Influence of corrosion environmental parameters on properties of constructional metal materials while testing in sea water (review)
Varchenko E.A., Kurs M.G. Influence of corrosion environmental parameters on properties of constructional metal materials while testing in sea water (review) // Proceedings of VIAM. 2019. No. 5. DOI: 10.18577/2307-6046-2019-0-5-85-93. URL: https://www.viam-works.ru/en/journal/2019/5/10
Keywords
corrosion, biological resistance of materials, fouling, sea tests, tests in moving sea water.
Abstract
The analysis of domestic and foreign experience of methods of testing materials in sea water. It has been shown that the following materials should be used in determining the characteristics of materials during operation in seawater: testing materials in a water flow moving with variable speed in order to identify the motor-electric effect and cavitation; testing materials in the period of wetting and in the near-surface water layers to determine the effect on materials resistance to aeration; biological resistance testing of materials to determine the degree of fouling and the degree of destruction of materials in a given water area.
Reference list
- Laptev A.B., Bugay D.E., Aleksandrov A.A., Larionov V.I. Ekologicheskiye i biologicheskiye faktory vozdeystviya na slozhnyye tekhnicheskiye sistemy [Ecological and biological factors affecting complex technical systems] // Bezopasnost v tekhnosfere. 2017. T. 6. №4. S. 21–30.
- Laptev A.B., Kolpachkov E.D., Kurs M.G., Lebedev M.P., Lutsenko A.N. Razrabotka metodiki opredeleniya resursa ekspluatatsii konstruktsiy iz polimernykh kompozitsionnykh materialov [Development of methods for determining the service life of structures made of polymer composite materials] // Plasticheskiye massy. 2018. №9–10. S. 36–40.
- Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metallomatrichnye kompozicionnye materialy na osnove Al–SiC [Metalmatrix composite materials on the basis of Al–SiC] // Aviacionnye materialy i tehnologii. 2012. №S. S. 373–380.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
- Kurs M.G., Karimova S.A. Naturno-uskorennye ispytaniya: osobennosti metodiki i sposoby ocenki korrozionnyh harakteristik alyuminievyh splavov [Salt-accelerated outdoor corrosion testing: methodology and evaluation of corrosion susceptibility of aluminum alloy] // Aviacionnye materialy i tehnologii. 2014. №1. S. 51–57. DOI: 10.18577/2071-9140-2014-0-1-51-57.
- Korogodova I.V., Boyko I.N. Aktualnye problemy zashchity dvigateley ot vozniknoveniya korrozii, ekspluatiruyemykh na samoletakh v morskikh usloviyakh i baziruyushchikhsya na pribrezhnykh aerodromakh [Actual problems of protecting engines against the occurrence of corrosion, operated on airplanes in marine conditions and based on coastal airfields] // Potentsial sovremennoy nauki. 2015. №1 (9). S. 25–31.
- Varchenko E.A., Kurs M.G. Naturnyye ispytaniya metallicheskikh materialov v morskoy vode: klyuchevyye podkhody k otsenke stoykosti k korrozii i biopovrezhdeniyu [Natural tests of metal materials in sea water: key approaches to estimation of resistance to corrosion and biodeterioration] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №11 (59). St. 12. Available at: http://www.viam-works.ru (accessed: November 15, 2018). DOI: 10.18577/2307-6046-2017-0-11-12-12.
- Laptev A.B., Lutsenko A.N., Kurs M.G., Bukharev G.M. Opyt issledovaniy biokorrozii metallov [Experience in the study of the biocorrosion of metals] // Praktika protivokorrozionnoy zashchity. 2016. №2 (80). S. 36–57.
- Bukharev G.M., Laptev A.B., Yakovenko T.V., Bobyreva T.V. Rol otsenki biologicheskogo faktora v obespechenii bezopasnoy ekspluatatsii slozhnykh tekhnicheskikh sistem v techeniye zhiznennogo tsikla [The role of the assessment of the biological factor in ensuring the safe operation of complex technical systems during the life cycle] // Klimat-2017. Problemy otsenki klimaticheskoy stoykosti materialov i slozhnykh tekhnicheskikh sistem: sb. dokl. II Vseros. nauch.-tekhnich. konf. M.: VIAM, 2017. S. 21–30 (CD).
- Kovalchuk Yu.L., Ilin I.N., Poltarukha O.P. O nekotorykh osobennostyakh raspredeleniya organizmov obrastaniya na sudakh i buykovykh stantsiyakh v morskoy srede [On some features of the distribution of fouling organisms on ships and buoy stations in the marine environment] // Voda: khimiya i ekologiya. 2012. №3. S. 59–64.
- Morskaya korroziya: spravochnik. Per. s angl. / pod red. M. Shumakhera [Marine corrosion: a handbook. Line from Engl/ / ed. M. Schumacher]. M.: Metallurgiya, 1983. 512 s.
- Nemtseva E.P., Suprun L.A., Feldman L.A. i dr. Spravochnik sudoremontnika-korpusnika [andbook of ship repairmen-corps]. M.: Transport, 1970. 320 s.
- Arkhangorodskiy A.G., Rozendent B.YA., Semenov L.N. Prochnost i remont korpusov promyslovykh sudov [Durability and repair of hulls of fishing vessels]. L.: Sudostroyeniye, 1982. 272 s.
- Mikheyev A.I. Vliyaniye obrastaniya i nizkikh temperatur na bezopasnuyu ekspluatatsiyu sudov [Influence of fouling and low temperatures on the safe operation of ships] // Vodnyy transport. 2013. Vyp. 3. S. 56–61.
- Shkabara N.A. Ekologo-tekhnologicheskoye izucheniye pokrytiya bar'yernogo tipa dlya zashchity ot korrozii i morskogo obrastaniya neftegazoprovodov, plavuchikh sredstv i portovykh sooruzheniy (na primere Gelendzhikskoy bukhty): avtoref. dis. … kand. tekhn. nauk cological and technological study of barrier-type coatings for protection against corrosion and marine fouling of oil and gas pipelines, floating facilities and port facilities (using the example of Gelendzhik Bay): thesis, Cand. Sc. (Tech.). Krasnodar. 2015. 113 s.
- Petrova N.E., Bayeva L.S. Biokorroziya korpusov sudov [Biocorrosion of ship hulls] // Vestnik MGTU. 2006. T. 9. №5. S. 890–892.
- Laptev A., Kurs M., Lonskaya N., Davydov D., Averina A. Investigation of corrosion damage of hydration aluminium alloys at full-scale accelerated tests // International Journal of Engineering & Technology. 2018. Vol. 7 (4). P. 5061–5066.
- Laptev A.B., Navalikhin G.P. Povysheniye bezpasnosti ekspluatatsii promyslovykh nefteprovodov [Improving the safety of operating oil pipeline] // Neftepromyslovoye delo. 2006. №1. S. 48–52.
- Sadawy M.M., Heseinov R.Q., Shirinov T.I. Corrosion and electrochemical behavior of austenitic-ferritic stainless steel in sulfuric acid // Neftin, qazm geotexnoloji problemlari va kimya. ET§ Elmi asarlarig Bakig. 2009. P. 327–332.
- Sharifov Z.Z. Ways of Increase of corrosion resistance provider materials // Journal of Metallurgy. 2002. Vol. 8. Is. 2. P. 7.
- Sadawy M.M., Shirinov T.I., Heseinov R.Q. The effect of heat treatment on the corrosion and electrochemical properties of ferric-austenitic stainless steel in sulfuric acid soluteon // Tr. Mezhdunar. foruma «Nauka i inzhenernoye obrazovaniye bez granits». Almaty: KazNTU im. K.I. Satpayeva, 2009. T. 1. S. 496–499.
- Sharifov Z.Z. Improvement of a corrosion stability of composite materials on the ferrum’s base. International valium of scientific lab our // Progressive Technology and Machine building systems. 2002. Vol. 19. P. 7.
- Bashirov F.R. Korrozionnoye povedeniye svarnykh soyedineniy iz stali RSD32 v kaspiyskoy morskoy vode [Corrosion behavior of welded joints made of RSD32 steel in the Caspian sea water] // Vestnik MGU. Ser.: Sudostroyeniye i sudoremont. 2014. T. 64. S. 5.
- Starokon I.V. O vliyanii korrozionnogo vozdeystviya na razvitiye ustalostnykh treshchin na morskikh neftegazovykh sooruzheniyakh (MNGS) [On the effect of corrosive effects on the development of fatigue cracks in offshore oil and gas structures (MNGS)] // Fundamentalnyye issledovaniya. 2012. №11-5. S. 1214–1219.
- Markovich R.A., Kan M.K., Mikhaylov S.V. Korroziya i metody zashchity zony peremennogo smachivaniya metallokonstruktsiy gidrotekhnicheskikh sooruzheniy estakadnogo tipa [Corrosion and methods of protection of the zone of variable wetting of metal structures of hydraulic structures of an overpass type] // Gidrotekhnika. 2014. №4. S. 71.
- Lyublinskiy E.Ya. Korroziya i zashchita sudov: spravochnik [Corrosion and protection of ships: a guide]. L.: Sudostroyeniye, 1987. 376 s.
- RD31.28.10–97. Kompleksnyye metody zashchity sudovykh konstruktsiy ot korrozii [Guidance document 31.28.10–97. Complex methods of protection of ship structures against corrosion]. L.: TSNIIMF, 1997. 122 s.
- Sorokin A.I. Issledovaniye protsessa razrusheniya alyuminiyevogo splava ot kontaktnoy korrozii v vysokoskorostnom potoke morskoy vody [Investigation of the process of destruction of aluminum alloy from contact corrosion in a high-speed flow of sea water] // Vísnik SevNTU. 2012. Ser.: Mekhaníka, energetika, ekologíya. Vip. 132. S. 135–141.
- Sorokín A.Í. Parametri yelektrokhímíchnogo zakhistu sudnobudívnikh metalív víd kontaktnoí̈ korozíí̈ [Electric parametric parameters for shipwreck metal metals in contact corrosion] // Zb. nauk. prats SVMÍ. Sevastopol, 2006. Vip. 1 (9). S. 78–84.
- Vaganov A.M. Proyektirovaniye skorostnykh sudov [Design of high-speed vessels]. L.: Sudostroyeniye, 1978. 279 s.
- Podgornyy Yu.I., Sorokin A.I. Korrozionno-erozionnaya stoykost' i elektrokhimicheskoye povedeniye nekotorykh sudostroitelnykh splavov v bystrodvizhushcheysya morskoy vode [Corrosion-erosion resistance and electrochemical behavior of some shipbuilding alloys in high-speed seawater] // Sostoyaniye i perspektivy sozdaniya i vnedreniya korrozionnostoykikh materialov, sredstv i metodov protivokorrozionnoy zashchity sudov: tez. dokl. vtorogo nauch.-tekhn. soveshchaniya (Leningrad, dek. 1982 g.). L., 1982. S. 53–55.
- Morrow S.J. Materials selection for seawater pumps // Proceedings of the 26 International Pump Users Symposium, 2010. P. 73–80.
- Melchers R.E. Effect of temperature on the marine immersion corrosion of carbon steels // Corrosion (NACE). 2002. Vol. 58 (9). P. 768–782.