Express method of a comparative assessment properties levels of materials

Podzhivotov N.Y.
Podzhivotov N.Y. Express method of a comparative assessment properties levels of materials // Proceedings of VIAM. 2019. No. 10. DOI: 10.18577/2307-6046-2019-0-10-111-124. URL: https://www.viam-works.ru/en/journal/2019/10/11
Keywords
probabilistic estimates, experimental data, levels of properties, characteristics of materials, analysis of data, comparison, preferential choice.
Abstract

The article is about the express method of a comparative assessment of levels properties of materials on experimental data in the conditions of the empirical uncertainty. The choice of a preferential material is carried out by means of comparisons of probabilistic estimates levels of values of materials characteristics with close levels of properties. The method allows to carry out the complex ranging of compared materials on level properties and to reveal the preferential material possessing with the greatest levels of properties. The characteristics of materials on which comparison is carried out, are considered the equivalent for the choice.

Reference list
  1. Normy letnoy godnosti samoletov transportnoy kategorii: AP-23 [Airworthiness standards for transport category aircraft: AP-23]: utv. Postanovleniyem 34-y sessii Soveta po aviatsii i ispolzovaniyu vozdushnogo prostranstva 06.12.2013. 4-ye izd. s popravkami 1–5. M.: Aviaizdat, 2014. 195 s.
  2. Primeneniye konstruktsionnykh metallicheskikh materialov i opredeleniye iz raschetnykh kharakteristik: RTS-AP23(25, 27, 29)-613 / Mezhgosudarstvennyy aviatsionnyy komitet [The use of structural metal materials and the determination of the calculated characteristics: RC-AP23 (25, 27, 29) -613 / Interstate Aviation Committee]. M.: Aviaizdat, 2002. 24 s.
  3. Raschetnyye znacheniya kharakteristik aviatsionnykh metallicheskikh konstruktsionnykh materialov: spravochnik [The calculated values of the characteristics of aircraft metal structural materials: a reference]. M.: OAK, 2012. Vyp. 4. 302 s.
  4. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  5. Kablov E.N., Grinevich A.V., Yerasov V.S. Kharakteristiki prochnosti metallicheskikh aviatsionnykh materialov i ikh raschetnyye znacheniya [Strength characteristics of metallic aviation materials and their calculated values] // 75 let. Aviatsionnyye materialy. Izbrannyye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 370–379.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Kablov E.N. Marketing materialovedeniya, aviastroyeniya i promyshlennosti: nastoyashcheye i budushcheye [Marketing of materials science, aircraft building and industry: present and future] // Direktor po marketingu i sbytu. 2017. №5–6. S. 40–44.
  8. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of a new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  9. Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Kvalifikatsionnye ispytaniya i issledovaniya prochnosti aviatsionnyh materialov [Qualification tests and researches of durability of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  10. Konovalov V.V., Dubinskiy S.V., Makarov A.D., Dotsenko A.M. Issledovaniye korrelyatsionnykh zavisimostey mezhdu mekhanicheskimi svoystvami aviatsionnykh materialov // Aviatsionnyye materialy i tekhnologii. 2018. №2 (51). S. 40–46. DOI: 10.18577/2071-9140-2018-0-2-40-46.
  11. Podzhivotov N.Yu., Kablov E.N., Antipov V.V., Erasov V.S., Serebrennikova N.Yu., Abdullin M.R., Limonin M.V. Sloistye metallopolimernyye materialy v elementakh konstruktsii vozdushnykh sudov [Layered metal-polymer materials in aircraft structural elements] // Perspektivnyye materialy. 2016. №10. S. 5–19.
  12. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PCM mechanical properties] // Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  13. Gaskarov D.V., Shapovalov V.I. Malaya vyborka [Small sample]. M.: Statistika, 1978. 248 s.
  14. Gorbunova E.B. Metod neparametricheskoy otsenki zakona raspredeleniya sluchaynogo parametra po malomu chislu nablyudeniy // Inzhenernyy vestnik Dona. 2014. №3. Available at: http://ivdon.ru/ru/magazine/archive/n3y2014/2516 (accessed: September 24, 2019).
  15. Grinevich A.V., Lutsenko A.N., Karimova S.A. Raschetnye harakteristiki metallicheskih materialov s uchetom vlazhnosti [The design characteristic of metallic materials taking into account the humidity] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 10. Available at: http://www.viam-works.ru (accessed: September 23, 2019). DOI: 10.18577/2307-6046-2014-0-7-10-10.
  16. Lutsenko A.N., Slavin A.V., Erasov V.S., Khvackij K.K. Prochnostnye ispytaniya i issledovaniya aviacionnyh materialov [Strength tests and researches of aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 527–546. DOI: 10.18577/2071-9140-2017-0-S-527-546.
  17. Erasov V.S., Podzhivotov N.Yu. Metody otsenki raschetnykh znacheniy kharakteristik prochnosti aviatsionnykh materialov v Rossii i za rubezhom [Methods for assessing the calculated values of the strength characteristics of aviation materials in Russia and abroad] // Kommentarii k standartam, TU, sertifikatam: prilozheniye k zhurnalu «Vse materialy. Entsiklopedicheskiy spravochnik». 2013. №12. S. 2–8.
  18. Podzhivotov N.Yu., Erasov V.S., Oreshko E.I. O metodakh otsenki staticheskoy prochnosti materialov, poluchennykh s pomoshch'yu additivnykh tekhnologicheskikh protsessov [About methods for assessing the static strength of materials obtained using additive processes] // Kommentarii k standartam, TU, sertifikatam: prilozheniye k zhurnalu «Vse materialy. Entsiklopedicheskiy spravochnik». 2017. №10. S. 54–60.
  19. Erasov V.S., Yakovlev N.O., Avtaev V.V. Sovremennoe sostoyanie laboratorii imeni professora S.I. Kishkinoj [Contemporary state of laboratory after the named of professor S.I. Kishkina] //Aviacionnye materialy i tehnologii. 2014. №S4. S. 136–139.
  20. Bobyr M.V., Titov D.V., Kulabukhov S.A. Otsenka prognozirovaniya prinyatiya resheniy v usloviyakh neopredelennosti [Assessment of forecasting decision making in conditions of uncertainty] // Telekommunikatsii. 2015. №11. C. 39–44.
  21. Zolotorev V.M. Sovremennaya teoriya summirovaniya nezavisimykh sluchaynykh velichin [The modern theory of summation of independent random variables]. M.: Nauka, 1986. 416 s.
  22. Kryanev A.V., Lukin G.V. Matematicheskiye metody obrabotki neopredelennykh dannykh [Mathematical methods for processing uncertain data]. M.: Fizmatlit, 2003. 216 s.
  23. Lapko A.V., Sharkov N.A. Neparametricheskiye metody obnaruzheniya zakonomernostey v usloviyakh malykh vyborok [Nonparametric methods for detecting patterns in small samples] // Priborostroyeniye, 2008. T. 51. №8. S. 62–67.
  24. Glukhov V.V., Anufriyev D.V. Butstrep-protsedury opredeleniya tochnostnykh kharakteristik [Bootstrap procedures for determining accuracy characteristics] // Nauchnyy vestnik MGTU GA. 2005. №89 (7). C. 30–35.
  25. Samoylenko A.P., Gorbunova E.B. Metod vosstanovleniya plotnosti veroyatnostey prognoziruyemoy sluchaynoy velichiny po ukorochennoy vyborke dannykh [A method for reconstructing the probability density of a predicted random variable from a shortened data sample] // Nelineynyy mir. 2015. №6. S. 10–17.
  26. Shitikov V.K., Rozenberg G.S. Randomizatsiya i butstrep: statisticheskiy analiz v biologii i ekologii s ispolzovaniyem R [Randomization and bootstrap: a statistical analysis in biology and ecology using R]. Tolyatti: Kassandra, 2013. 314 s.