Fast curing resins and prepregs: receiving, properties and areas of application (review)
Mishkin S.I., Malakhovskiy S.S. Fast curing resins and prepregs: receiving, properties and areas of application (review) // Proceedings of VIAM. 2019. No. 5. DOI: 10.18577/2307-6046-2019-0-5-32-40. URL: https://www.viam-works.ru/en/journal/2019/5/4
Keywords
RTM (Resin Transfer Molding), fast cure resins, fast cure prepregs, press method of forming CFRP, hardening, glass temperature.
Abstract
In article presented a review about fast curing resins and prepregs by means of which there is possibility of receiving finished product in only a few minutes is provided. Showed, that the main scopes of fast curing resins and prepregs is automotive industry, construction and transport. Showed, that such composite materials have number of advantages, including economic, by production small and large-size details. Data on the manufacturing companies are provided in article and properties of brands let out by them fast curing resins and prepregs.
Reference list
- Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials] // Polimernyye materialy i tekhnologii. 2016. T. 2. №2. S. 37–42.
- Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashchikh nanochastits v svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Prospects for the use of carbon-containing nanoparticles in binders for polymer composite materials] // Rossiyskiye nanotekhnologii. 2013. T. 8. №3–4. S. 24–42.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviaсionnye materialy i tehnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Doneckij K.I., Hrulkov A.V. Principy «zelenoj himii» v perspektivnyh tehnologiyah izgotovleniya izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing technologies of PCM articles] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 24–28.
- Hayase S., Ito T., Suzuki S., Wada M. Polymerization of cyclohexene oxide with Al(acac)3–silanol catalyst // Journal of Polymer Science. Polymer Chemistry Edition. 1981. Vol. 19. No. 10. P. 2541–2550.
- Hayase S., Ito T., Suzuki S., Wada M. Polymerization of cyclohexene oxide with aluminum complex-silanol catalysts. Part III. Dependence of catalytic activity on bulkiness of silanol and its intramolecular hydrogen bond // Journal of Polymer Science. Polymer Chemistry Edition. 1981. Vol. 19. No. 11. P. 2977–2985.
- Kamiya K., Suzuki N. A low-temperature fast curing latent catalyst microencapsulated in a porous resin structure // International Journal of Adhesion & Adhesives. 2016. Vol. 68. P. 333–340.
- Wang Y., Lakho D.A., Yao D. Effect of Additives on the rheological Properties of Fast Curing epoxy resins // Journal of Silicate Based and Composite Materials. 2015. Vol. 67. No. 4. P. 132–134.
- Xu Y.-J., Wang J., Tan Y. et al. A novel and feasible approach for one-pack flame-retardant epoxy resin with long pot life and fast curing // Chemical Engineering Journal. 2018. Vol. 337. P. 30–39.
- Zastrogina O.B., Shvets N.I., Postnov V.I., Serkova E.A. Fenolformaldegidnye svjazuyushhie novogo pokoleniya dlya materialov interera [Phenolformaldehyde binding new generation for interior materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 265–272.
- Dow Automotive Systems. VORAFORC 5300 ultra-fast cure composite epoxy system Available at: http://msdssearch.dow.com/ (accessed: October 22, 2018).
- Hexion Responsible Chemistry. Epoxy Systems for Automotive Structural Components. Available at: https://www.hexion.com/en-US/applications/composites/automotive/ structural/ (accessed: October 24, 2018).
- Solvay. Available at: https://www.solvay.com/en/press-release/solvay-launches-new-rapid-cure-resin-system-mtr-760-manufacture-new-bmw-m4-gts-hoods (accessed: October 26, 2018).
- Malnati P. Ultra-thin, preformed laminate designs enable CFRP decklid manufacture at lower-than-expected mass and at cycle times approaching mass-production speed // Composites World. 2015. Vol. 1. No. 6. P. 62–64.
- Kovalenko A.V., Tundaykin K.O., Lukina A.I., Sokolov I.I. Struktura i svoystva SMC-materialov na osnove epoksivinilefirnogo i poliefirnogo oligomerov [Structure and SMC-materials properties on the basis of epoxy blamed ethers and poly ethers oligomers] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2017. №1 (25). St. 05. Available at: http://materialsnews.ru (accessed: April 01, 2019).
- Groh F., Kappel E., Hühne C., Brymerski W. Investigation of fast curing epoxy resins regarding process induced distortions of reinforced composites // Composite Structures. 2018. Vol. 207. P. 923–934.
- Tyunina A.V. Kompozitnyye materialy: proizvodstvo, primeneniye, tendentsii rynka [Composite materials: production, application, market trends] // Polimernyye materialy. 2018. №2. S. 27–29.