Study of the possibility of use of new environmentally friendly organophosphorus flame retardants in the composition of binders for interior fire safety materials

Serkova E.A., Zastrogina O.B., Barbotko S.L.
Serkova E.A., Zastrogina O.B., Barbotko S.L. Study of the possibility of use of new environmentally friendly organophosphorus flame retardants in the composition of binders for interior fire safety materials // Proceedings of VIAM. 2019. No. 2. DOI: 10.18577/2307-6046-2019-0-2-24-34. URL: https://www.viam-works.ru/en/journal/2019/2/3
Keywords
polymer composite materials, flame retardants, organophosphorus compounds, interior materials, fire safety.
Abstract

At present, the share of polymer composite materials (PCM) used in the aviation industry is 15% of the total number of PCM produced. The priority directions for the development of civil aviation are, firstly, the reduction of the weight of an airliner, which significantly reduces fuel consumption and leads to a reduction in the cost of transportation, and secondly, increasing flight safety. Safety is associated with the reliable operation of all systems, components and structural elements of a passenger aircraft, and in particular, with fire safety and non-toxicity of materials used in the interior. The article describes the study of the impact of new environmentally safe organophosphorus flame retardants on the properties of polymeric materials of interior decoration (interior) liner.

Reference list
  1. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  2. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2. S. 16–22.
  3. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  4. Barbotko S.L., Kirillov V.N., Shurkova E.N. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov aviacionnogo naznacheniya [Fire safety evolution for polymer composites of aeronautical application] // Aviacionnye materialy i tehnologii. 2012. №3. S. 56–63.
  5. Kopylov V.V., Novikov S.N., Oksentyevich L.A. i dr. Polimernyye materialy ponizhennoy goryuchesti [Polymeric materials of low flammability]. M.: Khimiya, 1986. 224 s.
  6. Aseyeva R.M., Zaikov G.E. Snizheniye goryuchesti polimernykh materialov [Decrease in combustibility of polymeric materials]. M.: Znaniye, 1981. Ser.: Khimiya. №10. 63 s.
  7. Kodolov V.I. Zamedliteli goreniya polimernykh materialov [Flame retardants of polymeric materials]. M.: Khimiya, 1980. 274 s.
  8. Chizhova M.A., Khayrullin R.Z. Toksichnost produktov goreniya polimernykh materialov pri vvedenii v ikh sostav antipirenov [Toxicity of combustion products of polymeric materials with the introduction of flame retardants into their composition] // Vestnik Kazanskogo tekhnologicheskogo universiteta. 2014. T. 17. №9. S. 144–145.
  9. Lomakin S.M., Zaikov G.E., Mikitayev A.K. i dr. Zamedliteli goreniya dlya polimerov [Combustion retardants for polymers] // Vestnik Kazanskogo tekhnologicheskogo universiteta. 2012. T. 15. №7. S. 71–86.
  10. Shaov A.Kh., Alarkhanova Z.Z. Posledniye dostizheniya v oblasti sozdaniya ognestoykikh polimernykh materialov [Recent advances in the creation of fire-resistant polymeric materials] // Plasticheskiye massy. 2005. №6. S. 7–20.
  11. Zastrogina O.B., Shvets N.I., Serkova E.A., Veshkin E.A. Pozharobezopasnyye materialy na osnove fenoloformaldegidnykh svyazuyushchikh [Fireproof materials based on phenol-formaldehyde binders] // Klei. Germetiki. Tekhnologii. 2017. №7. S. 22–28.
  12. Normy letnoy godnosti samoletov transportnoy kategorii [Airworthiness standards for airplanes of the transport category]: AP-25: utv. Postanovleniyem 28-y sessii Soveta po aviatsii i ispolzovaniyu vozdushnogo prostranstva 11.12.2008. 3-e izd. s popravkami 1–6. M.: Aviaizdat. 2009. 274 s.
  13. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Organizatsiya po zapreshcheniyu khimicheskogo oruzhiya [Organization for the Prohibition of Chemical Weapons] // Konventsiya o khimicheskom oruzhii. Available at: http://www.opcw.org/ru (accessed: November 26, 2018).
  15. Berezkin M.Yu., Turygin V.V., Khudenko A.V. i dr. Elektrokhimicheskiy sintez raznozameshchennykh trialkilfosfatov [Electrochemical synthesis of differently substituted trialkylphosphates] // Elektrokhimiya. 2011. T. 47. №10. S. 1272–1275.
  16. Barbotko S.L. Razvitie metodov ocenki pozharobezopasnosti materialov aviacionnogo naznacheniya [Development of the fire safety test methods for aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  17. Antyufeeva N.V., Aleksashin V.M., Stolyankov Yu.V. Opredelenie stepeni otverzhdeniya PKM metodami termicheskogo analiza [Polymer composite curing degree evaluation by thermal analysis test methods] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 79–83.