Features of forming of the microstructure of the polymeric matrix in organoplasty on the basis of the multicomponent epoxy binding

Deev I.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V.
Deev I.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V. Features of forming of the microstructure of the polymeric matrix in organoplasty on the basis of the multicomponent epoxy binding // Proceedings of VIAM. 2019. No. 5. DOI: 10.18577/2307-6046-2019-0-5-22-31. URL: https://www.viam-works.ru/en/journal/2019/5/3
Keywords
organoplasty, multiphase microstructure, polymeric matrix, scanning electron microscopy, melt, epoxy binding, modifier.
Abstract

The microstructure of a polymeric matrix in organoplasty on the basis of an aramide fabric and the multicomponent epoxy binding modified by polysulphone is investigated. It is established that phase heterogeneity is peculiar to a polymeric matrix: the one-phase microdisperse structure is characteristic for a microstructure of epoxy polymer in zones with dense packing of fibers (in a thread); the two-phase structure is characteristic for a microstructure of the epoxy polymer modified by polysulphone, in zones with less dense packing of fibers (between threads and fabric layers). With researches of a microstructure it is confirmed that when manufacturing the organoplasty on the basis of an aramide fabric and the meltable multicomponent epoxy binding happens redistribution of components of a reinforcing filler binding in interfiber space to a primary arrangement of polysulphone between threads and the fabric layers, bringing to formation of two-phase structure.

Reference list
  1. Kablov E.N. Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii: sb. nauch.-inform. materialov. 3-e izd., pererab. i dop. [Trends and benchmarks of innovative development of Russia: collection of scientific-information materials. 3rd ed., rev. and add.]. M.: VIAM, 2015. 720 s.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya // Redkiye zemli. 2014. №3. S. 8–13.
  3. Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Kablov E.N. Sovremennyye materialy – osnova innovatsionnoy modernizatsii Rossii [Modern materials – the basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  5. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  6. Tikhonov I.V., Tokarev A.V., Shorin S.V. et al. Russian aramid fibres: past–present–future // Fibre Chemistry. 2013. No. 5. P. 1–8.
  7. Zimon A.D. Adgeziya plenok i pokrytiy [Adhesion of films and coatings]. M.: Khimiya, 1977. 352 s.
  8. Summ B.D., Goryunov Yu.V. Fiziko-khimicheskiye osnovy smachivaniya i rastekaniya [Physico-chemical basis of wetting and spreading]. M.: Nauka, 1976. 232 s.
  9. Derombise G., Chailleux E., Forest B. et al. Long-term mechanical behavior of aramid fibers in seawater // Polymer Engineering & Science. 2011. Vol. 51. No. 7. P. 1366–1375.
  10. De Ruijter C., Jager W.F., Li L., Picken S.J. Lyotropic rod-coil poly (amide-block-aramid) alternating block copolymers: phase behavior and structure // Macromolecules. 2006. Vol. 39. No. 13. P. 4411–4417.
  11. Derombise G., Vouyovitch Van Schoors L., Davies P. Degradation of aramid fibers under alkaline and neutral conditions: Relations between the chemical characteristics and mechanical properties // Journal of Applied Polymer Science. 2010. Vol. 116. No. 5. P. 888–898.
  12. Deyev I.S., Kurshev Ye.V., Lonskiy S.L., Zhelezina G.F. Vliyaniye dlitel'nogo klimaticheskogo stareniya na mikrostrukturu poverkhnosti epoksidnykh organoplastikov i kharakter yeye razrusheniya v usloviyakh izgiba [The effect of long-term climatic aging on the microstructure of the surface of epoxy organic plastics and the nature of its destruction under bending conditions] // Voprosy materialovedeniya. 2016. №3 (87). S. 104–114.
  13. Zhelezina G.F., Gulyaev I.N., Soloveva N.A. Aramidnye organoplastiki novogo pokoleniya dlya aviacionnyh konstrukcij [Aramide organic plastics of new generation for aviation designs] // Aviacionnye materialy i tehnologii. 2017. №S. S. 368–378. DOI: 10.18577/2071-9140-2017-0-S-368-378.
  14. Bielawski R. Composite materials in military aviation and selected problems with implementation // Review of the Air Force Academy. 2017. No. 1 (33). P. 11–16.
  15. Voynov S.I., Zhelezina G.F., Solovyeva N.A., Yamshchikova G.A. Vliyaniye vneshney sredy na svoystva organoplastika, poluchennogo metodom propitki pod davleniyem (RTM) [Environmental effects on properties of aramid fiber reinforced plastic manufactured by RTM method] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 72–78. DOI: 10.18577/2071-9140-2015-0-4-72-78.
  16. Shuldeshova P.M., Zhelezina G.F. Aramidnyj sloisto-tkanyj material dlya zashhity ot ballisticheskih i udarnyh vozdejstvij [The aramid layered and woven material for protection against impact and ballistic influences] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №9. St. 06. Available at: http://www.viam-works.ru (accessed: March 04, 2019). DOI: 10.18577/2307-6046-2014-0-9-6-6.
  17. Deyev I.S., Kobets L.P., Novikov V.U., Kozitskiy D.V. Vliyaniye nekotorykh parametrov tekhnologii na strukturoobrazovaniye polimernoy matritsy v kompozitakh [The influence of some technology parameters on the structure formation of the polymer matrix in composites] // Materialovedeniye. 2002. №9. S. 10–21.
  18. Kulagina G.S., Korobova A.V., Ilichev A.V., Zhelezina G.F. Fizicheskiye i fiziko-mekhanicheskiye svoystva antifriktsionnogo organoplastika na osnove kombinirovannogo tkanogo napolnitelya i epoksidnogo svyazuyushchego [Physical and physico-mechanical properties of antifriction organoplastics based on combined fabric filler and epoxy binder] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №10 (58). St. 08. Available at: http://www.viam-works.ru (accessed: March 11, 2019). DOI: 10.18577/2307-6046-2017-0-10-8-8.
  19. Li C.S., Zhan M.S., Huag X.C. et al. Hydrothermal aging mechanisms of aramid fibers via synchrotron small-angle X-ray scattering and dynamic thermal mechanical analysis // Journal of Applied Polymer Science. 2013. Vol. 128. No. 2. P. 1291–1296.
  20. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  21. Kablov E.N. Marketing materialovedeniya, aviastroyeniya i promyshlennosti: nastoyashcheye i budushcheye [Marketing materials, aviation and industry: present and future] // Direktor po marketingu i sbytu. 2017. №5–6. S. 40–44.
  22. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: March 04, 2019). DOI: 10.18577/2307-6046-2014-0-7-6-6.