National standardization specifics of polymer composites materials tests methods

Shershak P.V.
Shershak P.V. National standardization specifics of polymer composites materials tests methods // Proceedings of VIAM. 2019. No. 2. DOI: 10.18577/2307-6046-2019-0-2-77-88. URL: https://www.viam-works.ru/en/journal/2019/2/8
Keywords
ISO, ASTM, standard, interstate standard, national standard, equivalent standards, harmonized standards, GOST, GOST R, polymer composites, tests, properties.
Abstract

A comprehensive analysis of the GOST and GOST R standards developed in recent years as an equivalent of foreign standards for polymer composite materials test methods, has been carried out. The huge work done by the Technical сommittee 497 and companies of various industries was noted. Peculiarities and contradictions in the names of standards, scope of their application, designations of determinable indicators, etc., as the result of a large number of standards release in a relatively short time, are considered. The creation and development of technical standard basis for polymer composite materials test methods is a long process, which cannot be considered completed with the release of a certain number of standards. The constant maintenance, review and improvement by the feedback between the users of the standards and the Тechnical committee 497 is necessary.

 

Reference list
  1. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  2. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Vetokhin S.Yu. Standartnoye resheniye [Standard Solution] // Kompozitnyy mir. 2012. №1 (40). S. 70–72.
  5. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatatsii aviatsionnoy tekhniki [Quality control of materials - a guarantee of the safety of the operation of aviation equipment] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  6. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  7. Zabulonov D.Yu., Myktybekov B.M., Ukhov P.A. Standartizatsiya metodov ispytaniy polimernykh kompozitsionnykh materialov [Standardization of test methods for polymer composite materials] // Kompozitnyy mir. 2010. №4. S. 16–19.
  8. Adamov A.A., Laptev M.Yu., Gorshkova Ye.G. Analiz otechestvennoy i zarubezhnoy normativnoy bazy po mekhanicheskim ispytaniyam polimernykh kompozitsionnykh materialov [Analysis of the domestic and foreign regulatory framework for mechanical testing of polymer composite materials] // Konstruktsii iz kompozitsionnykh materialov. 2012. №3. S. 72–77.
  9. Kablov E.N., Shevchenko Yu.N., Kozhevnikov A.N. Otraslevyye standarty – osnova kachestva aviatsionnoy tekhniki [Industry standards – the basis of the quality of aviation technology] // Stal. 2008. №8. S. 121–122.
  10. Petrova A.P., Malysheva G.V. Klei, kleyevyye svyazuyushchiye i kleyevyye prepregi: uchebnoye posobiye / pod obshch. red. E.N. Kablova [Glues, adhesive binders and adhesive prepregs: a tutorial / gen. ed. by E.N. Kablov]. M.: VIAM, 2017. 472 s.
  11. Ilichev A.V. Sravneniye standartov GOST i ASTM dlya provedeniya mekhanicheskikh ispytaniy PKM na rastyazheniye [Comparison of GOST and ASTM standards for mechanical testing of PCM tensile] // Vse materialy. Entsiklopedicheskiy spravochnik. 2015. №8. S. 2–9.
  12. Fakhretdinov S.B. Innovatsionnyye zakupki v goskompaniyakh [Innovative procurement in state-owned companies] // Compositebook. 2018. №1. S. 30–31.
  13. Melnikov D.A., Ilichev A.V., Vavilova M.I. Sravnenie standartov dlia provedeniia mekha-nicheskikh ispytanii stekloplastikov na szhatie [Comparison of standards for carrying out mechanical tests of GRP compression strength] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №3 (51). St. 06. Available at: http://www.viam-works.ru (accessed: February 11, 2019). DOI: 10.18577/2307-6046-2017-0-3-6-6.
  14. Ilichev A.V., Raskutin A.E., Gulyayev I.N. Sravneniye geometricheskikh razmerov obraztsov PKM, ispolzuyemykh v mezhdunarodnykh standartakh ASTM i otechestvennykh GOST [Comparison of the geometrical sizes polymer matrix composite materials samples which are using international ASTM standards and domestic GOST] // Novosti materialovedeniya. Nauka i tekhnika: elktron. nauch.-tekhnich. zhurn. 2015. №4 (16). S. 33–42. Available at: http://www.materialsnews.ru (accessed: February 11, 2019).
  15. Erasov V.S., Krylov V.D., Panin S.V., Goncharov A.A. Ispytaniya polimernogo kompozitsionnogo materiala na udar padayushhim gruzom [Drop-weight impact testing of polymer composite material] // Aviacionnye materialy i tehnologii. 2013. №3. S. 60–64.
  16. Bolshakov V.A., Aleksashin V.M. Povyshenie ostatochnoj prochnosti pri szhatii posle nizkoskorostnogo udara ugleplastikov, izgotovlyaemyh infuzionnym metodom formovaniya [A way to increase the residual compression strength after low-speed impact of CFRP produced by vacuum infusion technology] // Aviacionnye materialy i tehnologii. 2013. №4. S. 47–50.
  17. Shershak P.V., Ryabovol D.Yu. Standarty po dinamicheskim mekhanicheskim ispytaniyam plastmass i polimernykh kompozitnykh materialov [Standards for dynamic mechanical testing of plastics and polymeric composite materials] // Aviatsionnaya promyshlennost. 2017. №4. S. 48–52.
  18. Yakovlev N.O., Erasov V.S., Petrova A.P. Sravneniye normativnykh baz razlichnykh stran po ispytaniyu kleyevykh soyedineniy materialov [Comparison of regulatory bases in different countries for the testing of adhesive joints of materials] // Vse materialy. Entsiklopedicheskiy spravochnik. 2014. №7. S. 2–8.