Features of the influence of atmospheric factors on the main technical characteristics of sealing materials of various types of aviation purposes

Chaykun A.М., Venediktova M.A., Smirnov D.N., Gerasimov D.M.
Chaykun A.М., Venediktova M.A., Smirnov D.N., Gerasimov D.M. Features of the influence of atmospheric factors on the main technical characteristics of sealing materials of various types of aviation purposes // Proceedings of VIAM. 2019. No. 2. DOI: 10.18577/2307-6046-2019-0-2-58-67. URL: https://www.viam-works.ru/en/journal/2019/2/6
Keywords
sealing materials, thiokol sealants, fluorsiloxane sealants, siloxane sealants, climatic aging, weather resistance, physic mechanical characteristics.
Abstract

The paper research the influence of atmospheric factors on the properties of various types of sealing materials after aging in various climatic zones. The evaluation of the physic mechanical characteristics of the sealing materials after aging under the conditions of the MSCI, GCCI, states of USA – Florida and Arizona, climatic sites of Vietnam. The main features of climatic aging of sealing materials of various types are considered. An assessment of structural changes in sealing materials as a result of climate exposure has been carried out.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsional'noy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologiya. 2016. №2 (14) S. 16–21.
  3. Nikolayev E.V., Pavlov M.R., Andreyeva N.P., Slavin A.V., Skirta A.A. Issledovaniye protsessov stareniya polimernykh kompozitsionnykh materialov v naturnykh usloviyakh tropicheskogo klimata Severnoy Ameriki [Investigation of the aging processes of polymeric composite materials in natural conditions of tropical climate of North America] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2018. №3–4 (30). St. 08. Available at: http://www.materialsnews.ru (accessed: December 12, 2018).
  4. Valevin E.O., Andreyeva N.P., Pavlov M.R. Kompleksnyy podkhod k issledovaniyu protsessov polimernykh kompozitsionnykh materialov pri vozdeystvii klimaticheskikh faktorov [An integrated approach to the study of processes of polymer composite materials under the influence of climatic factors] // Problemy otsenki klimaticheskoy stoykosti materialov i slozhnykh tekhnicheskikh sistem: sb. dokl. II Vseros. nauch.-tekhn. konf. «Klimat-2017» (Gelendzhik, 3–4 avgusta 2017). M.: VIAM, 2017. S. 8–20 (CD).
  5. Andreyeva N.P., Pavlov M.R., Nikolayev E.V., Slavin A.V. Vliyaniye klimaticheskikh faktorov tropicheskogo i umerennogo klimata na svoystva lakokrasochnykh pokrytiy na uretanovoy osnove [Influence of climatic factors of tropical and temperate climate on the properties of urethane-based paint and varnish coatings] // Lakokrasochnyye materialy i ikh primeneniye. 2018. №4. S. 24–28.
  6. Filatov I.S. Prognozirovaniye klimaticheskoy ustoychivosti polimernykh i kompozitsionnykh materialov na ikh osnove: dis. … d-ra tekhn. nauk [Prediction of climatic stability of polymer and composite materials based on them: tesis, Doct. Sc. (Tech.)]. Yakutsk, 1984. 489 s.
  7. Nikolaev E.V., Pavlov M.R., Laptev A.B., Ponomarenko S.A. K voprosu opredeleniya sorbi-rovannoj vlagi v polimernyh kompozitsionnyh materialah [To the problem of determining the moisture sorbed in polymeric composite materials] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №8 (56). St. 07. Available at: http://www.viam-works.ru (accessed: December 12, 2018). DOI: 10.18577/2307-6046-2017-0-8-7-7.
  8. Bolshoy spravochnik rezinshchika v 2 ch. [Great reference book of rubberman in 2 parts]. M.: Tekhinform, 2012. 1385 s.
  9. Uplotneniya i uplotnitelnaya tekhnika: spravochnik / pod obshch. red. A.I. Golubeva, L.A. Kondakova [Seals and sealing technology: a handbook / gen. ed. by A.I. Golubev, L.A. Kondakov]. M.: Mashinostroyeniye, 1986. 464 s.
  10. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie elastomernyh materialov dlya primeneniya vo vseklimaticheskih usloviyah [Development and modifying of elastomeric materials for application in all weather conditions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314.
  11. Mulrov O.A., Savchenko I.M., Shitov V.S. Spravochnik po elastomernym pokrytiyam i germetikam v sudostroyenii [Handbook of elastomeric coatings and sealants in shipbuilding]. L.: Sudostroyeniye, 1982. 184 s.
  12. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  13. Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
  14. Kablov E.N. Rol khimii v sozdanii materialov novogo pokoleniya dlya slozhnykh tekhnicheskikh system [The role of chemistry in the creation of a new generation of materials for complex technical systems] // Tez. dokl. «XX Mendeleyevskogo syezda po obshchey i prikladnoy khimii». UrO RAN, 2016. S. 25–26.
  15. Khakimulin Yu.N., Minkin V.S., Palyutin F.M., Derbedeyev T.R. Germetiki na osnove polisul'fidnykh oligomerov: sintez, svoystva, primeneniye [Sealants based on polysulfide oligomers: synthesis, properties, application]. M.: Nauka, 2007. 301 s.
  16. Luke H. Aliphatic Polysulfide’s: Monograph of an elastomer. Htidelberg, New York: Publisher Huthig & Wepf Basel, 1994. 191 p.
  17. Nikitina A.A., Solovey V.V. Toplivostoykiye germetiki [Fuel-resistant sealants] // Aviatsionnyye materialy na rubezhe XX–XXI vekov. M.: VIAM, 1994. S. 374–378.
  18. Savenkova A.A., Tikhonova I.V., Trebukova E.A. Teplomorozostoykiye germetiki [Heat and frost-resistant sealants] // Aviacionnyye materialy na rubezhe XX–XXI vekov. M.: VIAM, 1994. S. 432–439.
  19. Laptev A.B., Nikolayev E.V., Kolpachkov E.D. Termodinamicheskiye kharakteristiki stareniya polimernykh kompozitsionnykh materialov v usloviyakh realnoy ekspluatatsii [Thermodynamic characteristics of aging of polymeric composite materials under conditions of real exploitation] // Aviacionnye materialy i tehnologii. 2018. №3 (52). S. 80–88. DOI: 10.18577/2071-9140-2018-0-3-80-88.