Magnetoplastic and magnetomechanic effects in aluminum alloys with magnetostrictive micro inclusions
Morgunov R.B., Valeev R.A., Skvortsov A.A., Korolev D.V., Piskorsky V.P., Kunitsyna E.I., Kucheryaev V.V., Koplak O.V. Magnetoplastic and magnetomechanic effects in aluminum alloys with magnetostrictive micro inclusions // Proceedings of VIAM. 2019. No. 10. DOI: 10.18577/2307-6046-2019-0-10-3-13. URL: https://www.viam-works.ru/en/journal/2019/10/1
Keywords
creep, microhardness, dislocation, magnetoplasticity, magnetostriction.
Abstract
Effect of magnetic field on mechanical properties of aluminum alloys and magnetic after-effects are discussed. The FeAl microinclusions providing internal stresses in aluminum matrix were revealed. These stresses affect creep, microharness and dislocation dynamics in magnetic field. The opposite effect, which can be called magnetomechanic or piezoelectric, is also repor-ted. It consists in increasing the coercive force of microinclusions caused by plastic deformation of aluminum. These experiments show that microinclusions can be used as sensors of mechanical stresses, with the help of which residual stresses in materials can be measured.
Reference list
- Skvortsov A., Pshonkin D., Kunitsyna E., Morgunov R., Beaugnon E. Softening of the Al–Mg–Si–Fe alloy under magnetostriction of FeAl microinclusions // Journal of Applied Physics. 2019. Vol. 125. No. 2. P. 023903.
- Skvortsov A.A., Morgunov R.B., Pshonkin D.E., Piskorskii V.P., Valeev R.A. Magnetic Memory in Plasticity of an Aluminum Alloy with Iron Inclusions // Physics of the Solid State. 2019. Vol. 61. No. 6. P. 1023–1029.
- Morgunov R.B. Spinovaya mikromekhanika v fizike plastichnosti [Spin micromechanics in the physics of plasticity] // Uspekhi fizicheskikh nauk. 2004. T. 174. S. 131–153. DOI: 10.3367/UFNr.0174.200402c.0131.
- Morgunov R.B., Buchachenko A.L. Magnetic field response of NaCl:Eu crystal plasticity due to spin-dependent Eu2+ aggregation // Physical Review B. 2010. Vol. 82. P. 014115.
- Beaugnon E. 3D physical modeling of anisotropic grain growth at high temperature in local strong magnetic force field // Science Technology of Advanced Materials. 2008. Vol. 9. P. 024201. DOI: 10.1088/1468-6996/9/2/024201.
- Molodov D.A., Bollmann C., Gottstein G. Impact of a magnetic field on the annealing behavior of cold rolled titanium // Materials Science and Engineering A. 2007. Vol. 467. P. 71. DOI: 10.1016/j.msea.2007.02.084.
- Bhaumik S., Molodova X., Molodov D.A., Gottstein G. Magnetically enhanced recrystallization in an aluminum alloy // Scripta Materialia. 2006. Vol. 55. P. 995. DOI: 10.1016/j.scriptamat.2006.08.018.
- Tournier R.F., Beaugnon E. Texturing by cooling a metallic melt in a magnetic field // Science Technology of Advanced Materials. 2009. Vol. 10. P. 014501. DOI: 10.1088/1468-6996/10/1/014501.
- Li H., Liu S., Jie J. et al. Effect of pulsed magnetic field on the grain refinement and mechanical properties of 6063 aluminum alloy by direct chill casting // International Journal of Advanced Manufacturing Technology. 2017. Vol. 93. P. 3033. DOI: 10.1007/s00170-017-0724-0.
- Li C.J., Yang H., Ren Z.M. et al. On Nucleation Temperature of Pure Aluminum in Magnetic Fields // Progress in Electromagnetics Research Letters. 2010. Vol. 15. P. 45. DOI: 10.2528/PIERL10041412.
- Bustos O., Ordoñez S., Colás R. Rheological and microstructural study of A356 alloy solidified under magnetic stirring // International Journal of Cast Metals Research. 2013. Vol. 7. No. 1. P. 29–37.
- Kablov E.N., Ospennikova O.G., Piskorskij V.P., Valeev R.A. i dr. Fazovyj sostav spechennyh materialov sistemy Nd–Dy–Fe–Co–B [Phase composition of Nd–Dy–Fe–Co–B sintered materials] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 95–100. DOI: 10.18577/2071-9140-2014-0-s5-95-100.
- Kablov E.N., Ospennikova O.G., Piskorskij V.P., Rezchikova I.I., Valeev R.A., Davydova E.A. Fazovyj sostav spechennyh materialov sistemy Pr–Dy–Fe–Co–B [Phase composition of the Pr–Dy–Fe–Co–B sintered materials] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 5–10. DOI: 10.18577/2071-9140-2015-0-S2-5-10.
- Kablov E.N., Ospennikova O.G., Cherednichenko I.V., Rezchikova I.I., Valeev R.A., Piskorskij V.P. Vliyanie soderzhaniya medi na fazovyj sostav i magnitnye svojstva termostabilnyh spechennyh magnitov sistem Nd–Dy–Fe–Co–B i Pr–Dy–Fe–Co–B [Influence of Cu content to phase structure and magnetic properties of thermostable sintered magnets of Nd–Dy–Fe–Co–B and Pr–Dy–Fe–Co–B systems] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 11–19. DOI: 10.18577/2071-9140-2015-0-S2-11-19.
- Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. Termodinamicheskiy analiz magnitoplasticheskikh effektov v «nemagnitnykh» metallakh [Thermodynamics analysis of magnetoplastic effects in «non-magnetic» metals] // trudy viam: elektron. nauch.-tekhnich. zhurn. 2018. №12 (72). St. 09. Available at: http://www.viam-works.ru (accessed: September 20, 2019). DOI: 10.18577/2307-6046-2018-0-12-79-87.