Prospects for the use of ethylene-propylene-diene rubber as part of cold resistant rubber
UDC
678.741:536.485
DOI
10.18577/2307-6046-2019-0-12-29-36
Article PDF (Russian)
(637.81 KB)
How to cite
Kablov E.N., Semenova S.N., Suleymanov R.R., Chaykun A.М. Prospects for the use of ethylene-propylene-diene rubber as part of cold resistant rubber // Proceedings of VIAM. 2019. No. 12. DOI: 10.18577/2307-6046-2019-0-12-29-36. URL: https://www.viam-works.ru/en/journal/2019/12/4
Keywords
rubber, ethylene-propylene-diene rubber, cold resistance, compatibilizer, vulcanization.
Abstract
The ethylene-propylene-diene rubber (SKEPT-40) was investigated as the main component in the cold-resistant rubber. The optimal vulcanizing system and the ways to improve the cold-resistant indicators by adding the paraffin plasticizer and by combination with polybutadiene (SKD-N) and silicone rubber (SKTFV-803) are developed. The advantages of the investigated rubbers in comparison with the cold-resistant sealing rubber IRP-1375 containing ethylene-propylene rubber are shown. The ways to further improve the cold-resistant performance of rubbers based on ethylene-propylene-diene rubbers are proposed.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of a new generation – the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologiya. 2016. №2 (14). S. 16–21.
- Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
- Kablov E.N. Rol khimii v sozdanii materialov novogo pokoleniya dlya slozhnykh tekhnicheskikh sistem [The role of chemistry in the creation of new generation materials for complex technical systems] // Tez. dokl. XX Mendeleyevskogo syezda po obshchey i prikladnoy khimii. Ekaterinburg: UrO RAN, 2016. S. 25–26.
- Laptev A.B., Barbotko S.L., Nikolaev E.V. Osnovnye napravleniya issledovanij sokhranyaemosti svojstv materialov pod vozdejstviem klimaticheskikh i ekspluatatsionnykh faktorov [The main research areas of the persistence properties of materials under the influence of climatic and operational factors] // Aviacionnye materialy i tehnologii. 2017. №S. S. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
- Gryaznov V.I., Petrova G.N., Yurkov G.Yu., Buznik V.M. Smesevye termojelastoplasty so specialnymi svojstvami [Thermoplastic mixtures with special properties] // Aviacionnye materialy i tehnologii. 2014. №1. S. 25–29. DOI: 10.18577/2071-9140-2014-0-1-25-29.
- Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie elastomernyh materialov dlya primeneniya vo vseklimaticheskih usloviyah [Development and modifying of elastomeric materials for application in all weather conditions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314.
- Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 05. Available at: http://viam-works.ru (accessed: April 04, 2019).
- Man der Aar N. Introduction Lanxess. Available at: http://www.vizl.eu/ cms/uploads/files/d9570e623d578b72267b0f6d29810d6f.pdf (accessed: April 08, 2019).
- Monosulfidnye svyazi [Monosulfide bonds] // Spravochnik khimika 21. Khimiya i khimicheskaya tekhnologiya. Available at: https://chem21.info/info/749977/ (accessed: August 02, 2019).
- Abou-Helal M.O., El-Sabbagh S.H. A Study on the Compatibility of NR-EPDM Blends Using Electrical and Mechanical Techniques // Journal of Elastomer and Plastics. 2005. Vol. 37 (10). P. 319–346.
- Jalbert R.L. Modern Plastics Encyclopedia. New-York: McGraw-Hill, 1984. 841 p.
- Semenova S.N., Suleymanov R.R., Chaykun A.M. Sovmestnoye ispolzovaniye etilenpropilendiyenovogo i metilfenilsiloksanovogo kauchuka v retsepture morozostoykoy i ozonostoykoy reziny [Mixing ethylene-propylene-diene and methylphenylsiloxane rubbers in the formulation of cold and ozone resistant rubber] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2019. №9 (81). St. 07. Available at: http://www.viam-works.ru (accessed: September 24, 2019). DOI: 10.18577/2307-6046-2019-0-9-64-72.
- Bolshoy spravochnik rezinshchika v 2 ch. [the big reference book for specialist in rubbers in 2 parts]. M.: Tekhinform, 2012. 1385 s.