Investigation of the mechanical properties of powder materials of the Mo–W system obtained by spark plasma sintering

Batienkov R.V., Efimochkin I.Yu., Osin I.V., Khudnev A.A.
Batienkov R.V., Efimochkin I.Yu., Osin I.V., Khudnev A.A. Investigation of the mechanical properties of powder materials of the Mo–W system obtained by spark plasma sintering // Proceedings of VIAM. 2019. No. 2. DOI: 10.18577/2307-6046-2019-0-2-68-76. URL: https://www.viam-works.ru/en/journal/2019/2/7
Keywords
molybdenum, tungsten, electric-spark plasma sintering, mechanical properties.
Abstract

In this work, the effect of mixing time in a ball mill on the homogeneity and properties of molybdenum-tungsten powder mixtures was investigated. Consolidation of materials was carried out by spark plasma sintering. From the obtained compacts, samples were made for investigated the strength and plastic properties of materials. Optical and scanning electron microscopy was used to the analysis of the microstructure. Energy dispersive microanalysis was used to assess the elemental composition of the samples. The fractures of the samples were investigated.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  3. Kablov E.N. Klyuchevaya problema – materialy [The key problem is materials] // Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. M: VIAM, 2015. S. 458–464.
  4. Kablov E.N. Stanovleniye otechestvennogo kosmicheskogo materialovedeniya [The formation of domestic space materials science] // Vestnik Rossiyskogo fonda fundamentalnykh issledovaniy. 2017. №3 (95). S. 97–105.
  5. Molibden / per. s angl. M.A. Maurakha; pod. red. A.K. Natansona [Molybdenum / trans. from Engl. by M.A. Maurah; ed. by A.K. Natanson]. M.: Izd-vo inost. lit., 1959. S. 304.
  6. Savitskiy E.M., Burkhanov G.S., Povarova K.B. i dr. Tugoplavkiye metally i splavy [Refractory metals and alloys]. M.: Metallurgiya, 1986. 352 s
  7. Korneyev N.I., Pevzner S.B., Razuvayev E.I., Emelyanov. V.B. Obrabotka davleniyem tugoplavkikh metallov i splavov. 2-ye izd. [Pressure treatment of refractory metals and alloys. 2nd ed.] M.: Metallurgiya, 1975. 440 s.
  8. Trofimenko N.N., Efimochkin I.Yu., Bolshakova A.N. Problemy sozdaniya i perspektivy ispolzovaniya zharoprochnykh vysokoentropiynykh splavov [Problems of creation and prospects for the use of heat-resistant high-entropy alloys] // Aviatsionnyye materialy i tekhnologii. 2018. №2 (51). S. 3–8. DOI: 10.18577/2071-9140-2018-0-2-3-8.
  9. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. Vysokotemperaturnye metallomatrichnye kompozicionnye materialy, armirovannye chasticami i voloknami tugoplavkih soedinenij [High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds] // Aviacionnye materialy i tehnologii. 2017. №S. S. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  10. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  11. Trefilov V.I., Milman Yu.V., Firstov S.A. Fizicheskiye osnovy prochnosti tugoplavkikh metallov [Physical basis of the strength of refractory metals]. Kiyev: Naukova dumka, 1975. 315 s.
  12. Batiyenkov R.V., Bolshakova A.N., Yefimochkin I.Yu. Problema nizkotemperaturnoy plastichnosti molibdena i splavov na yego osnove (obzor) [The problem of low-temperature plasticity of molybdenum and alloys based on it (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №3 (63). St. 02. Available at: http://www.viam-works.ru (accessed: December 17, 2018). DOI: 10.18577/2307-6046-2018-0-3-12-17.
  13. Morgunova N.N., Klypin B.A., Boyarshinov V.A. i dr. Splavy molibdena [Alloys of molybdenum]. M.: Metallurgiya, 1975. 392 s.
  14. Savitskiy E.M., Burkhanov G.S. Metallovedeniye splavov tugoplavkikh i redkikh metallov [Metal science alloys of refractory and rare metals]. M.: Nauka, 1971. 356 s.
  15. Torresilyas San Millan R., Solis Pinargote N.V., Okunkova A.A., Peretyagin P.Yu. Osnovy protsessa iskrovogo plazmennogo spekaniya nanoporoshkov [Fundamentals of spark plasma sintering of nanopowders]. M.: Tekhnosfera, 2014. 96 s.