Effect of preliminary etching of alloy ML5 before plasma electrolytic oxidation
Kozlov I.A., Vinogradov S.S., Uridiya Z.P., Duyunova V.A., Manchenko V.A. Effect of preliminary etching of alloy ML5 before plasma electrolytic oxidation // Proceedings of VIAM. 2018. No. 9. DOI: 10.18577/2307-6046-2018-0-9-32-42. URL: https://www.viam-works.ru/en/journal/2018/9/4
Keywords
plasma electrolytic oxidation, microarc oxidation, anodic oxidation, magnesium alloys, coating structure, surface preparation.
Abstract
Protection of magnesium alloys by method of plasma electrolytic oxidation is the most perspective. Protective properties of received coverings in big degree depend on surface structure of magnesium alloy. Availability on surface of alloy the phases containing aluminum, the Mg17Al12 type leads to covering forming with large amount of through defects. Preliminary etching of magnesium alloy in solution of alkali or fluoric acid significantly reduces porosity of covering and, therefore, increases its protective properties.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Volkova E.F. Analiz i itogi Mezhdunarodnoj konferencii «Magnij–21. Novye gorizonty» (obzor) [The analysis and results of the International conference «Magnesium–21. Broad horizons» (review)] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 86–94. DOI: 10.18577/2071-9140-2016-0-1-86-94.
- Volkova E.F., Mostyaev I.V. Vliyanie nekotorykh primesej na strukturu, fazovyj sostav i svojstva magnievykh splavov, soderzhashchikh redkozemelnye element [Influence of some impurities on the structure, phase composition and properties of magnesium alloys containing rare-earth elements] // Metally. 2018. №1. S. 64–71.
- Kablov E.N. Korroziya ili zhizn [Corrosion or life] // Nauka i zhizn. 2012. №11. S. 16–21.
- Kozlova A.A., Kondrashov Je.K. Sistemy lakokrasochnyh pokrytij dlja protivokorro-zionnoj zashhity magnievyh splavov [Systems of paint coatings for anticorrosive protection of magnesium alloys] //Aviacionnye materialy i tehnologii. 2014. №2. S. 44–47. DOI: 10.18577/2071-9140-2014-0-2-44-47.
- Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviatsionnoj tekhniki [Main results and directions of development of materials for advanced aircraft technology] // 75 let. Aviacionnye materialy. Izbrannye trudy VIAM 1932–2007: yubil. nauch.-tekhnich. sb. M.: VIAM, 2007. S. 20–26.
- Darband B.G., Aliofkhazraei M., Hamghalam P., Valizade N. Plasma electrolytic oxidation of magnesium and its alloys: Mechanism, properties and applications // Journal of Magnesium and Alloys. 2017. Vol. 5. P. 74–132.
- Vladimirov B.V., Krit B.L., Morozova N.V., Epelfeld A.V. Issledovanie svojstv modifitsirovannogo magnievogo splava MA21, prednaznachennogo dlya ispolzovaniya v biosensornykh sistemakh [Investigation of the properties of the modified magnesium alloy MA21, intended for use in biosensor systems] // Biotekhnologiya i kachestvo zhizni: materialy Mezhdunar. nauch.-praktich. konf. 2014. S. 179–180.
- Kozlov I.A., Vinogradov S.S., Naprienko S.A. Struktura i svojstva PEO-pokrytiya, formiruemogo na splave ML5 v silikatno-fosfatnom elektrolite [Structure and properties of the PEO coating formed on the ML5 alloy in a silicate-phosphate electrolyte] // Korroziya: materialy, zashchita. 2017. №8. S. 35–41.
- Rakoch A.G., Gladkova A.A., Schneider O. i dr. Vliyanie katodnykh mikrorazryadov na skorost' obrazovaniya i stroenie pokrytij, formiruemykh na magnievom splave metodom plazmenno-elektroliticheskogo oksidirovaniya [Influence of cathode microdischarges on the rate of formation and structure of coatings formed on a magnesium alloy by the plasma-electrolytic oxidation method] // Perspektivnye materialy. 2014. №5. S. 59–64.
- Vladimirov B.V., Krit B.L., Lyudin V.B., Morozova N.V., Suminov I.V., Epelfeld A.V. Vliyanie sostava elektrolita na svojstva splava MA2-1 pri mikrodugovom oksidirovanii [Influence of the composition of electrolyte on the properties of the alloy MA2-1 with microarc oxidation] // Izvestiya Tomskogo politekhnicheskogo universiteta. 2014. T. 324. №2. S. 143–148.
- Felix Tjiang, Li-Wei Ye, Yan-Jang Huang et al. Effect of processing parameters on soft regime behavior of plasma electrolytic oxidation of magnesium // Ceramics International. 2017. Vol. 43. P. s567–s572.
- Kozlov I.A., Vinogradov S.S., Kulyushina N.V. Vliyanie formy polyarizuyushchikh impulsov na strukturu i zashchitnye svojstva PEO-pokrytiya, formiruemogo na splave ML5 [Influence of the form of the polarizing impulses on structure and protective properties PEO coating formed on alloy ML5] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №8 (56). St. 12. Available at: http://www.viam-works.ru (accessed: April 16, 2018). DOI: 10.18577/2307-6046-2017-0-8-12-12.
- Kozlov I.A., Vinogradov S.S., Kulyushina N.V., Kutyrev A.E., Pastukhov A. S. Vliyanie sootnosheniya amplitud polyarizuyushchego toka na zashchitnye svojstva PEO-pokrytiya, formiruemogo na splave ML5 [Influence of the polarization current amplitude correlation on the protective properties of the PEO coating formed on the ML5 alloy] // Korroziya: materialy, zashchita. 2016. №11. S. 40–48.
- Kozlov I.A., Kulyushina N.V., Kutyrev A.E. Vliyanie formy polyarizuyushchego toka na zashchitnye svojstva plazmennogo elektroliticheskogo pokrytiya na splave ML5 [Influence of the shape of the polarizing current on the protective properties of a plasma electrolytic coating on an ML5 alloy] // Materialovedenie. 2015. №9. S. 25–31.
- Olejnik S.V., Rudnev V.C., Kuzenkov Yu.A. i dr. Zashchitnye svojstva napolnennykh trialkoksisilanami PEO-pokrytij na magnievom splave MA-8 [Protective properties of PEO coatings filled with trialkoxysilanes on magnesium alloy MA-8] // Korroziya: materialy, zashchita. 2016. №12. S. 29–33.
- Olejnik S.V., Rudnev V.C., Kuzenkov YU.A. i dr. Ingibirovannye PEO-pokrytiya na magnievom splave MA-8 [Inhibited PEO coatings on magnesium alloy MA-8] // Korroziya: materialy, zashchita. 2015. №10. S. 39–44.
- Mingo B., Arrabal R., Mohedano M. et al. Influence of sealing post-treatments on the corrosion resistance of PEO coated AZ91 magnesium alloy // Applied Surface Science. 2018. Vol. 433. P. 653–667.
- Chen Y., Yang Y., Zhang W. et al. Influence of second phase on corrosion performance and formation mechanism of PEO coating on AZ91 Mg alloy // Journal of Alloys and Compounds. 2017. Vol. 718. P. 92–103.
- Kukhling Kh. Spravochnik po fizike. Per. s nem. [Handbook of Physics. Trans from Germ.] M.: Mir, 1982. 475 s.