Fiber-matrix adhesion strength measurement using nanoindentation (review)

Gulyaev A.I.
Gulyaev A.I. Fiber-matrix adhesion strength measurement using nanoindentation (review) // Proceedings of VIAM. 2019. No. 3. DOI: 10.18577/2307-6046-2019-0-3-68-78. URL: https://www.viam-works.ru/en/journal/2019/3/8
Keywords
fiber composite, polymer composite material, adhesion, interface, interphase, boundary interaction, indentation, push-out test.
Abstract

The review briefly reviewed the applied methods for determining the fiber-matrix adhesive strength. The main emphasis is on measuring the adhesive strength by the single fiber push-out method using instrumental micro- and nanoindentation. The issues of informativeness of this approach, modeling of the process of pushing the fiber by the indenter, the stress state in this process are considered. Attention is paid to the methods of testing, in particular, the features of sample preparation, the geometry of the indenters used, loading conditions.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally evrazii. 2015. №1. S. 36–39.
  3. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviaсionnye materialy i tehnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  4. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. Vysokotemperaturnye metallomatrichnye kompozicionnye materialy, armirovannye chasticami i voloknami tugoplavkih soedinenij [High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds] // Aviacionnye materialy i tehnologii. 2017. №S. S. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  5. Hughes J.D.H. The carbon fibre/epoxy interface – a review // Composites Science and Technology. 1991. Vol. 41. P. 13–45.
  6. Kim J.-K., Mai Y.-W. Engineered Interfaces in Fiber Reinforced Composites. Oxford: Elsevier, 1998. 486 р.
  7. Kinlok E. Adgeziya i adgezivy: nauka i tekhnologiya [Adhesion and adhesives: science and technology]. M.: Mir, 1991. 484 s.
  8. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.Ye., Rubtsova E.V., Petrova A.P. Issledovaniye epoksidno-polisul'fonovykh polimernykh sistem kak osnovy vysokoprochnykh kleyev aviatsionnogo naznacheniya [Study of epoxy-polysulfone polymer systems as the basis for high-strength aviation-grade adhesives] // Klei. Germetiki. Tekhnologii. 2017. №3. S. 7–12.
  9. Kuperman A.M., Gorbatkina Yu.A., Turusov R.A. Vysokoprochnyye armirovannyye plastiki [High-strength reinforced plastics] // Khimicheskaya fizika. 2012. №8. S. 50–59.
  10. Yakhyayeva Kh.Sh., Zaikov G.Ye., Deberdeyev T.R., Ulitin N.V. i dr. Strukturnyye osnovy mezhfaznoy adgezii (nanoadgezii) v polimernykh kompozitakh [Structural fundamentals of interfacial adhesion (nanoadhesion) in polymer composites] // Vestnik Kazanskogo tekhnologicheskogo universiteta. 2012. №5. S. 68–70.
  11. Kozlov G.V., Burya A.I., Aloyev V.Z., Yanovskiy Yu.G. Strukturnyy aspekt mezhfaznoy adgezii v ugleplastikakh [Structural aspect of interfacial adhesion in carbon plastics] // Fizicheskaya mezomekhanika. 2005. №2. S. 35–38.
  12. Gulyayev A.I., Petrova A.P., Zaytsev D.V., Rayevskikh A.N. Mikrostrukturnyy i fraktograficheskiy analiz kleyevogo soyedineniya, vypolnennogo epoksidno-kauchukovym kleyem VK-27 s podsloyem fenolokauchukovogo kleya VK-25 [Microstructural and fractographic analysis of adhesive bonding made with epoxy-rubber glue VK-27 with a sublayer of phenocrystalline glue VK-25] // Klei. Germetiki. Tekhnologii. 2018. №6. C. 14–20.
  13. Guigon M., Klinklin E. The interface and interphase in carbon fibre-reinforced composites // Composites. 1994. Vol. 25. P. 534–539.
  14. Gao S.-L., Mader E., Zhandarov S.F. Carbon fibers and composites with epoxy resins: Topography, fractography and interphases // Carbon. 2004. Vol. 42. P. 515–529.
  15. Garifullin A.R., Abdullin I.Sh. Sovremennoye sostoyaniye problemy poverkhnostnoy obrabotki uglerodnykh volokon dlya posleduyushchego ikh primeneniya v polimernykh kompozitakh v kachestve armiruyushchego elementa [The current state of the problem of surface treatment of carbon fibers for their subsequent use in polymer composites as a reinforcing element] // Vestnik Kazanskogo tekhnologicheskogo universiteta. 2014. №7. S. 80–85.
  16. Nelyub V.A., Belov P.A. Metody povysheniya stoykosti ugleplastikov k delaminatsii za schet upravleniya adgeziyey volokna k matritse [Methods to improve the resistance of carbon fiber to delamination by controlling the adhesion of the fiber to the matrix] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2013. №5. St. 03. Available at: http://www.materialsnews.ru (accessed: January 25, 2019).
  17. Karger-Kocsis J., Mahmood H., Pegoretti A. Recent advances in fiber/matrix interphase engineering for polymer composites // Progress in Materials Science. 2015. Vol. 73. P. 1–43.
  18. Liu L., Jia C., He J. et al. Interfacial characterization, control and modification of carbon fiber reinforced polymer composites // Composites Science and Technology. 2015. Vol. 121. P. 56–72.
  19. Kuznetsova V.A., Deev I.S., Semenova L.V. Vliyanie modifikacii epoksidnyh plenkoobrazuyushhih kompozicij na ih fazovuyu mikrostrukturu i adgeziyu k alyuminievomu splavu [Influence of modification of epoxy film-forming compositions on their phase microstructure and adgesion to aluminium alloy] // Aviacionnye materialy i tehnologii. 2016. №1. S. 72–78. DOI: 10.18577/2071-9140-2016-0-1-72-78.
  20. Kobets L.P., Deyev I.S. Strukturoobrazovaniye v termoreaktivnykh svyazuyushchikh i matritsakh kompozitsionnykh materialov na ikh osnove [Structure formation in thermosetting binders and matrices of composite materials based on them] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 67–78.
  21. Gulyaev A.I., Shurtakov S.V. Kolichestvennyj analiz mikrostruktury granichnogo sloya «volokno–matrica» v ugleplastikah [Quantitative analysis of fiber–matrix interface microstructure in carbon composites] // Trudy VIAM: elektron. nauch.-tehnich. zhurnal. 2016. №7. St. 08. Available at: http://www.viam-works.ru (accessed: January 25, 2019). DOI: 10.18577/2307-6046-2016-0-7-8-8.
  22. Wu Q., Li M., Gu Y. et al. Nano-analysis on the structure and chemical composition of the interphase region in carbon fiber composite // Composites: Part A. 2014. Vol. 56. P. 143–149.
  23. Munz M., Sturm H., Schulz E., Hinrichsen G. The scanning force microscope as a tool for the detection of local mechanical properties within the interphase of fibre reinforced polymers // Composites Part A. 1998. Vol. 29A. P. 1251–1259.
  24. Downing T.D., Kumar R., Cross W.M. et al. Determining the interphase thickness and properties in polymer matrix composites using phase imaging atomic force microscopy and nanoindentation // Journal of Adhesion Science and Technology. 2000. Vol. 14. P. 1801–1812.
  25. Gu Y., Li M., Wang J., Zhang Z. Characterization of the interphase in carbon fiber/polymer composites using a nanoscale dynamic mechanical imaging technique // Carbon. 2010. Vol. 48.
  26. P. 3229–3235.
  27. Niu Y.-F., Yang Y., Gao S., Yao J.-W. Mechanical mapping of the interphase in carbon fiber reinforced poly(ether-ether-ketone) composites using peak force atomic force microscopy: Interphase shrinkage under coupled ultraviolet and hydro-thermal exposure // Polymer Testing. 2016. Vol. 55. P. 257–260.
  28. Afaghi-Khatibia A., Mai Y.-W. Characterisation of fibre/matrix interfacial degradation under cyclic fatigue loading using dynamic mechanical analysis // Composites: Part A. 2002. Vol. 33. P. 1585–1592.
  29. Магомедов Г.М., Яхьяева Х.Ш., Козлов Г.В. Молекулярная подвижность и межфазные явления в композитах эпоксиполимер/стекловолокно // Известия ДГПУ. 2013. №4. С. 16–19.
  30. Thomason J.L. Investigation of composite interphase using dynamic mechanical analysis: artifacts and reality // Polymer Composites. 1990. Vol. 11. P. 105–113.
  31. Tsai H.C., Arocho A.M., Gause L.W. Prediction of fiber-matrix interphase properties and their influence on interface stress, displacement and fracture toughness of composite material // Materials Science and Engineering, 1990. Vol. A126. P. 295–304.
  32. Gohil P.P., Shaikh A.A. Analytical investigation and comparative assessment of interphase influence on elastic behavior of fiber reinforced composites // Journal of Reinforced Plastics and Composites. 2010. Vol. 29. P. 685–699.
  33. Turusov R.A., Manevich L.I. Contact layer method: Determining parameters of rigidity and true strength of an adhesion bond for a contact layer // Polymer Science. Series D. 2011. Vol. 4. P. 1–4.
  34. Erasov V.S., Makarycheva A.I. Opredelenie modulya uprugosti mezhfaznoj zony v sloistom polimernom kompozicionnom material [Determination of the elastic modulus of the interphase zone in a layered polymer composite material] // Aviacionnye materialy i tehnologii. 2014. №2. S. 53–55. DOI: 10.18577/2071-9140-2014-0-2-53-55.
  35. Williams J.G., Donnellan M.E., James M.R., Morris W.L. Properties of the interphase in organic matrix composites // Materials Science and Engineering. 1990. Vol. A126. P. 305–312.
  36. Lee S.-H., Wang S., Pharr G.M., Xu H. Evaluation of interphase properties in a cellulose fiber-reinforced polypropylene composite by nanoindentation and finite element analysis // Composites: Part A. 2007. Vol. 38. P. 1517–1524.
  37. Hardiman M., Vaughan T.J., McCarthy C.T. Fibrous composite matrix characterisation using nanoindentation: The effect of fibre constraint and the evolution from bulk to in-situ matrix properties // Composites: Part A. 2015. Vol. 68. P. 296–303.
  38. Hardiman M., Vaughan T.J., McCarthy C.T. A review of key developments and pertinent issues in nanoindentation testing of fibre reinforced plastic microstructures // Composite Structures. 2017. Vol. 180. P. 782–798.
  39. Herrera-Franco P.J., Drzal L.T. Comparison of methods for the measurement of fibre/matrix adhesion in composites // Composites. 1992. Vol. 23. P. 2–27.
  40. Zhandarov S., Mader E. Characterization of fiber/matrix interface strength: applicability of different tests, approaches and parameters // Composites Science and Technology. 2005. Vol. 65. P. 149–160.
  41. Gorbatkina Yu.A., Sopotov R.I., Gorbunova I.Yu. i dr. Sravneniye razlichnykh metodov otsenki prochnosti soyedineniy modifitsirovannyy epoksidnyy polimer–tverdoye telo [Comparison of Different Methods for Assessing the Strength of Compounds, Modified Epoxy Polymer–Solid] // Klei. Germetiki. Tekhnologii. 2015. №1. S. 16–20.
  42. Gorbatkina Yu.A. Adgezionnaya prochnost v sistemakh polimer–volokno [Adhesive strength in polymer–fiber systems]. M.: Khimiya, 1987. 192 s.
  43. Akhmatova O.V., Gorbatkina Yu.A., Gorbunova I.Yu. i dr. Vliyaniye nanorazmernykh chastits gliny i termoplastichnogo modifikatora na adgezionnuyu prochnost' soyedineniy epoksiaminnogo svyazuyushchego s voloknami [The effect of nanoscale clay particles and a thermoplastic modifier on the adhesion strength of epoxy-amine binder compounds with fibers] // Plasticheskiye massy. 2012. №10. S. 31–35.
  44. Gorbatkina Yu.A., Ivanova-Mumzhiyeva V.G., Kuperman A.M. Adgeziya modifitsirovannykh epoksidnykh matrits k armiruyushchim voloknam [Adhesion of modified epoxy matrices to reinforcing fibers] // Vysokomolekulyarnyye soyedineniya. Ser.: A. 2016. №5. S. 439–447.
  45. Gorbatkina Yu.A., Zhuravleva O.A., Ivanova-Mumzhiyeva V.G., Chebotarev V.P. Vliyaniye molekulyarnoy massy polisulfona na adgeziyu epoksipolisul'fonovykh svyazuyushchikh k voloknam [The effect of polysulfone molecular weight on the adhesion of epoxy-polysulfone binders to fibers] // Plasticheskiye massy. 2017. №5–6. S. 14–17.
  46. Baurova N.I., Sergeyev A.Yu. Strukturnyye issledovaniya mekhanizma razrusheniya kleyevykh soyedineniy posle ispytaniy metodom pull-out [Structural studies of the mechanism of destruction of adhesive joints after pull-out tests] // Klei. Germetiki. Tekhnologii. 2014. №4. S. 24–28.
  47. Sergeyev A.Yu., Turusov R.A., Baurova N.I. Opredeleniye adgezionnoy prochnosti soyedineniy na primere ispytaniy obraztsov metodom vydergivaniya volokon iz matritsy [Determination of adhesion strength of compounds by the example of sample testing by pulling fibers from the matrix] // Kompozity i nanostruktury. 2017. №1. S. 52–62.
  48. Kotomin S.V. Otsenka prochnosti adgezionnoy svyazi volokno–termoplastichnaya matritsa metodom petli [Evaluation of the strength of the adhesive bond fiber–thermoplastic matrix by the loop method] // Inzhenernyy zhurnal: nauka i innovatsii. 2015. №12 (48). St. 05. Available at: http://engjournal.ru (accessed: January 25, 2019).
  49. Tandon G.P., Pagano N.J. Micromechanical analysis of the fiber push-out and re-push test // Composites Science and Technology. 1998. Vol. 58. P. 1709–1725.
  50. Bechel V.T., Sottos N.R. A comparison of calculated and measured debond lengths from fiber push-out tests // Composites Science and Technology. 1998. Vol. 58. P. 1727–1739.
  51. Zidi M., Carpentier L., Chateauminois A., Sidoroff F. Quantitative analysis of the micro-indentation behaviour of fibre-reinforced composites: development and validation of an analytical model // Composites Science and Technology. 2000. Vol. 60. P. 429–437.
  52. Zidi M., Carpentier L., Chateauminois A., Kapsa P., Sidoroff F. Development of a micro-indentation model simulating different mechanical responses of the fibre/matrix interface // Composites Science and Technology. 2001. Vol. 61. P. 369–375.
  53. Chandra N., Ghonem H. Interfacial mechanics of push-out tests: theory and experiments // Composites: Part A. 2001. Vol. 32. P. 575–584.
  54. Hardiman M., Vaughan T.J., McCarthy C.T. The effect of fibre constraint in the nanoindentation of fibrous composite microstructures: A finite element investigation // Computational Materials Science. 2012. Vol. 64. P. 162–167.
  55. Hu Z., Farahikia M., Delfanian F. Fiber bias effect on characterization of carbon fiber-reinforced polymer composites by nanoindentation testing and modeling // Journal of Composite Materials. 2015. Vol. 49. P. 3359м72.
  56. Wang S.-W., Khan A., Sands R., Vasudevan A.K. A novel nanoindentor technique for measuring fibre-matrix interfacial strengths in composites // Journal of Materials Science Letters. 1992. Vol. 11. P. 739–741.
  57. Desaeger M., Verpoest I. On the use of the micro-indentation test technique to measure the interfacial shear strength of fibre-reinforced polymer composites // Composites Science and Technology. 1993. Vol. 48. P. 215–226.
  58. Janczak J., Burki G., Rohr L. Interfacial characterisation of MMCs and CMCs using SEM-pushout technique // Key Engineering Materials. 1997. Vol. 127–131. P. 623–630.
  59. Haeberle D.C. The use of nanoindentation to determine composite interfacial shear strength and the effects of environmental aging: Thesis for the degree of Master of Science in Engineering Science and Mechanics. Blacksburg, 2001. 112 p.
  60. Chawla N., Chawla K.K., Koopman M. et al. Thermal-shock behavior of a Nicalon-fiber-reinforced hybrid glass-ceramic composite // Composites Science and Technology. 2001. Vol. 61. P. 1923–1930.
  61. Kumar R., Cross W.M., Kjerengtroen L., Kellar J.J. Fiber bias in nanoindentation of polymer matrix composites // Composite Interfaces. 2004. Vol. 11. P. 431–440.
  62. Urena A., Rams J., Escalera M.D., Sanchez M. Characterization of interfacial mechanical properties in carbon fiber/aluminium matrix composites by the nanoindentation technique // Composites Science and Technology. 2005. Vol. 65. P. 2025–2038.
  63. Tezcan J., Ozcan S., Gurung B., Filip P. Measurement and analytical validation of interfacial bond strength of PAN-fiber-reinforced carbon matrix composites // Journal of Materials Science. 2008. Vol. 43. P. 1612–1618.
  64. Molina-Aldareguia J.M., Rodriguez M., Gonzalez C., LLorca J. An experimental and numerical study of the influence of local effects on the application of the fibre push-in test // Philosophical Magazine. 2011. Vol. 91. P. 1293–1307.
  65. Mueller W.M., Moosburger-Will J., Sause M.G.R., Horn S. Microscopic analysis of single-fiber push-out tests on ceramic matrix composites performed with Berkovich and flat-end indenter and evaluation of interfacial fracture toughness // Journal of the European Ceramic Society. 2013. Vol. 33. P. 441–451.
  66. Jager J., Sause M.G.R., Burkert F. et al. Influence of plastic deformation on single-fiber push-out tests of carbon fiber reinforced epoxy resin // Composites: Part A. 2015. Vol. 71. P. 157–167.
  67. Zhang L., Ren C., Zhou C., Xu H., Jin X. Single fiber push-out characterization of interfacial mechanical properties in unidirectional CVI-C/SiC composites by the nano-indentation technique // Applied Surface Science, 2015. Vol. 357. P. 1427–1433.
  68. Gallo S.C., Li X., Zhang Z., Charitidis C., Dong H. Viscoelastic response of carbon fiber reinforced polymer during push-out tests // Composites Part A. 2018. Vol. 112. P. 178–185.