Effect of isothermal exposures on hardness evolution of high-strength metastable-β-titanium alloy VT47

Shiryaev A.A., Nochovnaya N.A., Pomelnikova A.S.
Shiryaev A.A., Nochovnaya N.A., Pomelnikova A.S. Effect of isothermal exposures on hardness evolution of high-strength metastable-β-titanium alloy VT47 // Proceedings of VIAM. 2019. No. 10. DOI: 10.18577/2307-6046-2019-0-10-25-33. URL: https://www.viam-works.ru/en/journal/2019/10/3
Keywords
metastable--titanium alloys, VT47, heat treatment, diagram, hardness, microstructure.
Abstract

Rockwell hardness (HRC) studies have been accomplished on samples cut from sheets of metastable-b-titanium alloy VT47 after isothermal exposures (ageing) upon a wide range of temperatures and exposure durations. A diagram and C-shaped alloy hardness curves have been plotted, and a comparative assessment of hardness values with a microstructure was carried out. It has been established that VT47 alloy is hardened significantly (≥40 HRC) by ageing in the temperature range of 400–500°С. The temperature range of 450–500°Сcan be considered to be the most rational from the standpoint of achievable hardness values and required ageing times.

Reference list
  1. Titanium and titanium alloys. Fundamentals and applications / ed. C. Leyens, M. Peters. Wiley–VCH, 2003. 513 p.
  2. Nyakana S.L., Fanning J.C., Boyer R.R. Quick Reference Guide for β Titanium Alloys in the 00s // Journal of Materials Engineering and Performance. 2005. Vol. 14 (6). P. 799–811.
  3. Boyer R.R., Briggs R.D. The Use of β Titanium Alloys in the Aerospace Industry // Journal of Materials Engineering and Performance. 2005. Vol. 14 (6). P. 681–685.
  4. Kablov E.N., Nochovnaya N.A., Gribkov Yu.A., Shiryayev A.A. Razrabotka vysokoprochnogo titanovogo psevdo-β-splava i tekhnologiy polucheniya polufabrikatov iz nego [Development of high-strength titanium pseudo-β-alloy and technologies for producing semi-finished products from it ] // Voprosy materialovedeniya. 2016. №3 (87). S. 23–31.
  5. Ilin A.A., Skvortsova S.V., Dzunovich D.A., Panin P.V., Shalin A.V. Vliyaniye parametrov termicheskoy i termomekhanicheskoy obrabotki na teksturoobrazovaniye v listovykh polufabrikatakh iz titanovykh splavov [Influence of the parameters of thermal and thermomechanical processing on texture formation in sheet semi-finished products from titanium alloys] // Tekhnologiya mashinostroyeniya. 2012. №8. S. 8–12.
  6. Nochovnaya N.A., Panin P.V., Alekseyev E.B., Novak A.V. Zakonomernosti formirovaniya strukturno-fazovogo sostoyaniya splavov na osnove orto- i gamma-alyuminidov titana v protsesse termomekhanicheskoy obrabotki [Patterns of formation of the structural phase state of alloys based on titanium ortho and gamma aluminides during thermomechanical processing] // Vestnik Rossiyskogo fonda fundamental'nykh issledovaniy. 2015. №1 (85). S. 18–26.
  7. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Vysokoprochnyy splav na osnove titana i izdeliye, vypolnennoye iz vysokoprochnogo splava na osnove titana: pat. 2569285 Ros. Federatsiya. №2014153690/02 [High-strength alloy based on titanium and a product made of high-strength alloy based on titanium: pat. 2569285 Rus. Federation. No. 2014153690/02]; zayavl. 29.12.14; opubl. 20.11.15.
  9. Nochovnaya N.A., Shiryayev A.A., Dzunovich D.A., Panin P.V. Issledovaniye khimicheskogo sostava krupnogabaritnogo opytno-promyshlennogo slitka iz novogo vysokolegirovannogo psevdo-b-titanovogo splava VT47 [Study of chemical composition of large-dimensioned experimental-industrial ingot from a new high-alloyed metastable β-titanium alloy VT47] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №1 (61). St. 06. Available at: http://www.viam-works.ru (accessed: June 18, 2019). DOI: 10.18577/2307-6046-2018-0-1-6-6.
  10. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  11. Shiryaev A.A., Antashev V.G. Osobennosti razrabotki vysokoprochnogo samozakalivaiushchegosia vysokotekhnologichnogo psevdo-β-titanovogo splava [Peculiarities of development of advanced high-strength self-hardening high-processable pseudo-β-titanium alloys] // Aviacionnye materialy i tehnologii. 2014. №4. S. 23–30. DOI: 10.18577/2071-9140-2014-0-4-23-30.
  12. Skupov A.A., Panteleev M.D., Ioda E.N., Movenko D.A. Effektivnost primeneniya redkozemelnyh metallov dlya legirovaniya prisadochnyh materialov [The efficiency of rare earth metals for filler materials alloying] // Aviacionnye materialy i tehnologii. 2017. №3 (48). S. 14–19. DOI: 10.18577/2071-9140-2017-0-3-14-19.
  13. Lyasotskaya V.S. Termicheskaya obrabotka svarnykh soyedineniy titanovykh splavov [Heat treatment of welded joints of titanium alloys]. M.: Ekomet, 2003. 352 s.
  14. Dehghan-Manshadi A., Dippenaar R.J. Development of α-phase morphologies during low temperature isothermal heat treatment of a Ti–5Al–5Mo–5V–3Cr alloy // Material Science and Engineering A. 2011. Vol. 528. P. 1833–1839.
  15. Tetyukhin V.V., Gribkov Yu.A., Moder N.I., Vodolazskiy V.F. Issledovaniye strukturnykh i fazovykh prevrashcheniy v splave VT35 pri izgotovlenii tonkikh listov [Study of structural and phase transformations in VT35 alloy in the manufacture of thin sheets] // Titan. 1996. №1 (9). S. 25–29.
  16. Furuhara T., Maki T., Makino T. Microstructure control by thermomechanical processing in β-Ti-15-3 alloy // Journal of Materials Processing Technology. 2001. Vol. 117. P. 318–323.
  17. Martin B., Samimi P., Collins P. Engineered, spatially varying isothermal holds: enabling combinatorial studies of temperature effects, as applied to metastable titanium alloy β-21S // Metallography, Microstructure, and Analysis. 2017. No. 6. P. 216–220.
  18. Terlinde G., Fischer G. Beta titanium alloys // Proceedings of 8th World Conference on Titanium «Titanium 95: Science and technology». The Institute of Materials, UK. 1996. P. 2177–2194.
  19. Zhanal P., Harcuba P., Hajek J. et al. Evolution of ɷ phase during heating of metastable β titanium alloy Ti–15Mo // Journal of Material Science. 2018. Vol. 53. P. 837–845.
  20. Ivasishin O.M., Markovsky P.E., Matviychuk Yu.V., Semiatin S.L. Precipitation and recrystallization behavior of beta titanium alloys during continuous heat treatment // Metallurgical and Materials Transactions A. 2003. Vol. 34A. P. 147–158.
  21. Furuhara T. Role of defects on microstructure of beta titanium alloys // Metals and Materials. 2000. Vol. 6. No. 3. P. 221–224.
  22. Clement N., Lenain A., Jacques P.J. Mechanical property optimization via microstructural control of new metastable beta titanium alloys // JOM. 2007. Vol. 1. P. 50–53.
  23. Zhou Z., Fei Y., Lai M. et al. Microstructure and mechanical properties of new metastable β type titanium alloy // Transactions of Nonferrous Metals Society of China. 2010. Vol. 20. P. 2253–2258.
  24. Novak A.V., Alekseev E.B., Ivanov V.I., Dzunovich D.A. Izuchenie vliyaniya parametrov zakalki na strukturu i tverdost intermetallidnogo titanovogo orto-splava VTI-4 [The study of the quenching parameters influence on structure and hardness of orthorhombic titanium aluminide alloy VТI-4] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №2. St. 05. Available at: http://www.viam-works.ru (accessed: June 18, 2019). DOI: 10.18577/2307-6046-2018-0-2-5-5.
  25. Schmidt P., El-Chaikh A., Christ H.-J. Effect of Duplex Aging on the Initiation and Propagation of Fatigue Cracks in the Solute-rich Metastable β Titanium Alloy Ti 38-6-44 // Metallurgical and Materials Transactions A. 2011. Vol. 42A. P. 2652–2667.
  26. Shiryayev A.A., Nochovnaya N.A. Issledovaniye formirovaniya struktury v protsesse stareniya vysokoprochnogo psevdo-b titanovogo splava VT47 [Investigation of the structure formation during aging of high-strength pseudo-β titanium alloy VT47] // Metallurg. 2019. №9. S. 76–84.