Prerequisites for the selection of the structure model of highly porous fibrous materials to take into account the influence of technological factors and the calculation of heat transfer
UDC
66.045.3:678.6
DOI
10.18577/2307-6046-2019-0-12-109-118
Article PDF (Russian)
(785.51 KB)
How to cite
Zuev A.V., Zarichnyak Yu.P., Razmakhov M.G. Prerequisites for the selection of the structure model of highly porous fibrous materials to take into account the influence of technological factors and the calculation of heat transfer // Proceedings of VIAM. 2019. No. 12. DOI: 10.18577/2307-6046-2019-0-12-109-118. URL: https://www.viam-works.ru/en/journal/2019/12/12
Keywords
highly porous fibrous materials, structure model, thermal conductivity, calculation.
Abstract
The prerequisites for selecting and constructing a model of the structure of a highly porous fibrous material used as the main component of thermal protection, including on the outer surface of high-speed aircraft, are considered. The possibility is shown through the model of the structure of taking into account the influence of technological parameters on thermal conductivity by the example of forming a semi-finished product of highly porous fibrous material with unfixed contacts.
Reference list
- Dulnev G.N., Zarichnyak Yu.P. Teploprovodnost smesey i kompozitsionnykh materialov [Thermal conductivity of mixtures and composite materials]. L.: Energiya, 1974. 264 s.
- Dulnev G.N., Novikov V.V. Protsessy perenosa v neodnorodnykh sredakh [Transfer processes in heterogeneous environments]. L.: Energoatomizdat, 1991. 248 s.
- Alifanov O.M., Cherepanov V.V. Matematicheskoye modelirovaniye vysokoporistykh voloknistykh materialov i opredeleniye ikh fizicheskikh svoystv [Mathematical modeling of highly porous fibrous materials and determination of their physical properties] // Teplofizika vysokikh temperatur. 2009. T. 47. №3. S. 463–472.
- Zuev A.V., Prosuntsov P.V., Mayorova I.A. Raschetno-eksperimentalnoe issledovaniye protsessov teploperenosa v vysokoporistykh voloknistykh teploizolyatsionnykh materialakh [Calculation and experimental study of heat transfer processes in highly porous fibrous heat-insulating materials] // Teplovyye protsessy v tekhnike. 2014. T. 6. №9. S. 410–419.
- Zuyev A.V., Prosuntsov P.V. Model struktury voloknistykh teploizolyatsionnykh materialov dlya analiza protsessov kombinirovannogo teploperenosa [The structure model of fibrous heat-insulating materials for the analysis of combined heat transfer processes] // Inzhenerno-fizicheskiy zhurnal. 2014. T. 87. №6. S. 1319–1330.
- Lukashevich V.P., Afanasev I.B. Kosmicheskiye krylya [Cosmic wings]. M.: Lenta stranstviy, 2009. 496 s.
- Semenov Yu.P., Lozino-Lozinskiy G.E., Lapygin V.L. i dr. Mnogorazovyy orbitalnyj korabl «Buran» [Reusable orbiter «Buran»]. M.: Mashinostroyeniye, 1995. 468 s.
- Mordovin S.G., Davydov I.Z., Kulikov V.I., Gofin M.Ya. Teplozashchitnaya konstruktsiya mnogorazovogo orbitalnogo korablya [Heat shield design of a reusable orbital ship] // Tr. Pervoy mezhdunar. aviakosmicheskoy konf. «Chelovek–Zemlya–Kosmos» (Moskva, 28 sentyabrya–2 oktyabrya, 1992). M., 1995. T. 5: Materialy i tekhnologiya proizvodstva aviakosmicheskikh sistem. S. 315–327.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Dospekhi dlya «Burana». Materialy i tekhnologii VIAM dlya MKS «Energiya–Buran» / pod obshch. red. E.N. Kablova [Armor for the «Buran». VIAM materials and technologies for the ISS «Energiya–Buran» / gen. ed. E.N. Kablov]. M.: Nauka i zhizn, 2013. 128 s.
- Kablov E.N. Stanovleniye otechestvennogo kosmicheskogo materialovedeniya [Formation of domestic space materials science] // Vestnik RFFI. 2017. №3. S. 97–105.
- Majorova I.A. Matematicheskoe modelirovanie processa teploperenosa i optimizaciya konstrukcii mnogoslojnogo teplozashhitnogo pokrytiya [Mathematical modeling of heat transfer and optimization of multilayer thermal protective system] // Aviacionnye materialy i tehnologii. 2013. №2. S. 16–18.
- Ivakhnenko Yu.A., Baruzdin B.V., Varrik N.M., Maksimov V.G. Vysokotemperaturnye voloknistye uplotnitelnye materialy [High-temperature fibrous sealing materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 272–289. DOI: 10.18577/2071-9140-2017-0-S-272-289.
- Istomin A.V., Kolyshev S.G. Elektrostaticheskiy metod formovaniya ultratonkikh volokon tugoplavkikh oksidov [Electrostatic method of forming ultrathin fibers of refractory oxides] // Aviacionnye materialy i tehnologii. 2019. №2 (55). S. 40–46. DOI: 10.18577/2071-9140-2019-0-2-40-46.
- Kostylev V.M. Makroskopicheskaya kinetika fotonnogo gaza. Radiatsionnyy teploobmen v dispersnykh sredakh [Macroscopic kinetics of photon gas. Radiation heat transfer in dispersed media]. M.: Mashinostroyeniye, 2000. 240 s.
- Alifanov O.M., Bojkov N.A. Les Methodes des Previsions In Formatiquers des Materaux Composities de Haute Porosite et de L΄analise des Systems de la Protection Thermique a leur Basc // Proceedings of Conference on Spacecraft Structures, Materials and Mechanical Testing (Noordwijk, Netherlands, March 27–29, 1996). Noordwijk, 1996. P. 73.
- Barinov D.Ya., Ospennikova O.G., Marakhovskiy P.S., Zuyev A.V. Izucheniye dinamiki progreva destruktiruyushchego teplozashchitnogo materiala metodom matematicheskogo modelirovaniya temperaturnykh poley [Study of heating dynamics of destructive heat protective material by the method of mathematical modeling of temperature fields] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2019. №8 (80). St. 12. Available at: http//www.viam-works.ru (accessed: September 01, 2019). DOI: 10.18577/2307-6046-2019-0-8-109-118.
- Dozhdikov V.S., Petrov V.A., Stepanov S.V. Izluchatelnaya sposobnost i koeffitsiyenty zatukhaniya i pogloshcheniya voloknistoy kvartsevoy teploizolyatsii [Emissivity and attenuation and absorption coefficients of fibrous quartz thermal insulation] // Nauchnyye trudy ITES OIVT RAN. 2006. Vyp. 7-2004. S. 65–70.
- Prosuntsov P.V., Mayorova I.A., Zuyev A.V. Ispolzovanie modeley kombinirovannogo teploperenosa dlya analiza temperaturnogo sostoyaniya elementov teplovoy zashchity mnogorazovykh kosmicheskikh apparatov [The use of combined heat transfer models for analyzing the temperature state of the thermal protection elements of reusable spacecraft] // Teplovye protsessy v tekhnike. 2014. T. 6. №7. S. 317–323.
- Shalin R.E., Solntsev S.S., Bersenev A.Yu. Issledovaniye svoystv pokrytiy plitochnoy teplozashchity dlya vozdushno-kosmicheskogo letatelnogo apparata [Investigation of the properties of tiled thermal protection coatings for an aerospace aircraft] // Tr. Pervoy mezhdunar. aviakosmicheskoy konf. «Chelovek–Zemlya–Kosmos» (Moskva, 28 sentyabrya–2 oktyabrya, 1992). M., 1995. T. 5: Materialy i tekhnologiya proizvodstva aviakosmicheskikh sistem. S. 240–249.
- Bersenev A.Yu., Ryakhovskaya Z.I., Semenov E.V., Solntsev S.S., Tyurin V.M. Vysokoeffektivnye erozionnostoykiye pokrytiya dlya teplozashchitnykh materialov aviatsionno-kosmicheskoy tekhniki [Highly effective erosion-resistant coatings for heat-protective materials of aerospace engineering] // Tr. Pervoy mezhdunar. aviakosmicheskoy konf. «Chelovek–Zemlya–Kosmos» (Moskva, 28 sentyabrya–2 oktyabrya, 1992). M., 1995. T. 5: Materialy i tekhnologiya proizvodstva aviakosmicheskikh sistem. S. 235–240.
- Dozhdikov V.S., Petrov V.A. Izluchatelnye kharakteristiki teplozashchitnykh materialov orbitalnogo korablya «Buran» [Radiative characteristics of heat-shielding materials of the Buran orbital ship] // Inzhenerno-fizicheskiy zhurnal. 2000. T. 73. №1. S. 26–30.
- Prosuntsov P.V., Reznik S.V. Issledovaniye obemnykh opticheskikh svoystv chastichno prozrachnykh rasseivayushchikh materialov na osnove resheniya obratnoy zadachi perenosa izlucheniya [Investigation of the bulk optical properties of partially transparent scattering materials based on the solution of the inverse radiation transfer problem] // Identifikatsiya dinamicheskikh sistem i obratnyye zadachi: materialy 2-y Mezhdunar. konf. SPb., 1994. T. 2. S. D–12–1–9.
- Petrov V.A. Model diffuzii izlucheniya dlya radiatsionno-konduktivnogo teploperenosa v vysokotemperaturnykh poluprozrachnykh rasseivayushchikh teploizolyatsionnykh materialakh [Radiation diffusion model for radiation-conductive heat transfer in high-temperature translucent scattering heat-insulating materials]. M.: Mosk. gos. tekhn. un-t radiotekhniki, elektroniki i avtomatiki, 2012. 140 s.
- Gribkov V.N., Mizyurina G.T., Shchetanov B.V., Lyapin V.V. Vozmozhnosti voloknistoy teplovoy zashchity [Possibilities of fibrous thermal protection] // Tr. Pervoy mezhdunar. aviakosmicheskoy konf. «Chelovek–Zemlya–Kosmos» (Moskva, 28 sentyabrya–2 oktyabrya, 1992). M., 1995. T. 5: Materialy i tekhnologiya proizvodstva aviakosmicheskikh sistem. S. 223–231.
- Litovskiy E.Ya., Bondarenko S.L., Polonskiy Yu.A., Ganichev N.I. O vliyanii diametra volokna na effektivnuyu teploprovodnost [On the effect of fiber diameter on effective thermal conductivity /] // Teplofizika vysokikh temperatur. 1979. T. 17. №5. S. 997–1000.
- Kats S.M. Vysokotemperaturnyye teploizolyatsionnyye materialy [High temperature insulation materials]. M.: Metallurgiya, 1981. 232 s.
- Alifanov O.M., Budnik S.A., Nenarokomov A.V., Cherepanov V.V. Eksperimentalno-teoreticheskoye issledovaniye protsessov teploobmena v vysokoporistykh materialakh [Experimental and theoretical study of heat transfer processes in highly porous materials] // Teplovyye protsessy v tekhnike. 2011. T. 3. №2. S. 53–65.
- Volarovich M.P., Demkin N.V., Berkovich I.I. Eksperimentalnoe issledovanie treniya i uplotneniya voloknistykh materialov [An experimental study of friction and compaction of fibrous materials] // Problemy fiziko-khimicheskoy mekhaniki voloknistykh i poristykh dispersnykh struktur i materialov. Riga: Zinatne, 1967. 620 s.
- Zhdanovich G.M. Nekotorye voprosy teorii protsessa pressovaniya metallicheskikh poroshkov [Some questions of the theory of the process of pressing metal powders]. Minsk: Izd-vo Belorus. politekh. in-ta, 1960. 98 s.