Comparative evaluation of methods for determining the content of hydrogen in metal materials

Davydov D.M., Titov V.I., Letov A.F., Lutsenko A.N.
Davydov D.M., Titov V.I., Letov A.F., Lutsenko A.N. Comparative evaluation of methods for determining the content of hydrogen in metal materials // Proceedings of VIAM. 2019. No. 11. DOI: 10.18577/2307-6046-2019-0-11-75-84. URL: https://www.viam-works.ru/en/journal/2019/11/9
Keywords
hydrogen, analysis methods, determination of hydrogen content, metallic mate-rials, optical emission method, heating in a current of inert carrier gas, vacuum heating.
Abstract

Assesses three methods for determining the hydrogen content in metallic materials: optical emission, heating in a carrier inert gas with a conductometric termination, and vacuum heating with a mass spectrometric end. Also considers the optimal scope of each of the considered methods for solving specific problems aimed at determining the hydrogen content with different binding energies (common, diffusion-mobile, strongly bonded) in metallic materials.

Reference list
  1. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  2. Lutsenko A.N., Perov N.S., Chabina E.B. Novye etapy razvitiya Ispytatelnogo tsentra [The new stages of development of Testing Center] // Aviacionnye materialy i tehnologii 2017. №S. S. 460–468. DOI: 10.18577/2071-9140-2017-0-S-460-468.
  3. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Tendencii razvitiya intermetallidnyh splavov na osnove nikelya [Development trends of nickel-based intermetallic alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  4. Fridlyander I.N., Dobromyslov A.V., Tkachenko E.A., Senatorova O.G. Perspektivnyye vysokoprochnyye materialy na alyuminiyevoy osnove [Promising high-strength materials based on aluminum] // Metallovedeniye i termicheskaya obrabotka metallov. 2005. №7. S. 17–23.
  5. Yoshioka M., Ueno A., Kishimoto H. Analysis of hydrogen behaviour in crack growth tests of g-TiAl by means of the hydrogen microprint technique // Journal of Intermetallics. 2004. Vol. 12. P. 23–31.
  6. Kurs M.G., Laptev A.B., Kutyrev A.E., Morozova L.V. Issledovaniye korrozionnogo razrusheniya deformiruyemykh alyuminiyevykh splavov pri naturno-uskorennykh ispytaniyakh. Chast 1 [Investigation of corrosion failure of wrought aluminum alloys during field accelerated tests. Part 1] // Voprosy materialovedeniya. 2016. №1 (85). S. 116–126.
  7. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  8. Kablov E.N., Startsev O.V., Medvedev I.M., Panin S.V. Korrozionnaya agressivnost primorskoy atmosfery. Ch. 1. Faktory vliyaniya (obzor) [Corrosive aggressiveness of the coastal atmosphere. Part 1. Influence factors (review)] // Korroziya: materialy, zashchita. 2013. №12. S. 6–18.
  9. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  10. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallidnyye splavy na osnove titana i nikelya [Intermetallic alloys based on titanium and nickel]. M.: VIAM, 2018. 308 s.
  11. Kablov E.N., Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Study of the structure and properties of heat-resistant alloys based on titanium aluminides with gadolinium microadditives // Inorganic Materials: Applied Research. 2017. Vol. 8. No. 4. P. 634–641.
  12. Zhanga L.T., Itoa K., Vasudevanb V.K., Yamaguchi M. Beneficial effects of O-phase on the hydrogen absorption of Ti–Al–Nb alloys // Journal of Intermetallics. 2001. Vol. 9. P. 1045–1052.
  13. Khadzhiyeva O.G., Grib S.V., Malevich Yu.A., Illarionov A.G. Vliyaniye vodoroda na prevrashcheniya v splave na osnove intermetallida Ti2AlNb [Beneficial effects of O-phase on the hydrogen absorption of Ti–Al–Nb alloys] // Sb. dokl. VIII Vseros. shkoly-konf. molodykh uchenykh «KoMU-2010». Izhevsk, 2010. S. 108–109.
  14. Laptev A., Kurs M., Lonskaya N., Davydov D., Averina A. Investigation of corrosion damage of hydration aluminum alloys at full-scale accelerated tests // International Journal of Engineering and Technology. 2018. Vol. 7. No. 4. P. 5061–5066.
  15. Knight S.P., Salsgaras M., Trueman A.R. The study of intergranular corrosion in aircraft aluminum alloys using X-ray tomography // Corrosion science. 2011. No. 53. P. 727–734.
  16. Soltis J. Passivity breakdown, pit initiation and propagation of pits in metallic materials // Corrosion Science. 2015. No. 90. P. 5–22.
  17. Zhilikov V.P., Karimova S.A., Leshko S.S., Chesnokov D.V. Issledovanie dinamiki korrozii alyuminievyh splavov pri ispytanii v kamere solevogo tumana (KST) [Research of dynamics of corrosion of aluminum alloys when testing in the salt spray chamber (SSC)] // Aviacionnye materialy i tehnologii. 2012. №4. S. 18–22.