Research of climatic factors influence of cold, temperate (moderate) and tropical climates on properties of construction fibreglass

Andreeva N.P., Pavlov M.R., Nikolaev E.V., Kurnosov A.O.
Andreeva N.P., Pavlov M.R., Nikolaev E.V., Kurnosov A.O. Research of climatic factors influence of cold, temperate (moderate) and tropical climates on properties of construction fibreglass // Proceedings of VIAM. 2019. No. 3. DOI: 10.18577/2307-6046-2019-0-3-105-114. URL: https://www.viam-works.ru/en/journal/2019/3/12
Keywords
fiberglass composite, climatic factory, aging, cyanether binder, flexural strength, tropic climate.
Abstract

The results of climatic tests of fibreglass on the basis of the tsianefirny binding are provided in the paper. Tests have been carried out under natural conditions at climatic stations of Russia (Moscow, Gelendzhik, Sochi, Yakutsk) and North America (Arizona and Florida), three stations of Vietnam (Hoa Lac, Dam Bay, Can Gio). Thereby research and results of changes of properties of fibreglass have been conducted have been analyzed for different types of climates on different continents – cold, moderate, moderate warm, tropical dry and tropical wet. In work the analysis of results researchs has been carried out and conclusions on resistance of material of such type to influence of climatic factors are drawn.

Reference list
  1. Raskutin A.E. Rossiiskie polimernye kompozitsionnye materialy novogo pokoleniia, ikh osvoenie i vnedrenie v perspektivnykh razrabatyvaemykh konstruktsiiakh [Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions] // Aviacionnye materialy i tehnologii. 2017. №S. S. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  2. Kurnosov A.O., Melnikov D.A. Kharakteristiki stekloplastikov na osnove vysokodeformativnykh rasplavnykh svyazuyushchikh v usloviyakh vozdeystviya ekspluatatsionnykh faktorov [Characteristics of glass-reinforced plastics on the basis of highly deformative melt binders under the influence of operational factors] // Vse materialy. Entsiklopedicheskiy spravochnik. 2015. №11. S. 14–17.
  3. Filatov M.Ya. Opticheskiye metody issledovaniya razrusheniya polimernykh materialov [Optical methods for studying the destruction of polymeric materials]. Kiev: Naukova dumka, 1989. 132 s.
  4. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  5. Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
  6. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  7. Klimaticheskiye ispytaniya [Climatic tests] // Istoriya aviatsionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshch. red. E.N. Kablova. M.: VIAM, 2012. S. 429–438.
  8. Gurtovnik I.G., Sportsmen V.N. Stekloplastiki radiotekhnicheskogo naznacheniya [Fiberglass plastics]. M.: Khimiya, 1987. 160 s.
  9. Laptev A.B., Barbotko S.L., Nikolaev E.V. Osnovnye napravleniya issledovanij sokhranyaemosti svojstv materialov pod vozdejstviem klimaticheskikh i ekspluatatsionnykh faktorov [The main research areas of the persistence properties of materials under the influence of climatic and operational factors] // Aviacionnye materialy i tehnologii. 2017. №S. S. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
  10. Valevin E.O., Andreyeva N.P., Pavlov M.R. Kompleksnyy podkhod k issledovaniyu protsessov stareniya polimernykh kompozitsionnykh materialov pri vozdeystvii klimaticheskikh faktorov [An integrated approach to the study of the aging process of polymer composite materials under the influence of climatic factors] // Sb. dokl. II Vseross. nauch.-tekhnich. konf. «Klimat-2017. Problemy otsenki klimaticheskoy stoykosti materialov i slozhnykh tekhnicheskikh sistem». Gelendzhik, 2017. S. 8–20.
  11. Gurtovnik I.G., Sokolov V.I., Trofimov N.N., Shalgunov S.I. Radioprozrachnyye izdeliya iz stekloplastikov [Fiberglass radioplastic products]. M.: Mir, 2002. 368 s.
  12. Emanuel N.M., Buchachenko A.L. Khimicheskaya fizika molekulyarnogo razrusheniya i stabilizatsii polimerov [Chemical physics of molecular destruction and stabilization of polymers]. M.: Nauka, 1988. 365 s.
  13. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Nikolayev E.V., Pavlov M.R., Andreyeva N.P., Slavin A.V., Skirta A.A. Issledovaniye protsessov stareniya polimernykh kompozitsionnykh materialov v naturnykh usloviyakh tropicheskogo klimata Severnoy Ameriki [Investigation of the aging processes of polymeric composite materials in natural conditions of tropical climate of North America] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2018. №3–4. St. 08. Available at: http://www.materialsnews.ru (accessed: May 23, 2018).
  15. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Kompleksnoe issledovanie vozdeystviya klimaticheskikh i ekspluatatsionnykh faktorov na novoe pokolenie epoksidnogo svyazuyushchego i polimernykh kompozitsionnykh materialov na ego osnove. Chast 4. Naturnye klimaticheskie ispytaniya polimernykh kompozitsionnykh materialov na osnove epoksidnoy matritsy [Complex research of influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 4. Natural climatic tests of polymeric composite materials on the basis of epoxy matrix] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №6. St. 11. Available at: http://www.viam-works.ru (accessed: May 23, 2018). DOI: 10.18577/2307-6046-2016-0-6-11-11.
  16. Nikolaev E.V., Pavlov M.R., Laptev A.B., Ponomarenko S.A. K voprosu opredeleniya sorbi-rovannoj vlagi v polimernyh kompozitsionnyh materialah [To the problem of determining the moisture sorbed in polymeric composite materials] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №8 (56). St. 07. Available at: http://www.viam-works.ru (accessed: September 20, 2018). DOI: 10.18577/2307-6046-2017-0-8-7-7.
  17. Laptev A.B., Nikolayev E.V., Kolpachkov E.D. Termodinamicheskiye kharakteristiki stareniya polimernykh kompozitsionnykh materialov v usloviyakh realnoy ekspluatatsii [Thermodynamic characteristics of aging of polymeric composite materials under conditions of real exploitation] // Aviacionnye materialy i tehnologii. 2018. №3 (52). S. 80–88. DOI: 10.18577/2071-9140-2018-0-3-80-88.
  18. Valevin E.O., Laptev A.B., Nikolayev E.V., Pavlov M.R. Vliyaniye meteoparametrov na ekspluatatsiyu polimernykh kompozitsionnykh materialov v izdeliyakh aviatsionnoy i raketno-kosmicheskoy tekhniki [Influence of meteorological parameters on the operation of polymer composite materials in the products of aviation and rocket-space technology] // Modelirovaniye parametrov atmosfery v raketno-kosmicheskoy tekhnike: tr. po materialam nauch.-tekhnich. konf. Korolev, 2017. S. 91–94.