The influence of directional solidification parameters on the structure and properties of the intermetallic alloys

Koljadov E.V., Visik E.M., Gerasimov V. V., Arginbaeva E.G.
Koljadov E.V., Visik E.M., Gerasimov V. V., Arginbaeva E.G. The influence of directional solidification parameters on the structure and properties of the intermetallic alloys // Proceedings of VIAM. 2019. No. 3. DOI: 10.18577/2307-6046-2019-0-3-14-26. URL: https://www.viam-works.ru/en/journal/2019/3/2
Keywords
intermetallic alloys, directional solidification, single crystal casting equipment, temperature gradient.
Abstract

Comparative studies of the influence of thermal conditions of the process of directional crystallization in plants of two types are presented: liquid metal cooling (UVKH-9A installation) – LMC process (Liquid Metal Cooling) and radiation cooling (ALD installation) – HRS process (High Rate of Solidification ) on the parameters of the cast structure of the VKNA-4UMONO alloy. A comparative quantitative analysis of the microstructure, strength characteristics during short-term tensile tests of castings from VKNA-4UMONO alloy with crystallographic orientation of СGO [111], obtained on installations of two types, and analysis of fractures of VKNA-4U samples of single-crystal structure after short-term tests on stretching. The effect of temperature gradient at the growth front on the structure and mechanical properties of VKNA-4U alloy with KGO [111] and a new alloy for single-crystal casting VIN4 with СGO [001] is shown. The main characteristics of melting and casting plants for casting intermetallic alloys by the method of directional solidification with liquid metal cooling are presented.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Buntushkin V.P., Bazyleva O.A., Gerasimov V.V., Timofeyeva O.B. Zharoprochnyye splavy na osnove intermetallida Ni3Al [Heat-resistant alloys based on the Ni3Al intermetallic compound] // Tr. Mezhdunar. nauch.-tekhn. konf. «Nauchnyye idei S.T. Kishkina i sovremennoye materialovedeniye». M.: VIAM, 2006. S. 71–75.
  3. Kablov E.N., Ospennikova O.G., Petrushin N.V. Novyj monokristallicheskij intermetallidnyj (na osnove γʹ-fazy) zharoprochnyj splav dlya lopatok GTD [New single crystal heat-resistant intermetallic γʹ-based alloy for GTE blades] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 34–40. DOI: 10.18577/2071-9140-2015-0-1-34-40.
  4. Buntushkin V.P., Kablov E.N., Kachanov E.B., Shalin R.E. Vysokotemperaturnyye konstruktsionnyye splavy na osnove intermetallida Ni3Al [High-temperature structural alloys based on the Ni3Al intermetallic compound] // Aviacionnyye materialy na rubezhe XX–XXI vekov. M.: VIAM, 1994. S. 278–284.
  5. Harada H. Development of Superalloys for 1700°C ultra-efficient gas turbines // Proceedings of 9th Liege Conference «Materials for Advanced Power Engineering 2010». Belgium: University of Liège. 2010. P. 604–614.
  6. Ospennikova O.G. Tendencii sozdaniya zharoprochnyh nikelevyh splavov nizkoj plotnosti s polikristallicheskoj i monokristallicheskoj strukturoj (obzor) [Tendencies of development of heat-resistant nickel alloys of low density with polycrystalline and single-crystal structures (review)] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 3–19. DOI: 10.18577/2071-9140-2016-0-1-3-19.
  7. Sharova N.A., Tikhomirova E.A., Barabash A.L., Zhivushkin A.A., Brauer V.E. K voprosu o vybore novykh zharoprochnykh nikelevykh splavov dlya perspektivnykh aviatsionnykh GTD [On the choice of new heat-resistant nickel alloys for promising aviation gas turbine engines] // Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta. 2009. №3 (19). S. 249−255.
  8. Drozdov A.A., Povarova K.B., Morozov A.E. i dr. Dendritnaya likvatsiya v monokristallakh intermetallidnykh splavov na osnove Ni3Al, legirovannykh Cr, Mo, W, Ti, Co, Re [Dendritic segregation in single crystals of intermetallic alloys based on Ni3Al doped with Cr, Mo, W, Ti, Co, Re] // Metally. 2015. №4. S. 48–55.
  9. Petrushin N.V., Elyutin E.S., Korolev A.V. Monokristallicheskiye zharoprochnyye splavy: sostav, tekhnologii, struktura i svoystva [Single-crystal superalloys: composition, technology, structure, and properties] // Materialy Vseross. nauch.-tekhnich. konf. «Fundamentalnyye i prikladnyye issledovaniya v oblasti sozdaniya liteynykh zharoprochnykh nikelevykh i intermetallidnykh splavov i vysokoeffektivnykh tekhnologiy izgotovleniya detaley GTD». M.: VIAM, 2017. S. 271–303.
  10. Kablov E.N., Petrushin N.V., Elyutin E.S. Monokristallicheskiye zharoprochnyye splavy dlya gazoturbinnykh dvigateley [Monocrystalline superalloys for gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye. 2011. №SP2. S. 38–52.
  11. Kablov E.N., Petrushin N.V., Morozova G.I., Svetlov I.L. Fiziko-khimicheskiye faktory zharoprochnosti nikelevykh splavov, soderzhashchikh reniy [Physico-chemical factors of heat resistance of nickel alloys containing rhenium] // Liteynyye zharoprochnyye splavy. Effekt S.T. Kishkina. M.: Nauka, 2006. S. 116–130.
  12. Shalin R.E., Svetlov I.L., Kachanov E.B., Toloraiya V.N., Gavrilin O.S. Monokristally nikelevykh zharoprochnykh splavov [Single crystals of nickel superalloys]. M.: Mashinostroyeniye, 1997. 336 s.
  13. Skibin V.A., Solonin V.I. Aviatsionnoye dvigatelestroyeniye. Doroga v zavtrashniy den [Aviation engine building. Road to tomorrow] // Dvigatel. 2007. №5 (53). S. 1–4.
  14. Kablov E.N. Lityye lopatki gazoturbinnykh dvigateley (splavy, tekhnologiya, pokrytiya) [Cast blades of gas turbine engines (alloys, technology, coatings)]. M.: MISiS, 2006. 632 s.
  15. Gerasimov V.V., Petrushin N.V., Visik E.M. Usovershenstvovanie sostava i tehnologiya lit'ya monokristallicheskih lopatok iz zharoprochnogo intermetallidnogo splava [Improvement of casting technology and composition of single crystal blades made of heat-resistant intermetallic alloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 01. Available at: http://www.viam-works.ru (accessed: August 10, 2018). DOI: 10.18577/2307-6046-2015-0-3-1-1.
  16. Kolyadov E.V., Gerasimov V.V. Vliyanie privedennogo razmera otlivki na osevoj gradient temperatury i makrostrukturu otlivok pri napravlennoj kristallizacii na ustanovke UVNK-15 [The influence of the reduced size of the casting on the axial temperature gradient and the macrostructure of casting for directional solidification at the facility UVNK-15] // Aviacionnye materialy i tehnologii. 2014. №3. S. 3–9.
  17. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizatsii v resursosberegayushchej tehnologii proizvodstva detalej GTD [Role of the directed crystallization in the resource-saving production technology of details of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 01. Available at: http://www.viam-works.ru (accessed: December 15, 2018).
  18. Kablov E.N., Tolorajya V.N. VIAM – osnovopolozhnik otechestvennoj tehnologii litya monokristallicheskih turbinnyh lopatok GTD i GTU [VIAM – the founder of domestic casting technology of single-crystal turbine blades of GTE and GTU] // Aviacionnye materialy i tehnologii. 2012. №S. S. 105–117.
  19. Miller J.D., Pollock T.M. Development and Application of Optimization Protocol For Directional Solidification: Integration Fundamental Theory, Experimentation and Modeling Tools // Superalloys 2012. ТМS: Minerals, Metals & Materials Society, 2012. P. 653−662.
  20. Esser W. Direction Solidification of Blades for Industrial Gas Turbines // Materials for Advanced Power Engineering. 1994. P. 641–659.