The influence of the spheroidization process on the fractional composition and morphology of alloy VKNA-4U in a particle-reinforced sheath Al2O3–Y2O3

Rodionov A.I., Efimochkin I.Yu., Samokhin A.V., Sinayskiy M.A.
Rodionov A.I., Efimochkin I.Yu., Samokhin A.V., Sinayskiy M.A. The influence of the spheroidization process on the fractional composition and morphology of alloy VKNA-4U in a particle-reinforced sheath Al2O3–Y2O3 // Proceedings of VIAM. 2019. No. 11. DOI: 10.18577/2307-6046-2019-0-11-12-21. URL: https://www.viam-works.ru/en/journal/2019/11/2
Keywords
VKNA-4U alloy, mechanical alloying, plasma spheroidization, reinforcing filler.
Abstract

This article discusses the influence of the plasma spheroidization process on the morphology, microstructure and fractional composition of the VKNA-4U alloy reinforced with Al2O3–Y2O3 particles. During the experiment, it was found that the process of spheroidization significantly affects the morphology of the granuls. Studies show how the morphology of particles changes. After machining, the particles have a fragmentation shape. Due to the process of spheroidization, the granuls take a rounded shape, which affects such a parameter as fluidity, which is necessary for use in plants for additive manufacturing. When analyzing the microstructure, it was found that the particles of the reinforcing filler after plasma spheroidization are shifted to the surface of the granule, in contrast to the initial state after mechanical doping, where the particles of the reinforcing filler are evenly distributed in the volume of the granules.

Reference list
  1. Casati R., Vedani M. Metal Matrix Composites Reinforced by Nano-Particles: A Review // Metals. 2014. Vol. 4. P. 65–83.
  2. Tjong S.C. Novel nanoparticle-reinforced metal matrix composites with enhanced mechanical properties // Advanced Engineering Materials. 2007. Vol. 9. P. 639–652.
  3. Sanaty-Zadeh A. Comparison between current models for the strength of particulate-reinforced metal matrix nanocomposites with emphasis on consideration of Hall–Petch effect // Materials Science and Engineering. 2012. Vol. 531. P. 112–118.
  4. Viswanathan V., Laha T., Balani K. et al. Challenges and advances in nanocomposite processing techniques // Materials Science and Engineering: R. 2006. Vol. 54 (5). P. 121–285.
  5. Dovbysh V.M., Zabednov P.V., Zlenko M.A. Additivnyye tekhnologii i izdeliya iz metalla [Additive technologies and metal products]. Available at: http://nami.ru/upload/AT_metall.pdf (accessed: October 08, 2019).
  6. Frazier W.E. Metal Additive Manufacturing: A Review // Journal of Materials Engineering and Performance. 2014. Vol. 23(6). P. 1917–1928.
  7. Emmelmann C., Kranz J., Herzog D., Wycisk E. Laser Additive Manufacturing of Metals, Laser Technology in Biomimetics // Biological and Medical Physics, Biomedical Engineering. 2013. P. 143–162.
  8. Kumar S., Kruth J.-P. Composites by rapid prototyping technology // Materials and Design. 2010. Vol. 31. P. 850–856.
  9. Song B., Dong S., Coddet C. Rapid in-situ fabrication of Fe/SiC bulk nanocomposites by selective laser melting directly from a mixed powder of micro-sized Fe and micro-sized SiC // Scripta Materialia. 2014. Vol. 75. P. 90–93.
  10. Dadbakhsh S., Hao L., Jerrard P.G.E., Zhang D.Z. Experimental investigation on selective laser melting behaviour and processing windows of in situ reacted Al/Fe2O3 powder mixture // Powder Technology. 2012. Vol. 231. P. 112–121.
  11. Simchi A., Godlinski D. Effect of SiC particles on the laser sintering of Al–7Si–0.3Mg alloy // Scripta Materialia. 2008. Vol. 59. No. 2. P. 199–202.
  12. Singha S.S., Royb D., Mitraa R. et al. Studies on laser sintering of mechanically alloyed Al50Ti40Si10 composite // Materials Science and Engineering: A. 2009. Vol. 501. No. 1–2. P. 242–247.
  13. Gua D., Meiners W. Microstructure characteristics and formation mechanisms of in situ WC cemented carbide based hardmetals prepared by Selective Laser Melting // Materials Science and Engineering: A. 2010. Vol. 527. No. 29–30. P. 7585–7592.
  14. Gu D., Shen Y., Lu Z. Preparation of TiN–Ti5Si3 in-situ composites by Selective Laser Melting // Materials Letters. 2009. Vol. 63. No. 18–19. P. 1577–1579.
  15. Gu D., Wang Z., Shen Y. et al. In-situ TiC particle reinforced Ti–Al matrix composites: Powder preparation by mechanical alloying and Selective Laser Melting behavior // Applied Surface Science. 2009. Vol. 255. No. 22. P. 9230–9240.
  16. Zhang D., Cai Q., Liu J., He J., Li R. Microstructural evolvement and formation of selective laser melting W–Ni–Cu composite powder // The International Journal of Advanced Manufacturing Technology. 2013. Vol. 67. P. 2233–2242.
  17. Biedunkiewicz A., Biedunkiewicz W., Figiel P., Grzesiak D. Preparation of stainless steel-TiC composite by selective laser melting // Chemike Listy. 2011. Vol. 105. P. 773–774.
  18. Ghosh S.K., Saha P., Kishore S. Influence of size and volume fraction of SiC particulates on properties of ex situ reinforced Al–4.5Cu–3Mg metal matrix composite prepared by direct metal laser sintering process // Materials Science and Engineering. A. 2010. Vol. 527. No. 18–19. P. 4694–4701.
  19. Nizkotemperaturnaya plazma / pod red. M.F. Zhukova [Low-temperature plasma / ed. M.F. Zhukov]. Novosibirsk: Nauka, 1999. T.17: Elektrodugovyye generatory termicheskoy plazmy. 712 s.
  20. Tsvetkov Yu.V., Panfilov S.A. Nizkotemperaturnaya plazma v protsessakh vosstanovleniya [Low-temperature plasma in the recovery process]. M.: Nauka, 1980. 360 s.
  21. Tsvetkov Yu.V. Plasma metallurgy. Current state, problems and prospects // Pure and Applied Chemistry. 1999. Vol. 71. No. 10. P. 1853–1862.
  22. Alekseev N.V., Grechikov M.I., Samokhin A.V., Tsvetkov Yu.V. Upravleniye dispersnostyu metallicheskikh poroshkov, poluchayemykh v protsessakh plazmennogo vosstanovleniya [Dispersion control of metal powders obtained in plasma reduction processes] // Fizika i khimiya obrabotki materialov. 1997. №6. S. 54–60.
  23. Alekseev N.V., Samokhin A.V., Tsvetkov Yu.V. Sintez nanoporoshkov karbonitrida titana pri vzaimodeystvii tetrakhlorida titana s uglevodorodno-vozdushnoy plazmoy [Synthesis of nanopowders of titanium carbonitride in the interaction of titanium tetrachloride with hydrocarbon-air plasma] // Khimiya vysokikh energiy. 1999. T. 33. №3. S. 238–242.
  24. Alekseyv N.V., Balikhin I.L., Kurkin E.N. i dr. Formirovaniye ultradispersnogo poroshka oksida alyuminiya v usloviyakh ogranichennoy strui vozdushnoy plazmy [The formation of ultrafine aluminum oxide powder in a limited jet of air plasma] // Fizika i khimiya obrabotki materialov. 1994. №4–5. S.72–78.
  25. Alekseev N.V., Agafonov K.N., Kurkin E.N. i dr. Sintez nanochastits oksida alyuminiya pri okislenii metalla v potokakh termicheskoy plazmy [Synthesis of aluminum oxide nanoparticles during metal oxidation in thermal plasma flows] // Fizika i khimiya obrabotki materialov. 1997. №3. S. 33–38.
  26. Plazmennaya ustanovka dlya polucheniya nanoporoshkov: pat. 2311225. Ros. Federatsiya. №2006110838/15 [Plasma apparatus for producing nanopowders: pat. 2311225. Rus. Federation. No. 2006110838/15]; zayavl. 05.04.06; publ. 27.11.07.
  27. Kotlyarov V.I., Beshkarev V.T., Kartsev V.E. i dr. Polucheniye sfericheskikh poroshkov dlya additivnykh tekhnologiy na osnove metallov IV gruppy [Obtaining spherical powders for additive technologies based on metals of group IV] // Fizika i khimiya obrabotki materialov. 2016. №2. S. 63–70.
  28. Tsvetkov Yu.V., Samokhin A.V., Fadeyev A.A. i dr. Sferoidizatsiya metallicheskikh poroshkov v termicheskoy plazme elektrodugovogo razryada [Spheroidization of metal powders in thermal plasma of an electric arc discharge] // Tekhnologiya legkikh splavov. 2016. №2. S.19–24.
  29. Kotlyarov V.I., Beshkarev V.T., Yuzhakova E.A. i dr. Puti povysheniya kachestva poroshkov na osnove titana dlya additivnykh tekhnologiy [Ways to improve the quality of titanium-based powders for additive technologies] // Sb. dokl. III Vseros. nauch.-tekhnich. konf. «Rol' fundamental'nykh issledovaniy pri realizatsii «Strategicheskikh napravleniy razvitiya materialov i tekhnologiy ikh pererabotki na period do 2030 goda». M.: VIAM, 2016. S. 18.
  30. Kotlyarov V.I., Beshkarev V.T., Kartsev V.E. i dr. Polucheniye poroshkov na osnove titana dlya additivnykh tekhnologiy [Obtaining powders based on titanium for additive technologies] // Sb. dokl. II Mezhdunar. konf. «Additivnyye tekhnologii: nastoyashcheye i budushcheye». M.: VIAM, 2016. S. 2.
  31. Popovich A.A., Razumov N.G., Grigorev A.V. i dr. Polucheniye poroshka splava Nb–16Si metodom mekhanicheskogo legirovaniya i sferoidizatsii v termicheskoy plazme elektrodugovogo razryada dlya additivnykh tekhnologiy [Obtaining Nb–16Si alloy powder by mechanical alloying and spheroidization in thermal plasma of an electric arc discharge for additive technologies] // Izvestiya vuzov. Poroshkovaya metallurgiya i funktsional'nyye pokrytiya. 2017. T. 3. S. 32–40.
  32. Fadeyev A.A. Sferoidizatsiya poroshka nerzhaveyushchey stali v termicheskoy plazme elektrodugovogo razryada [Spheroidization of stainless steel powder in thermal plasma of an electric arc discharge] // Sb. dokl. XIII Ros. yezhegod. konf. molodykh nauchnykh sotrudnikov i aspirantov «Fiziko-khimiya i tekhnologiya neorganicheskikh materialov». M.: IMET RAN, 2016. S. 243–245.
  33. Sposob polucheniya uzkofraktsionnykh sfericheskikh poroshkov iz zharoprochnykh splavov na osnove alyuminida nikelya: pat. 2681022 Ros. Federatsiya. №2018123137 [A method of obtaining narrow fractional spherical powders from heat-resistant alloys based on nickel aluminide: pat. 2681022 Rus. Federation. No. 2018123137]; zayavl. 26.06.18; publ. 01.03.19.
  34. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  35. Kablov E.N., Bondarenko Yu.A., Echin A.B. Razvitiye tekhnologii napravlennoy kristallizatsii liteynykh vysokozharoprochnykh splavov s peremennym upravlyayemym temperaturnym gradiyentom [Development of technology of cast superalloys directional solidification with variable controlled temperature gradient] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  36. Ospennikova O.G., Podieiachev V.N., Stoliankov Yu.V. Tugoplavkie splavy dlia novoi tekhniki [Refractory alloys for innovative equipment] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №10. St. 05. Available at: http://www.viam-works.ru (accessed: April 10, 2019). DOI:10.18577/2307-6046-2016-0-10-5-5.
  37. Kablov E.N., Buntushkin V.P., Bazyleva O.A. Konstruktsionnyye zharoprochnyye materialy na osnove soyedineniya Ni3Al dlya detaley goryachego trakta GTD [Heat-resistant structural materials based on the Ni3Al compound for the details of a hot gas turbine engine] // Tekhnologiya legkikh splavov. 2007. №2. S. 75−80.
  38. Ospennikova O.G., Bazyleva O.A., Evgenov A.G., Arginbayeva E.G., Turenko Ye.Yu. Mikrostrukturnyye i fazovyye prevrashcheniya v intermetallidnom splave na osnove Ni3Al posle vozdeystviya termicheskoy obrabotki i goryachego izostaticheskogo pressovaniya [Microstructural and phase transformations in intermetalliс Ni3Al-based alloy after heat treatment and hot isostatic pressing] // Aviacionnyye materialy i tehnologii. 2016. №S1. S. 36–43. DOI: 10.18577/2071-9140-2016-0-S1-36-43.