F., Gorbovec M.A., Bakradze M.M., Goldberg M.A. Malociklovaya ustalost pri zadannoj deformacii i parametry uprugoplasticheskogo deformirovaniya zharoprochnogo splava VZh175 [Low-cycle fatigue for a given deformation and parameters of elastic-plastic deformation of superalloy VZh175] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 87–92. DOI: 10.18577/2071-9140-2014-0-s4-87-92.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Chen Y., Prasath R., Slater T.J.A. et al. An investigation of diffusion – mediated cyclic coarsening and reversal coarsening in an advanced Ni-based superalloy // Acta Materialia. 2016. Vol. 110. P. 295–305.
- Goodfellow A.J., Galindo-Nava E.I., Christofidou K.A. et al. Gamma Prime Precipitate Evolution During Aging of a Model Nickel-Based Superalloy // Metallurgical and materials transaction A. 2018. Vol. 49A. P. 718–728. Available at: http://www.link.springer.com (accessed: August 25, 2019). DOI: 10.1007/s11661-017-4336-y.