The calculation of the ratio of the components of the prepreg stamps VPS-53/120, determination of physico-mechanical and operational characteristics of GRP

Melnikov D.A., Petrova A.P., Gromova A.A., Sokolov I.I., Raskutin A.E.
Melnikov D.A., Petrova A.P., Gromova A.A., Sokolov I.I., Raskutin A.E. The calculation of the ratio of the components of the prepreg stamps VPS-53/120, determination of physico-mechanical and operational characteristics of GRP // Proceedings of VIAM. 2019. No. 1. DOI: 10.18577/2307-6046-2019-0-1-92-104. URL: https://www.viam-works.ru/en/journal/2019/1/10
Keywords
GRP, contact corrosion, prepreg, PCM, physical and mechanical, performance characteristics.
Abstract

Process of selection of ratio of components of prepreg is described. The data on electrochemical corrosion in the contact zone of «metal–carbon» fiber and describes a method of protection against contact corrosion by isolating the carbon-plastic metal layer prepreg GRP. The initial components of prepreg GRP VPS-53/120, designed to prevent contact corrosion between metal and carbon fiber, were selected. Two methods for calculating the surface density of the binder and prepreg are described. The ranges of permissible dispersion of the surface densities of the binder and prepreg film are calculated taking into account the dispersion of the surface density of GRP and the selected range of the binder content in the prepreg. The actual values of the prepreg characteristics of the VPS-53/120 brand are determined and their statistical analysis is carried out, the high convergence of the actual values with the calculated ones is shown. Physical-mechanical and operational characteristics of GRP of the VPS-53/120 brand are defined.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Sivakov D.V., Gulyaev I.N., Sorokin K.V., Fedotov M.Yu., Goncharov V.A. Metody issledovaniya konstrukcionnyh kompozicionnyh materialov s integrirovannoj elektromehanicheskoj sistemoj [Methods of research of constructional composite materials with the integrated electromechanical system] // Aviacionnye materialy i tehnologii. 2010. №4. S. 17–20.
  3. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  4. Kablov E.N., Kirillov V.N., Zhirnov A.D., Startsev O.V., Vapirov Yu.M. Tsentry dlya klimaticheskikh ispytaniy aviatsionnykh PKM [Climate Test Centers for Aviation PCM] // Aviatsionnaya promyshlennost. 2009. №4. S. 36–46.
  5. Melnikov D.A., Ilichev A.V., Vavilova M.I. Sravnenie standartov dlia provedeniia mekha-nicheskikh ispytanii stekloplastikov na szhatie [Comparison of standards for carrying out mechanical tests of GRP compression strength] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №3 (51). St. 06. Available at: http://www.viam-works.ru (accessed: June 21, 2018). DOI: 10.18577/2307-6046-2017-0-3-6-6.
  6. Karimova S.A., Pavlovskaya T.G., Chesnokov D.V., Semenova L.V. Korrozionnaya aktivnost ugleplastikov i zashchita metallicheskikh silovykh konstruktsiy v kontakte s ugleplastikom [Corrosion activity of carbon fiber plastic and protection of metal power structures in contact with carbon plastic] // Rossiyskiy khimicheskiy zhurnal. 2010. T. 54. №1. S. 110–116.
  7. Sinyavskiy V.S., Valkov V.D., Kalinin V.D. Korroziya i zashchita alyuminiyevykh splavov [Corrosion and protection of aluminum alloys]. M.: Metallurgiya, 1986. 368 s.
  8. Bosze E., Nutt S. Potential for Galvanic Corrosion between Carbon Fibers and Al Wires in ACCC/TW Conductor // Gill Foundation Composites Center University of Southern California. 2008. Available at: https://www.ctcglobal.com/ftp/Reports/Galvanic_Corrosion_Test.pdf (accessed: September 20, 2018).
  9. Kiselev B.A. Stekloplastiki. M.: Gos. nauch.-tekhnich. izd-vo khim. lit., 1961. 240 s.
  10. Gunyayev G.M. Struktura i svoystva polimernykh voloknistykh kompozitov [Structure and properties of polymer fiber composites]. M.: Khimiya, 1981. 232 s.
  11. Skudra A.M., Bulave F.Ya. Prochnost armirovannykh plastikov [Strength of reinforced plastics]. M.: Khimiya, 1982. 216 s.
  12. Tarnopolskiy Yu.M., Zhigun I.G., Polyakov V.A. Prostranstvenno-armirovannyye kompozitnyye materialy: spravochnik [Spatially reinforced composite materials: a guide]. M.: Mashinostroyeniye, 1987. 224 s.
  13. Tarnopolskiy Yu.M., Skudra A.M. Konstruktsionnaya prochnost i deformativnost stekloplastikov [Structural strength and deformability of fiberglass]. Riga: Zinatne, 1966. 260 s.
  14. Nemets Ya., Serensen S.V., Strelyayev V.S. Prochnost plastmass [Durability of plastics]. M.: Mashinostroyeniye, 1970. 335 s.
  15. Kucher N.K., Dveyrin A.Z., Zemtsov M.P., Ankyanets O.K. Kharakteristiki uprugosti sloistykh tkanykh stekloplastikov [Characteristics of elasticity of laminated woven fiberglass] // Problemy prochnosti. 2004. №6. S. 26–32.
  16. Kucher N.K., Dveyrin A.Z., Zarazovskiy M.N., Zemtsov M.P. Deformirovaniye sloistykh stekloplastikov, armirovannykh tkan'yu satinovoy struktury pri komnatnoy i nizkikh temperaturakh [Deformation of laminated glass-reinforced plastics reinforced with satin-structure fabric at room and low temperatures] // Mekhanika kompozitnykh materialov. 2004. №3. S. 341–354.
  17. Melnikov D.A., Gromova A.A., Raskutin A.E., Kurnosov A.O. Teoreticheskij raschet i eksperimentalnoe opredelenie modulya uprugosti i prochnosti stekloplastika VPS-53/120 [Theoretical calculation and experimental determination of modulus of elasticity and strength of GRP VPS-53/120] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №1 (49). St. 08. Available at: http://www.viam-works.ru (accessed: July 12, 2018). DOI: 10.18577/2307-6046-2017-0-1-8-8.
  18. Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokoleniya [Modern production technologies of polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 07. Available at: http://www.viam-works.ru (accessed: September 12, 2018).
  19. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polimernyye kompozitsionnyye materialy novogo pokoleniya na osnove svyazuyushchego VSE-1212 i napolniteley, alternativnykh napolnitelyam firm Porcher Ind. i Toho Tenax [Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax] // Aviacionnye materialy i tehnologii. 2018. №3 (52). S. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  20. Kurnosov A.O., Vavilova M.I., Melnikov D.A. Tehnologii proizvodstva steklyannyh napolnitelej i issledovanie vliyaniya appretiruyushhego veshhestva na fiziko-mehanicheskie harakteristiki stekloplastikov [Manufacturing technologies of glass fillers and study of effects of finishing material on physical and mechanical properties of fiberglass plastics] // Aviacionnye materialy i tehnologii. 2018. №1 (50). S. 64–70. DOI: 10.18577/2071-9140-2018-0-1-64-70.