Approbation of tape sealant for sealing removable constructive elements operable at temperatures from -60 to +180°С

Krasnov L.L., Kirina Z.V., Venediktova M.A., Bryk Ya. А.
Krasnov L.L., Kirina Z.V., Venediktova M.A., Bryk Ya. А. Approbation of tape sealant for sealing removable constructive elements operable at temperatures from -60 to +180°С // Proceedings of VIAM. 2019. No. 3. DOI: 10.18577/2307-6046-2019-0-3-53-60. URL: https://www.viam-works.ru/en/journal/2019/3/6
Keywords
tape sealan, silicone elastomer, hydrophobic liquid, physicomechanical properties, relative compressive strain, bolted connection.
Abstract

The short description of process of manufacturing of tape sealant is provided in article. Physicomechanical properties of tape sealant are defined, have been defined, dependence of way of forming of joint of tape hermetic has been investigated at assembly of pressurized compartments. Relative deformation at compression of hermetic tape, residual relative deformation after compression is established. Degree of fit of the tape sealant to interfaced surfaces in different combinations of materials: «aluminum–PCM» with two-row and single-row bolted, «aluminum–organic glass» with two-row bolted.

Reference list
  1. Kablov E.N. Klyuchevaya problema – materialy [The key problem is materials] // Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. M.: VIAM, 2015. S. 458–464.
  2. Kablov E.N. Khimiya v aviatsionnom materialovedenii [Chemistry in Aviation Materials Science] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  4. Shvetsov G.V., Akimova D.U., Baryshnikova M.D. Tekhnologiya pererabotki plasticheskikh mass [Plastics processing technology]. M.: Khimiya, 1988. 512 s.
  5. Mak-Kelvi D.M. Pererabotka polimerov. Per. s angl. [Polymer processing. Trans. from Engl.]. M.: Khimiya, 1965. 444 s.
  6. Koshelev F.F., Kornev A.E., Bukanov A.M. Obshchaya tekhnologiya rezin [General technology of rubber]. M.: Khimiya, 1978. S. 321–327.
  7. Kryzhanovskiy V.K., Kerber M.L. Polimernyye kompozitsionnyye materialy: struktura, svoystva, materialy [Polymer composite materials: structure, properties, materials]. SPb.: Professiya, 2008. 560 s.
  8. Kryzhanovskiy V.K., Kerber M.L., Burlov V.V., Panimatchenko A.D. Proizvodstvo izdeliy iz polimernykh materialov [Production of products from polymeric materials]. SPb.: Professiya, 2004. 464 s.
  9. Savenkova A.V., Chursova L.V., Eliseev O.A., Glazov P.A. Germetiki aviacionnogo naznacheniya [Hermetics of aviation assignment] // Aviacionnye materialy i tehnologii. 2012. №3. S. 40–43.
  10. Eliseev O.A., Naumov I.S., Smirnov D.N., Bryk Ya.A. Reziny, germetiki i ogne-teplozashhitnye materialy [Rubbers, sealants, fireproof and heat-shielding materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 437–451. DOI: 10.18577/2071-9140-2017-0-S-437-451.
  11. Savenkova A.V., Chursova L.V., Eliseev O.A., Shragin D.I., Kopylov V.M., Glazov P.A. Vosstanovitelnye tehnologii izgotovleniya teplomorozostojkih germetikov na osnove kremnijorganicheskih kauchukov, sintezirovannyh po novym promyshlennym tehnologiyam [Recovery manufacturing techniques of heatcold-resistant hermetics on the basis of the organic silicon rubbers synthesized on new industrial technologies] // Aviacionnye materialy i tehnologii. 2012. №4. S. 25–31.
  12. Baranovskaya N.B. Problema germetizatsii i germetiziruyushchiye materialy [The problem of sealing and sealing materials] // Germetizatsiya samoletnykh konstruktsiy. M.: VIAM, 1959. S. 5–11.
  13. Venediktova M.A., Naumov I.S., Chajkun A.M., Eliseev O.A. Sovremennye tendencii v oblasti ftorsiloksanovyh i siloksanovyh kauchukov i rezin na ih osnove (obzor) [Current trends in fluorosiloxane and siloxane rubbers and rubber compounds based thereon (rеview)] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 17–24. DOI: 10.18577/2071-9140-2014-0-S3-17-24.
  14. Eliseev O.A., Bryk Ya.A., Smirnov D.N. Modifikaciya polisulfidnyh germetikov ingibitorami korrozii [Polysulfide sealants modification by corrosion inhibitors] // Aviacionnye materialy i tehnologii. 2016. №S2 (44). S. 15–21. DOI: 10.18577/2071-9140-2016-0-S2-15-21.
  15. Bolshoy spravochnik rezinshchika [Great reference rubberman]. M.: Tekhinform, 2012. Ch. 2 S. 179–180.
  16. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  17. Konstruktivnyye osobennosti germeticheskikh kabin [Design features of hermetic cabs] // Studopediya [Elektronnyy resurs]. Available at: http://www.studopedia.su (accessed: July 18, 2018).
  18. Edward M. Petrie Handbook of Adhesives and Seals. New York: McGraw-Hill, 2000. P. 14–23.