The test pieces to determine the performanceof magnetic particle flaw detectors and magnetic media (review)
Kadosov A.D., Lednev I.S., Pavlova T.D., Golovkov A.N. The test pieces to determine the performanceof magnetic particle flaw detectors and magnetic media (review) // Proceedings of VIAM. 2019. No. 5. DOI: 10.18577/2307-6046-2019-0-5-76-84. URL: https://www.viam-works.ru/en/journal/2019/5/9
Keywords
magnetic particle inspection, test pieces, determination of performance, magnetic media, magnetizing field, quality control, magnetic flaw detector, flux indicator strips, quantitative quality indicators.
Abstract
The article describes the main types of Russian and worldwide test pieces for magnetic particle inspection, used to assess the performance of magnetic particle flaw detectors, the performance of magnetic indicators, as well as to determine the direction of the magnetizing field. Their device is shown, recommendations on their use, interpretation of results, and also factors which can lead to damage and failure of samples are given. The problems of using special test pieces for magnetic particle inspection are shown.
Reference list
- Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation – the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Rossiya na rynke intellektualnykh resursov [Russia in the market of intellectual resources] // Ekspert. 2015. №28 (951). S. 48–51.
- Lutsenko A.N., Perov N.S., Chabina E.B. Novye etapy razvitiya Ispytatelnogo tsentra [The new stages of development of Testing Center] // Aviacionnye materialy i tehnologii 2017. №S. S. 460–468. DOI: 10.18577/2071-9140-2017-0-S-460-468.
- Murashov V.V. Ocenka stepeni nakopleniya mikropovrezhdenij struktury PKM v detalyah i konstrukciyah nerazrushayushhimi metodami [Assessment of accumulation degree of microdamages of PCM structure in structures determined by nondestructive methods] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 73–81. DOI: 10.18577/2071-9140-2016-0-3-73-81.
- Boychuk A.S., Generalov A.S., Stepanov A.V. Nerazrushayushhij kontrol ugleplastikov na nalichie nesploshnostej s ispolzovaniem ultrazvukovyh fazirovannyh reshetok [NDT monitoring of CFRP structural health by ultrasonic phased array technique] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 84–89. DOI: 10.18577/2071-9140-2015-0-3-84-89.
- GOST R ISO 9934-2–2011. Kontrol nerazrushayushchiy. Magnitoporoshkovyy metod. Chast 2. Defektoskopicheskiye materialy [State Standard R ISO 9934-2-2011. Nondestructive control. Magnetic particle method. Part 2. Flaw detection materials]. M.: Standartinform, 2013. 20 s.
- Nerazrushayushchiy kontrol: spravochnik v 7 t. / pod obshch. red. V.V. Klyuyeva [Non-destructive testing: a reference book in 7 vol. / gen. ed. by V.V. Klyuev]. M.: Mashinostroyeniye, 2004. T. 6. Kn. 1: Magnitnyye metody kontrolya / V.V. Klyuyev, V.F. Muzhitskiy, E.S. Gorkunov, V.E. Shcherbinin. 832 s.
- Gerasimov V.G., Pokrovskiy A.D., Sukhorukov V.V. Nerazrushayushchiy kontrol v 5 kn. [Non-destructive testing in 5 books]. M.: Vysshaya shkola, 1992. Kn. 3: Elektromagnitnyy kontrol: prakt. posobiye / pod red. V.V. Sukhorukova. 312 s.
- Bondareva V.S., Pavlova T.D. Trebovaniya k magnitoporoshkovomu kontrolyu v yevropeyskikh normakh i rossiyskikh standartakh [Requirements for magnetic particle inspection in European norms and Russian standards] // Kommentarii k standartam, TU, sertifikatam: yezhemesyachnoye prilozheniye k zhurnalu «Vse materialy. Entsiklopedicheskiy spravochnik». 2013. №11. S. 14–18.
- Shelikhov G.S. Magnitoporoshkovaya defektoskopiya detaley i uzlov Magnetic particle inspection of parts and assemblies. M.: Gos. predpriyatiye Nauch.-tekhnich. tsentr «Ekspert», 1995. 224 s.
- GOST R 56512–2015. Kontrol nerazrushayushchiy. Magnitoporoshkovyy metod. Tipovyye tekhnologicheskiye protsessy [State Standard R 56512–2015. Nondestructive control. Magnetic particle method. Typical technological processes]. M.: Standartinform, 2016. 56 s.
- ASTM E1444/E1444M-16e1. Standart practive for magnetic particle testing. ASTM International, West Conshohocken, PA, 2016. 22 p
- Pavlova T.D., Kadosov A.D., Stepanov A.V., Golovkov A.N. Vliyaniye kharakteristik magnitnykh indikatornykh materialov na chuvstvitelnost magnitoporoshkovogo kontrolya // Kommentarii k standartam, TU, sertifikatam: yezhemesyachnoye prilozheniye k zhurnalu «Vse materialy. Entsiklopedicheskiy spravochnik». 2016. №6. S. 12–15.
- HELLING Rossiya. Available at: http://www.helling-russia.ru (accessed: March 26, 2019).
- Reference block type 1 according to DIN EN ISO 9934-2. Available at: http://www.karldeutsch.de/PDF/Produktinformationen/PI%20FLUXA%20Vergleichskörper%201%206904.001%20d%20e%202017-09-06.pdf (accessed: March 26, 2019).
- Reference block type 2 according to DIN EN ISO 9934-2. Available at: http://www.karldeutsch.de/PDF/Produktinformationen/PI%20FLUXA%20Vergleichskörper%202%20d%20e%202017-08-17.pdf (accessed: March 26, 2019).
- NPTS «Kropus». Available at: http://www.kropus.com (accessed: March 26, 2019).
- Magnaflux Non-Destructive Testing Product & Equipment. Available at: https://www.magnaflux.com/Magnaflux (accessed: March 26, 2019).
- Magnetic Particle Test Bar Product Data Sheet. Available at: https://www.magnaflux.com/Files/Product-Data-Sheets/Accessories/Magnetic-Particle-Test-Bar_Product-Data-Sheet_English.pdf (accessed: March 26, 2019).
- Tool Steel Ring Product Data Sheet. Available at: https://www.magnaflux.com/Files/Product-Data-Sheets/Accessories/Tool-Steel-Ring__Product-Data-Sheet_English.pdf (accessed: March 26, 2019).
- Quantitative Quality Indicator Test Piece Shims. Available at: https://www.magnaflux.com/Files/Product-Data-Sheets/Accessories/Quantitative-Quality-Indicator-Test-Pieces_Product-Data-Sheet_English.pdf (accessed: March 26, 2019).
- Laminated Magnetic Flux Indicator Strips. Available at: https://www.magnaflux.com/Files/Product-Data-Sheets/Accessories/Magnetic-Flux-Indicators_Product-Data-Sheet_English.pdf (accessed: March 26, 2019).