Application of aerogels for the heat insulation materials (review)

Babashov V.G., Varrik N.M., Karaseva T.A.
Babashov V.G., Varrik N.M., Karaseva T.A. Application of aerogels for the heat insulation materials (review) // Proceedings of VIAM. 2019. No. 6. DOI: 10.18577/2307-6046-2019-0-6-32-42. URL: https://www.viam-works.ru/en/journal/2019/6/4
Keywords
aerogel, silicon dioxide, heat insulation, composite material, oxide fibers, high temperature heat insulation.
Abstract

In recent years there were many messages about development and use of a new class of materials – aero gels of various structure. Aero gels represent solid substance with very low density and a large number of the time filled with air or gas. Aero gel has low heat conductivity, index of refraction of light, dielectric permeability and speed of distribution of a sound. Modern technologies allowed to begin mass production of aero gels of dioxide of silicon which find more and more broad application at production of thermal insulation for industrial and construction use. This article submits the review of the heat-insulating materials intended for protection both from high, and from low temperatures, with use of aero gels.

Reference list
  1. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing are the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Bez novykh materialov – net budushchego [Without new materials there is no future] // Metallurg. 2013. №12. S. 4–8.
  4. Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 05. Available at: http://www.viam-works.ru (accessed: April 03, 2019).
  5. Babashov V.G., Varrik N.M. Vysokotemperaturnyj gibkij voloknistyj teploizolyacionnyj material [High-temperature flexible fibrous insulation material] // Trudy VIAM :elektron. nauch.-tehnich. zhurn. 2015. №1. St. 03. Available at: http://viam-works.ru (accessed: April 03, 2019). DOI: 10.18577/2307-6046-2015-0-1-3-3.
  6. Buchilin N.V., Lyulyukina G.Yu. Osobennosti spekaniya vysokoporistykh keramicheskikh materialov na osnove oksida alyuminiya [Characteristics of sintering of highly porous alumina-based ceramic materials] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 40–46. DOI: 10.18577/2071-9140-2016-0-4-40-46.
  7. Istomin A.V., Bespalov A.S., Babashov V.G. Pridaniye povyshennoy ognestoykosti teplozvukoizolyatsionnomu materialu na osnove smesi neorganicheskikh i rastitelnykh volokon [Adding increased resistance to heat and sound insulation of material based on mixture of inorganic and plant fibers] // Aviacionnye materialy i tehnologii. 2018. №4 (53). S. 74–78. DOI: 10.18577/2071-9140-2018-0-4-74-78.
  8. Smirnov B.M. Aerogeli [Aerogels] // Uspekhi fizicheskikh nauk. 1987. T. 152. Vyp. 1. S. 133–157.
  9. Danilyuk A.F., Kononov S.A., Kravchenko Ye.A., Onuchin A.P. Aerogelevyye cherenkovskiye detektory v eksperimentakh na vstrechnykh puchkakh [Airgel Cherenkov detectors in experiments on colliding beams] // Uspekhi fizicheskikh nauk. 2015. T. 185. №5. S. 540–548.
  10. Lermontov S.A., Malkova A.N., Sipyagina N.A. i dr. Upravleniye gidrofobnostyu/gidrofilnostyu aerogeley na osnove SiO2: rol sverkhkriticheskogo rastvoritelya [Hydrophobicity / hydrophilicity control of SiO2-based aerogels: the role of a supercritical solvent] // Zhurnal neorganicheskoy khimii. 2015. T. 60. №10. S. 1283–1286.
  11. Kovalko N.Yu., Kalinina M.V., Malkova A.N. i dr. Sintez i sravnitelnoye issledovaniye kserogeley, aerogeley i poroshkov na osnove sistemy ZrO2–Y2O3–CeO2 [Synthesis and Comparative Study of Xerogels, Aerogels, and Powders Based on the ZrO2–Y2O3–CeO2 System] // Fizika i khimiya stekla. 2017. T. 43. №4. S. 415–424.
  12. Shindryayev A.V., Kozhevnikov Yu.Yu., Lebedev A.E., Menshutina N.V. Issledovaniye protsessa polucheniya teploizolyatsionnykh materialov na osnove aerogeley [Investigation of the Process of Obtaining Thermal Insulating Materials Based on Aerogels] // Uspekhi v khimii i khimicheskoy tekhnologii. 2017. T. 31. №6. S. 130–132.
  13. Lebedev A.Ye. Modelirovaniye i masshtabirovaniye protsessov polucheniya aerogeley i funktsionalnykh materialov na ikh osnove: dis. … kand. tekhn. nauk [Modeling and scaling of the processes of obtaining aerogels and functional materials based on them: thesis, Cand. Sc. (Tech.)]. M., 156 s.
  14. Ivanov S.I., Tsygankov P.Yu., Khudeyev I.I., Menshutina N.V. Polucheniye gidrofobnykh aerogeley [Production of hydrophobic airgel] // Uspekhi v khimii i khimicheskoy tekhnologii. 2015. T. 29. №4. S. 112–114.
  15. Aerogel matrix composites: pat. US 5306555, No. 904777; filed 26.06.92; publ. 26.04.94.
  16. Aerogel composites, process for producing the same and their use: pat. US 5789075, No. 793178; filed 17.08.95; publ. 04.08.98.
  17. Flexible aerogel superinsulation and its manufacture: pat. US 6068882, No. 09/056413; filed 07.04.98; publ. 30.05.00.
  18. Aerogel composite with fibrous batting: pat. US 7078359, No. 10/034296; filed 21.12.01; publ. 18.07.06.
  19. Advanced gel sheet production: pat. US 7780890, No. 11/762654; filed 13.06.07, publ. 24.08.10.
  20. Hydrophobic Аerogel Мaterials: pat. US 9868843, No. 14/873753; filed 02.10.15; publ. 16.01.18.
  21. Teploizolyatsiya s aerogelyami [Thermal insulation with airgel] // Kompaniya Aspen Aerogels Inc.: ofits. sayt. Available at: www.aerogel.com (accessed: March 27, 2019).
  22. Thermal insulation assemblies and methods the fabrication the same: pat. US 8357258, №12/983918; filed 04.01.11; publ. 22.01.13.
  23. Laminate Thermal Insulation Blanket for Aircraft Applications and Process thereof:
  24. pat. 20120308369, No. 13/118867; filed 31.05.11; publ. 06.12.12.
  25. Preparation method of fiber-reinforced Al2O3–SiO2 aerogel material with wave transmission and heat insulation integrated function: pat. CH 106630931, No. 20161885973; filed 10.10.16; publ. 10.05.17.
  26. Ceramic composite material of high temperature insulation sandwich structure and method for preparing ceramic composite material: pat. CH 10264235, No. 20121120442; filed 24.04.12; publ. 22.08.12.
  27. External thermal insulation material and preparation method thereof: pat. CH 106584942, No. 201611114754; filed 07.12.16; publ. 24.06.17.
  28. Silicon dioxide aerogel with high specific surface area and fast preparation method thereof: pat. US 106672985, No. 20171005206; filed 04. 01.17; publ. 17.05.17.
  29. Preparation system and preparation method of gel composites: pat. CH 108381949, No. 201810130441; filed 08. 02.18; publ.10.08.18.
  30. Packaging method for aerogel felts, and aerogel felt packaged product: pat. CH 108910112, No. 201810901381; filed 09.08.18; publ. 30.11.18.
  31. Teploizolyatsiya s aerogelyami (Rossiya) [Thermal insulation with aerogels (Russia)] // OOO «TIM»: ofits. sayt. Available at: www.tim-firm.ru (accessed: April 04, 2019).
  32. Teploizolyatsiya s aerogelyami (KNR) [Thermal insulation with aerogels (PRC)] // Kompaniya Joda: ofits. sayt. Available at: www.joda-tech.ru (accessed: April 04, 2019).
  33. Preparation method of high-zirconia aerogel: pat. CH 108483493, No. 201810522250; filed 28.05.18; publ. 04.09.18.
  34. Method for preparing alumina aerogel: pat. CH 108328635, No. 201810234361; filed 21.03.18; publ. 27.07.18.
  35. Preparation of a metastable tetragonal zirconia aerogel: pat. US 20190023581, No. 15/518599; filed 13.10.15; publ. 24.01.19.