Investigation of properties of coating system based on fluorine polyurethane enamel and primer with low toxical pigment content

Merkulova Yu.I., Kuznetsova V.A., Novikova T.A.
Merkulova Yu.I., Kuznetsova V.A., Novikova T.A. Investigation of properties of coating system based on fluorine polyurethane enamel and primer with low toxical pigment content // Proceedings of VIAM. 2019. No. 5. DOI: 10.18577/2307-6046-2019-0-5-68-75. URL: https://www.viam-works.ru/en/journal/2019/5/8
Keywords
fluorine polyurethane enamel, first coat, external coloring, weather-resistant, adhesion, water resistance.
Abstract

Properties of coatings system on the basis of fluorine polyurethane enamel and first coat with the lowered maintenance of toxical pigments after aging factors in comparison with domestic UR-1161 enamel and import analog of C21/100, firm AkzoNobel are investigated. It is established that after influence of factors of aging system of paintwork coatings on the basis of fluorine polyurethane enamel and universal without chromate first coat of cold drying possess high resistance to effect of aggressive fluids, to UF to radiation, high adhesive, physicomechanical and decorative properties.

Reference list
  1. . Yakovlev A.D., Yakovlev S.A. Lakokrasochnyye pokrytiya funktsionalnogo naznacheniya [Paint coatings functional purpose]. SPb.: Khimizdat, 2016. 272 s.
  2. Chebotarevskiy V.V., Kondrashov E.K. Tekhnologiya lakokrasochnogo pokrytiya v mashinostroyenii [Technology paintwork in engineering]. M: Mashinostroyeniye, 1978. 295 s.
  3. Kuznetsova V.A., Semenova L.V., Kondrashov E.K., Lebedeva T.A. Lakokrasochnye materialy s ponizhennym soderzhaniem vrednyh i toksichnyh komponentov dlya okraski agregatov i konstrukcij iz PKM [Paint-and-lacquer materials with a low content of harmful and design of polymer composite materials] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2013. №8. St. 05. Available at: http://www.viam-works.ru (accessed: April 01, 2019).
  4. Kablov E.N., Semenova L.V., Yeskov A.A., Lebedeva T.A. Kompleksnyye sistemy lakokrasochnykh pokrytiy dlya zashchity metallicheskikh i polimernykh kompozitsionnykh materialov, a takzhe ikh kontaktnykh soyedineniy ot vozdeystviya agressivnykh faktorov [Complex systems of paint and varnish coatings for protection of metal and polymer composite materials, as well as their contact compounds from the effects of aggressive factors] // Lakokrasochnyye materialy i ikh primeneniye. 2016. №6. S. 32–35.
  5. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  6. Semenova L.V., Nefedov N.I., Belova M.V., Laptev A.B. Sistemy lakokrasochnyh pokrytij dlya vertoletnoj tehniki [Systems of paint coatings for helicopter equipment] // Aviacionnye materialy i tehnologii. 2017. №4 (49). S. 56–61. DOI: 10.18577/2071-9140-2017-0-4-56-61.
  7. Semenova L.V., Malova N.E., Kuznetsova V.A., Pozhoga A.A. Lakokrasochnye materialy i pokrytiya [Paint and varnish materials and coatings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 315–327.
  8. Kuznecova V.A., Kuznecov G.V. Tendencii razvitiya v oblasti toplivostojkih lakokrasochnyh pokrytij dlya zashhity toplivnyh kesson-bakov letatelnyh apparatov (obzor) [Development trends in the field of fuel resistant paintwork coatings for protection of integral fuel tanks of aircrafts (review)] // Trudy VIAM: elektron. nauchn.-tehn. zhurn. 2014. №11. St. 08. Available at: http://www.viam works.ru (accessed: April 02, 2019). DOI: 10.18577/2307-6046-2014-0-11-8-8.
  9. Kuznetsova V.A., Semenova L.V., Shapovalov G.G. Tendentsii razvitiya v oblasti antikorrozionnykh polimernykh sostavov dlya zashchity ot korrozii krepezhnykh soyedineniy kontaktnykh par kombinirovannykh konstruktsiy (obzor) [Development trends in the field of anticorrosive polymeric systems for corrosion protection of fixing connections of contact couples of combined structures (review)] // Aviacionnye materialy i tehnologii. 2017. №1 (46). S. 25–31. DOI: 10.18577/2071-9140-2017-0-1-25-31.
  10. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Kondrashov E.K., Kozlova A.A., Malova N.E. Issledovanie kinetiki otverzhdeniya ftorpoliuretanovyh emalej alifaticheskimi poliizocianatami razlichnyh tipov [Study and curing kinetics of fluoropolyurethane enamels by the use of aliphatic polysocyanates of various types] // Aviacionnye materialy i tehnologii. 2013. №1. S. 48–49.
  12. Mitrofanova S.E. Dinamika proizvodstva poliuretanovykh lakokrasochnykh materialov na mirovom i rossiyskom rynkakh [Dynamics of production of polyurethane paints and varnishes in the world and Russian markets] // Vestnik Kazanskogo tekhnologicheskogo universiteta. 2014. №14. S. 304–305.
  13. Malova N.E., Kondrashov E.K., Vereninova N.P., Kozlova A.A. Termostoykaya atmosferostoykaya ftorpoliuretanovaya emal [Heat-resistant weatherproof fluoride polyurethane enamel] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 28–30. DOI: 10.18577/2071-9140-2014-0-S3-28-30.
  14. Kablov E.N. Marketing materialovedeniya, aviastroyeniya i promyshlennosti: nastoyashcheye i budushcheye [Marketing materials, aviation and industry: present and future] // Direktor po marketingu i sbytu. 2017. №5–6. S. 40–44.
  15. Voytovich V.A. Lakokrasochnyye materialy s ftorirovannymi komponentami [Paintwork materials with fluorinated components] // Lakokrasochnyye materialy: novinki otrasli. 2013. №4. S. 23–27.
  16. Nefyodov N.I., Semyonova L.V. Nanesenie lakokrasochnyh pokrytij metodom «syroj po syromu» [The application of paint and varnish coatings by method «crude on crude»] // Aviacionnye materialy i tehnologii. 2013. №4. S. 39–42.
  17. Semenova L.V., Rodina N.D., Nefedov N.I. Vliyanie sherohovatosti sistem lakokrasochnyh pokrytij na ekspluatacionnye svojstva samoletov [An effect of roughness of paint and varnish coating systems on service properties of aircraft] // Aviacionnye materialy i tehnologii. 2013. №2. S. 37–40.