Synthesis, structure and properties of ceramics based on aluminium oxynitride (AlON), obtained by the method of spark plasma sintering

Zabelin D.A., Chaynikova A.S., Kachaev A.A., Osin I.V., Grachshencov D.V.
Zabelin D.A., Chaynikova A.S., Kachaev A.A., Osin I.V., Grachshencov D.V. Synthesis, structure and properties of ceramics based on aluminium oxynitride (AlON), obtained by the method of spark plasma sintering // Proceedings of VIAM. 2019. No. 6. DOI: 10.18577/2307-6046-2019-0-6-13-19. URL: https://www.viam-works.ru/en/journal/2019/6/2
Keywords
aluminum oxynitride, transparent ceramics, spark plasma sintering, microhardness, crack resistance, oxynitride ceramics.
Abstract

Ceramics based on aluminum oxynitride (AlON) by the method of spark plasma sintering (SPS) were synthesized. It has been established that a decrease in the particle size of the initial powders leads to an intensification of the AlON phase formation process and an increase in the physicomechanical properties of ceramics. It is shown that the introduction of sintering additive Y2O3 contributes to a more complete transformation of the initial components into the AlON phase due to the formation of a liquid phase at the grain boundaries. It was revealed that an increase in the sintering temperature by the SPS method from 1600 to 1700°С leads to a decrease in the va-lues of density and physicomechanical properties of ceramics based on aluminium oxynitride.

Reference list
  1. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  2. Kablov E.N., Ospennikova O.G., Svetlov I.L. Vysokoeffektivnoe ohlazhdenie lopatok goryachego trakta GTD [Highly efficient cooling of GTE hot section blades] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  3. Kablov E.N., Grashchenkov D.V., Isayeva N.V., Solntsev S.S., Sevastyanov V.G. Vysokotemperaturnye konstruktsionnye kompozitsionnye materialy na osnove stekla i keramiki dlya perspektivnykh izdeliy aviatsionnoy tekhniki [High-temperature structural composite materials based on glass and ceramics for promising products of aeronautical engineering] // Steklo i keramika. 2012. №4. S. 7–11.
  4. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.St. Perspektivnye vysokotemperaturnye keramicheskie kompozitsionnye materialy [Prospective high-temperature ceramic composite materials] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 20–24.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Grashchenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  7. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsional'noy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2. S. 16–21.
  8. Kablov E.N. Innovatsionnoye razvitiye – vazhneyshiy prioritet gosudarstva [Innovative development is the most important priority of the state] // Metally Evrazii. 2010. №2. S. 6–11.
  9. McCauley J.W., Patel P., Chen M. AlON: a brief history of its emergence and evolution // Journal of the European Ceramic Society. 2009. Vol. 29. No. 2. P. 223–236.
  10. Evdokimov S.A., Shchegoleva N.E., Sorokin O.Yu. Keramicheskiye materialy v aviatsionnom dvigatelestroyenii (obzor) [Ceramic materials in aviation engineering (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №12 (72). St. 06. Available at: http://www.viam-works.ru (accessed: March 22, 2019). DOI: 10.18577/2307-6046-2018-0-12-54-61.
  11. Liu X.J., Chen F., Zhang F. Hard transparent AlON ceramic for visible/IR windows // International Journal of Refractory Metals and Hard Materials. 2013. Vol. 39. P. 38–43.
  12. Method of making aluminum oxynitride: US8211356B1; filed 18.07.00; publ. 03.07.12.
  13. Wang J., Lin J., Zhang Z., Chen S. Effect of Y2O3 and La2O3 on the sinterability of g-AlON transparent ceramics // Journal of the European Ceramic Society. 2015. Vol. 35. No. 1. P. 23–28.
  14. Li X., Luo J., Zhou Y. Spark plasma sintering behavior of AlON ceramics doped with different concentrations of Y2O3 // Journal of the European Ceramic Society. 2015. Vol. 35. No. 7. P. 2027–2032.
  15. Vaganova M.L., Sorokin O.YU., Osin I.V. Soyedineniye keramicheskikh materialov metodom iskrovogo plazmennogo spekaniya // Aviatsionnyye materialy i tekhnologii. 2017. №S. S. 306–317. DOI: 10.18577/2071-9140-2017-0-S-306-317.
  16. Kessel Kh.U. Tekhnologiya spekaniya v elektricheskom pole: «FAST» (field assisted sintering technology)-novyy metod spekaniya metallicheskikh i keramicheskikh materialov. Available at: http://www.fct-systeme.de/ (accessed: March 28, 2019).
  17. Xidong W., Fuming W., Wenchao L. Synthesis, microstructures and properties of g-aluminum oxynitride // Materials Science and Engineering: A. 2003. Vol. 342. No. 1. P. 245–250.
  18. Graham E.K., Munly W.C., McCauley J.W. Elastic properties of polycrystalline aluminum oxynitride spinel and their dependence on pressure, temperature, and composition // Journal of the American Ceramic Society. 1988. Vol. 71. No. 10. P. 807–812.