Alternative technologies of the incresing of mechanical properties of P/M Ni-based superalloys for jet-engine disk application (review)

Volkov A.M., Karashaev M.M., Bakradze M.M., Pustynnikov T.O.
Volkov A.M., Karashaev M.M., Bakradze M.M., Pustynnikov T.O. Alternative technologies of the incresing of mechanical properties of P/M Ni-based superalloys for jet-engine disk application (review) // Proceedings of VIAM. 2019. No. 8. DOI: 10.18577/2307-6046-2019-0-8-3-8. URL: https://www.viam-works.ru/en/journal/2019/8/1
Keywords
Ni-base superalloy, jet-engine disk, powder, mechanical properties, hot isostatic pressing (HIP).
Abstract

The review of technological solutions which not yet has come to wide apply in production of jet-engine disk billets from Ni-based superalloy powder are presented. The methods of formation of particular phase composition are reviewed. The manners of powder production which are alternative to atomizing and PREP techniques are cited. The results of works carried out on liquid-phase sintering at the stage of consolidation of powder particles are described. Some original methods of material treatment for dual microstructure formation are enumerated.

Reference list
  1. Chabina E.B., Lomberg B.S., Filonova E.V., Ovsepyan S.V., Bakradze M.M. [Change of structural and phase condition of heat resisting deformable nickel alloy at alloying tantalum and rhenium] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 03. Available at: http://www.viam-works.ru (accessed: July 25, 2019). DOI: 10.18577/2307-6046-2015-0-9-3-3.
  2. Logunov A.V., Shmotin Yu.N., Danilov D.V. Metodologicheskiye osnovy avtomatizirovannogo proyektirovaniya zharoprochnykh splavov na nikelevoy osnove. Ch. 1 [Methodological principles of computer-aided design of heat-resistant nickel-based alloys. Part 1] // Tekhnologiya metallov. 2014. №5. S. 3–9.
  3. Chabina E.B. Vliyaniye mikrolegirovaniya lantanoidami na osobennosti formirovaniya struktury granits zeren i mezhfaznykh granits /zharoprochnogo nikelevogo splava tipa VZH175 [Microalloying influence by lanthanoids on feature of forming of structure grain boundaries and interphase boundaries of / heat resisting nickel alloy of the VZh175 type] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №2. St. 09. Available at: http://www.viam-works.ru (accessed: July 25, 2019). DOI: 10.18577/2307-6046-2017-0-2-9-9.
  4. Razuvaev E.I., Bubnov M.V., Bakradze M.M., Sidorov S.A. GIP i deformatsiia granulirovannykh zharoprochnykh nikelevykh splavov [HIP and deformation of the granulated heat resisting nickel alloys] // Aviatsionnye materialy i tekhnologii. 2016. №S1. S. 80–86. DOI: 10.18577/2071-9140-2016-0-S1-80-86.
  5. Karasev O.I., Vishnevskiy K.O., Veselitskaya N.N., Velikanova N.P., Kablov E.N. Forsayt razvitiya aviatsionnoy nauki i tekhnologiy do 2030 goda i na dalneyshuyu perspektivu [Foresight of the development of aviation science and technology until 2030 and beyond]. M.: TsAGI, 2014. 280 s.
  6. Kablov E.N., Bronfin M.B. Effekt S.T. Kishkina, ili pochemu struktura zharoprochnykh nikelevykh splavov dolzhna byt geterofaznoy [Effect S.T. Kishkina, or why the structure of heat-resistant nickel alloys should be heterophasic] // Liteynyye zharoprochnyye splavy. Effekt S.T. Kishkina. M.: Nauka, 2006. S. 7–14.
  7. Logunov A.V., Shmotin Yu.N. Sovremennyye zharoprochnyye nikelevyye splavy dlya diskov gazovykh turbin (materialy i tekhnologii) [Modern heat-resistant nickel alloys for gas turbine disks (materials and technologies)]. M.: Nauka i tekhnologiya, 2013. 264 s.
  8. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  9. A ternary nickel eutectic alloy: pat. EP 2065479A2; filed 21.10.08; publ. 03.06.09.
  10. Letnikov M.N., Lomberg B.S., Ovsepyan S.V. Issledovanie kompozicij sistemy Ni–Al–Co pri razrabotke novogo zharoprochnogo deformiruemogo intermetallidnogo splava [Investigation experimental alloys based on Ni–Al–Co ternary system for development a new high-temperature intermetallic alloy for disk application] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. № 10. St. 01. Available at: http://www.viam-works.ru (accessed: July 25, 2019).
  11. Smythe J. Superalloy powders: An amazing history // Advanced Materials & Processes. 2008. November. P. 53–55.
  12. Koshelev V.Ya., Khodkin V.I., Musiyenko V.T. Issledovaniye svoystv granul zharoprochnykh nikelevykh splavov, poluchennykh razlichnymi metodami raspyleniya [Investigation of the properties of granules of heat-resistant nickel alloys obtained by various spraying methods] // Metallovedeniye i obrabotka titanovykh i zharoprochnykh splavov. 1991. S. 333–340.
  13. Gessinger G.Kh. Poroshkovaya metallurgiya zharoprochnykh splavov. Per. s angl. [Powder metallurgy of heat-resistant alloys. Line from Engl.]. Chelyabinsk: Metallurgiya, 1988. 320 s.
  14. Serov M.M., Kazberovich A.M., Ber L.B., Konyayev V.S., Tarmosin E.V. Sravnitelnye issledovaniya struktury diskretnykh volokon i granul iz zharoprochnogo nikelevogo splava EP741NP [Comparative studies of the structure of discrete fibers and granules of heat-resistant nickel alloy EP741NP] // Tekhnologiya legkikh splavov. 2012. №2. S. 48–52.
  15. Tarmosin E.V., Logachev A.V., Stepkin E.P., Serov M.M. Issledovaniye protsessa polucheniya kompaktnykh zagotovok iz bystrozakalennykh chastits splava EP741NP [Investigation of the process of producing compact billets from rapidly quenched particles of EP741NP alloy] // Vakuumnaya tekhnika i tekhnologiya. 2014. T. 24. №2. S. 135–140.
  16. Tyagunov A.G., Baryshev E.E., Tyagunov G.V., Shmakova K.Yu. Optimizatsiya temperaturnogo rezhima polucheniya volokon iz zharoprochnogo splava EP741NP [Optimization of the temperature regime for producing fibers from the heat-resistant alloy EP741NP] // Elektrometallurgiya. 2016. №7. S. 3–8.
  17. Libenson G.A., Lopatin V.Yu., Komarnitskiy G.V. Protsessy poroshkovoy metallurgii: ucheb. dlya vuzov v 2 t. [The processes of powder metallurgy: textbook. for universities in 2 vol.]. M.: MISIS, 2002. T. 2: Formovaniye i spekaniye, 320 s.
  18. Jeandin M., Bienvenu Y., Koutny J.L. Liquid phase sintering of nickel base superalloys // Superalloys–1984. 1984. P. 467–476.
  19. Morishita M., Nagai H., Shoji K. Liquid phase sintering of Ni-base superalloy IN-100 // Transactions of Japan Institute of Metals. 1986. Vol. 27. No 1. P. 61–69.
  20. Pierron X., Banik A., Maurer G.E., Lemsky J., Furrer D.U. Sub-solidus HIP process for P/M superalloy conventional billet conversation // Superalloys–2000. 2000. P. 425–433.
  21. Bratukhin A.G., Maslenkov S.B., Logunov A.V. Fiziko-khimicheskiye osnovy tekhnologii zhidkofaznogo spekaniya granul [Physicochemical principles of the technology of liquid-phase sintering of granules] // Materialovedeniye. 1997. №2. S. 53–56.
  22. Method of selective grain growth in nickel-based superalloys by controlled boron diffusion: pat. US 4401480; filed 19.1081; publ. 30.08.83.
  23. Graded metallic structures and method of forming and related articles: application US 2008/0142126 A1; filed 19.06.08.
  24. Multi-alloy turbine rotor disk: pat. US 4900635; filed 09.02.89; publ. 13.02.90.