The research of a specific electrical conductivity of Mo–W powder alloys obtained by SPS

Batienkov R.V., Efimochkin I.Yu., Khudnev A.A.
Batienkov R.V., Efimochkin I.Yu., Khudnev A.A. The research of a specific electrical conductivity of Mo–W powder alloys obtained by SPS // Proceedings of VIAM. 2019. No. 7. DOI: 10.18577/2307-6046-2019-0-7-50-58. URL: https://www.viam-works.ru/en/journal/2019/7/6
Keywords
refractory metals, molybdenum and tungsten alloys, specific electrical conductivity, powder metallurgy, spark plasma sintering.
Abstract

The relationship between specific electrical conductivity of Mo–W powder alloys obtained by SPS and tungsten content and process parameters was studied in this work. The specific electrical conductivity’s values for the alloy with 20% (wt) tungsten are in the range between 7,10·10-8 and 9,04·10-8 Ohm·m depending on the sintering temperature while with the increase of tungsten content till 30% (wt) the values of the specific electrical conductivity are increasing too and are within the range of 7,83·10-8 to 10,60·10-8 Ohm·m. A porosity alloys phases content and a grain size were determined as having the most impact on a specific electrical conductivity values. The evaluation of the main factors’ influence on a specific electrical conductivity values was carried out.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Svetlov I.L., Neiman A.V., Min P.G., Karachevtsev F.N., Karpov M.I. High-temperature composites based on the Nb–Si system reinforced with niobium silicides // Inorganic Materials: Applied Research. 2017. Vol. 8. No. 4. P. 609–617.
  3. Kablov E.N., Bondarenko Yu.A., Echin A.B. Razvitiye tekhnologii napravlennoy kristallizatsii liteynykh vysokozharoprochnykh splavov s peremennym upravlyayemym temperaturnym gradiyentom [Development of technology of cast superalloys directional solidification with variable controlled temperature gradient] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  4. Ospennikova O.G., Podieiachev V.N., Stoliankov Yu.V. Tugoplavkie splavy dlia novoi tekhniki [Refractory alloys for innovative equipment] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №10. St. 05. Available at: http://www.viam-works.ru (accessed: April 10, 2019). DOI:10.18577/2307-6046-2016-0-10-5-5.
  5. Kucher A.M. Tekhnologiya metallov [Metal technology]. L.: Mashinostroyeniye, 1987. 214 s.
  6. Agte K., Vatsek I. Volfram i molibden [Wolfram and molybdenum]. L.: Energiya, 1964. 455 s.
  7. Batiyenkov R.V., Bolshakova A.N., Yefimochkin I.Yu. Problema nizkotemperaturnoy plastichnosti molibdena i splavov na yego osnove (obzor) [The problem of low-temperature plasticity of molybdenum and alloys based on it (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №3 (63). St. 02. Available at: http://www.viam-works.ru (accessed: April 11, 2019). DOI: 10.18577/2307-6046-2018-0-3-12-17.
  8. Samodurova M.N., Barkov L.A., Ivanov V.A. Metallurgiya i tekhnologiya poroshkovogo molibdena: ucheb. Posobiye [Metallurgy and molybdenum powder technology: tutorial]. Chelyabinsk: YuUrGU, 2014. 186 s.
  9. Morgunova N.N., Klypin B.A., Boyarshinov V.A. i dr. Splavy molibdena [Alloys of molybdenum]. M.: Metallurgiya, 1975. 392 s.
  10. Svoystva i primeneniye metallov i splavov dlya elektrovakuumnykh priborov: spravochnoye posobiye / pod obshch. red. R.A. Nilendera [Properties and applications of metals and alloys for vacuum devices: a reference guide / gen. ed. R.A. Nilender]. M.: Energiya, 1973. 336 s.
  11. Torresilyas San Millan R., Pinargote Solis N.V., Okunkova A.A., Peretyagin P.Yu. Osnovy protsessa iskrovogo plazmennogo spekaniya nanoporoshkov [Fundamentals of spark plasma sintering of nanopowders]. M.: Tekhnosfera, 2014. 96 s.
  12. Ermakov S.S. Fizika metallov i defekty kristallicheskogo stroyeniya: ucheb. posobiye [Physics of metals and defects of a crystal structure: tutrial]. L.: Izd-vo Leningr. un-ta, 1989. 280 s.
  13. Sevostyanova I.N., Anisimov V.Zh., Gnyusov S.F., Kulkov S.N. Fiziko-mekhanicheskiye svoystva poristykh kompozitov na osnove karbida titana [Physical and mechanical properties of porous composites based on titanium carbide] // Fizicheskaya mezomekhanika. 2004. Ch. 2. №7. Spetsvypusk. S. 89–92.
  14. Livshits B.G., Kraposhin V.S., Linetskiy Ya.L. Fizicheskiye svoystva metallov i splavov [Physical properties of metals and alloys]. M.: Metallurgiya, 1980. 318 s.
  15. Batiyenkov R.V., Efimochkin I.Yu., Osin I.V., Khudnev A.A. Issledovaniye mekhanicheskikh svoystv poroshkovykh materialov sistemy Mo–W, poluchennykh elektroiskrovym plazmennym spekaniyem [Investigation of the mechanical properties of powder materials of the Mо–W system obtained by spark plasma sintering] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2019. №2 (74). St. 07. URL: http://www.viam-works.ru (April 08, 2019). DOI: 10.18577/2307-6046-2019-0-2-68-76.