The criteria of the failure of polymer matrix composites (review)

Grinevich D.V., Yakovlev N.O., Slavin A.V.
Grinevich D.V., Yakovlev N.O., Slavin A.V. The criteria of the failure of polymer matrix composites (review) // Proceedings of VIAM. 2019. No. 7. DOI: 10.18577/2307-6046-2019-0-7-92-111. URL: https://www.viam-works.ru/en/journal/2019/7/11
Keywords
composite materials, lamina, reinforcement, glass-reinforced plastic, carbon-reinforced plastic, finite element method, simulation, failure criteria.
Abstract

The paper deals of the main failure criteria of polymer matrix composites, used in modern simulation’s software systems by calculating the strength of composite plates and shells.The limit criteria (for stress and strain) are noted, and the polynomial failure criteria: Tsai-Wu, Tsai-Hill, Yamada-Sun, Hoffman, Cowin, Hankinson, Norris, and separated modes failure criteria: Puck (in various modifications), Hashin, Christensen, LaRC, Cuntze and others. Much attention is given to the theoretical background of the criteria and the applied approaches for the calculation of the strength of composite materials.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  3. Kablov E.N. Stanovleniye otechestvennogo kosmicheskogo materialovedeniya [Formation of domestic space materials science] // Vestnik RFFI. 2017. №3. S. 97–105.
  4. Yakovlev N.O., Gulyaev A.I., Lashov O.A. Treshchinostoikost sloistykh polimernykh kompozitsionnykh materialov (obzor) [Crack firmness of layered polymeric composite materials (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №4 (40). St. 12. Available at: http://www.viam-works.ru (accessed: March 19, 2019) DOI: 10.185772307-6046-2016-0-4-12-12.
  5. Krylov V.D., Yakovlev N.O., Kurganova Yu.A., Lashov O.A. Mezhsloevaya treshchinostoikost konstruktsionnykh polimernykh kompozitsionnykh materialov [Mezhsloyevy crack firmness of constructional polymeric composite materials] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 79–85. DOI: 10.18577/2071-9140-2016-0-1-79-85.
  6. Vlasenko F.S., Raskutin A.E. Primenenie polimernyh kompozicionnyh materialov v stroitelnyh konstrukcijah [Applying FRP in building structures] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 03. Available at: http://viam-works.ru (accessed: March 20, 2019).
  7. Kondrashov S.V., Shashkeev K.A., Popkov O.V., Solovyanchik L.V. Fiziko-mehanicheskie svojstva nanokompozitov s UNT (obzor) [Mechanical properties of CNT nanocomposites (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5. St. 08. Available at: http://www.viam-works.ru (accessed: March 19, 2019). DOI: 10.18577/2307-6046-2016-0-5-8-8.
  8. Doriomedov M.S., Daskovskij M.I., Skripachev S.Yu., Shein E.A. Polimernye kompozicionnye materialy v zheleznodorozhnom transporte Rossii (obzor) [Polymer composite materials in the Russian railways (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 12. Available at: http://www.viam-works.ru (accessed: March 19, 2019). DOI: 10.18577/2307-6046-2016-0-7-12-12.
  9. Dimitriyenko Yu.I., Gubareva E.A., Sborshchikov S.V., Erasov V.S., Yakovlev N.O. Chislennoye modelirovaniye i eksperimental'noye issledovaniye deformirovaniya uprugoplasticheskikh plastin pri smyatii [Numerical modeling and experimental study of the deformation of elastoplastic plates when bent] // Matematicheskoye modelirovaniye i chislennyye metody. 2015. №1 (5). S. 67–82.
  10. Dimitriyenko Yu.I., Fedonyuk N.N., Gubareva E.A., Sborshchikov S.V., Prozorovskiy A.A., Erasov V.S., Yakovlev N.O. Modelirovaniye i razrabotka trekhsloynykh kompozitsionnykh materialov s sotovym zapolnitelem [Modeling and development of three-layer composite materials with honeycomb] // Vestnik MGTU im. N.E. Baumana. Ser.: Estestvennyye nauki. 2014. №5. S. 66–81.
  11. Erasov V.S., Yakovlev N.O., Gladkikh A.V., Goncharov A.A., Skiba O.V., Boyarskikh A.V., Podzhivotov N.Yu. Ispytaniya krupnogabaritnykh konstruktsiy iz polimernykh kompozitsionnykh materialov na silovom polu GTSKI VIAM im. G.V. Akimova [Testing of large-sized structures made of polymer composite materials on the power floor G.V. Akimov GTCT of VIAM] // Kompozitnyy mir. 2014. №1. S. 72–78.
  12. Amelina E.V., Golushko S.K., Erasov V.S., Idimeshev S.V., Nemirovskiy Yu.V., Semisalov B.V., Yurchenko A.V., Yakovlev N.O. O nelineynom deformirovanii ugleplastikov: eksperiment, model, raschet [On the nonlinear deformation of carbon plastics: experiment, model, calculation] // Vychislitelnyye tekhnologii. 2015. №5. S. 27–52.
  13. Skvortsov Yu.V. Mekhanika kompozitsionnykh materialov: konspekt lektsiy [Mechanics of composite materials: lecture notes]. Samara: SGAU, 2013. 94 s.
  14. Cuntze R. Neue Bruchkriterien und Festigkeitsnachweise für unidirektionalen Faserkunststoffverbund unter mehrachsiger Beanspruchung: Modellbildung und Experimente. Düsseldorf: VDI-Verlag, 1997. 249 p.
  15. Stowell E.Z., Liu T.S. On the Mechanical Behavior of Fiber Reinforces Crystalline Solids // Journal of the Mechanics and Physics of Solids. 1961. Vol. 9. P. 242–260.
  16. Kelly A., Davies G.J. The Principles of the Fibre Reinforcement of Metals // Metallurgical Reviews. 1965. Vol. 10. No. 37. P. 1–77.
  17. Zakharov K.V. Kriteriy prochnosti dlya sloistykh mass [Strength criterion for layered masses] // Plasticheskiye massy. 1961. №8. S. 61–67.
  18. Malmeyster A.K. Geometriya teoriy prochnosti [Geometry of theories of strength] // Mekhanika polimerov. 1966. №4. S. 519–534.
  19. Goldenblat I.I., Kopnov V.A. Kriteriy prochnosti anizotropnykh materialov [Strength criterion for anisotropic materials] // Mekhanika. 1965. №6. S. 77–83.
  20. Goldenblat I.I., Kopnov V.A. Kriterii prochnosti i plastichnosti konstruktsionnykh materialov [Criteria of strength and plasticity of structural materials]. M.: Mashinostroyeniye, 1968. 192 s.
  21. Makovenko S.Ya. O vzaimnosti komponent tenzorov prochnosti nekotorykh teoriy prochnosti anizotropnykh materialov [On the reciprocity of the component tensors of strength of some theories of strength of anisotropic materials] // Stroitelnaya mekhanika inzhenernykh konstruktsiy i sooruzheniy. 2005. №1. S. 65–70.
  22. Reddy J.N., Pandey A.K. A first-ply failure analysis of composite laminates // Computers & Structures, 1987. No. 25 (3). P. 371–393. DOI: 10.1016/0045-7949(87)90130-1.
  23. ANSYS Composite PrepPost User's Guide. Available at: https://ansyshelp.ansys.com (accessed: March 19, 2019).
  24. Muyzemnek A.Yu., Kartashova E.D. Mekhanika deformirovaniya i razrusheniya polimernykh sloistykh kompozitsionnykh materialov: ucheb. Posobiye. [Mechanics of deformation and destruction of polymer layered composite materials: tutorial] Penza: Izd-vo PGU, 2017. 77 s.
  25. Abrate S. Criteria for yielding or failure of cellular materials // Journal of Sandwich Structures and Materials. 2008. Vol. 10. P. 5–51.
  26. Hill R. The Mathematical theory of plasticity. London: Oxford University Press, 1950. 317 p.
  27. Azzi V.D., Tsai S.W. Anisotropic Strength of Composites // Experimental Mechanics. 1965. Vol. 5. Nо. 9. P. 283–288. DOI: 10.1007/BF02326292.
  28. Yamada S.E., Sun C.T. Analysis of Laminate Strength and Its Distribution // Journal of Composite Materials. 1978. No. 12 (3). P. 275–284. DOI: 10.1177/002199837801200305.
  29. Hoffman O. The brittle strength of orthotropic materials // Journal of Composite Materials. 1967. No. 1. P. 200–206.
  30. Tsai S.W., Wu E.M. A General Theory of Strength for Anisotropic Materials // Journal of Composite Materials. 1971. No. 5 (1). P. 58–80. DOI:10.1177/002199837100500106.
  31. Tarnopolskiy Yu.M., Kintsis T.YA. Metody staticheskikh ispytaniy armirovannykh plastikov. 2-e izd. pererab. i dop. [Static test methods for reinforced plastics. 2nd ed. eev. and add]. M.: Khimiya, 1975. 262 s.
  32. Hankinson R.L. Investigation of crushing strength of spruce at varying angles of grain // Air Force Information Circular. 1921. No. 259. P. 3–15.
  33. Cowin S.C. Fabric Dependence of an Anisotropic Strength Criterion // Mechanics of Materials. 1986. No. 5 (3). P. 251–260. DOI: 10.1016/0167-6636(86)90022-0.
  34. MSC Laminate Modeler Version 2008 r2. User’s Guide. MSC Software Corporation, 2008. 176 p.
  35. Mascia N.T., Simoni R.A. Analysis of failure criteria applied to wood // Engineering Failure Analysis. 2013. No. 35. P. 703–712. DOI: 10.1016/j.engfailanal.2013.07.001.
  36. Puck A., Schneider W. On Failure Mechanisms and Failure Criteria of Filament-wound Glass-Fiber/Resin Composites // Plastic and Polymer Technology. 1969. Vol. 00/Publisher. P. 33–43.
  37. Puck A. Festigkeitsberechnung an Glasfaser/Kunststoff-Laminaten bei zusam-mengesetzter Beanspruchung // Kunststoffe. 1969. Vol. 59. No. 11. P. 780–787.
  38. Knops M. Analysis of Failure in Fiber Polymer Laminates. Springer Berlin Heidelberg, 2008. 205 p. DOI: 10.1007/978-3-540-75765-8.
  39. Puck A., Schurmann H. Failure analysis of FRP laminates by means of physically based phenomenological models // Composites Science and Technology. 1998. Vol. 58. P. 1045–1067.
  40. Puck A., Kopp J., Knops M. Failure analysis of FRP laminates by means of physically based phenomenological models // Composites Science and Technology. 2002. Vol. 62. P. 1633–1662.
  41. Puck A., Kopp J., Knops M. Guidelines for the determination of the parameters in Puck's action plane strength criterion // Composites Science and Technology. 2002. Vol. 62. P. 371–378.
  42. Hashin Z., Rotem A.A. Fatigue Failure Criterion for Fiber Reinforced Materials // Journal of Composite Materials. 1973. No. 7 (4). P. 448–464. DOI: 10.1177/002199837300700404.
  43. Hashin Z. Failure Criteria for Unidirectional Fiber Composites // Journal of Applied Mechanics. 1980. No. 47. P. 329–334.
  44. Christensen R.M. Stress Based Yield/Failure Criteria for Fiber Composites // International Journal of Solids and Structures. 1997. No. 34. P. 529–543.
  45. Davila C., Navin J. Failure Criteria for FRP Laminates in Plane-Stress. NASA Langley Research Center, 2003. 28 p.
  46. Pinho S., Davila C., Camanho P. et al. Failure models and criteria for FRP under in-plane or three-dimensional stress states including shear non-linearity: TM-2005-213530. NASA, 2005. 69 p.
  47. Laws N. A note on interaction energies associated with cracks in anisotropic solids // Philosophical Magazine. 1977. No. 36 (2). P. 367–372. DOI: 10.1080/14786437708244940.
  48. Pinho S.T., Robinson P., Iannucci L. Fracture toughness of the tensile and compressive fibre failure modes in laminated composites // Composites Science and Technology. 2006. No. 66 (13). P. 2069–2079.
  49. Davila C., Jaunky N., Goswami S. Failure Criteria for FRP Laminates in Plane Stress // 44th AI-AA/AME/ASCE/AHS/ASC Structures, Structural Dynamics, and Materials Conference. (Norfolk, Virginia, April 7–10, 2003). 2003. 11 p. DOI: 10.2514/6.2003-1991.
  50. Cuntze R., Freund A. The predictive capability of failure mode concept-based strength criteria for multidirectional laminates // Composites Science and Technology. 2004. Vol. 64. P. 343–377.
  51. Cuntze R. Efficient 3D and 2D failure conditions for UD laminae and their application within the verification of the laminate design // Composites Science and Technology. 2006. Vol. 66. No. 7–8. P. 1081–1096.
  52. Cuntze R. The predictive capability of failure mode concept-based strength conditions for laminates composed of UD laminas under static tri-axial stress states. Part A of the WWFE-II // Journal of Composite Materials. 2012. No. 46 (19–20). P. 2563–2594. DOI: 10.1177/0021998312449894.
  53. Boehler J.P. Failure Criteria for Glass-Fiber Reinforced Composites under Confining Pressure // Journal of Structural Mechanics. 1985. No. 13. 371 p.