Research of process of out-of-autoclave formation semi-pregs on the basis of carbon fillers (review)

Dushin M.I., Donetskiy K.I., Timoshkov P.N., Karavaev R.Y.
Dushin M.I., Donetskiy K.I., Timoshkov P.N., Karavaev R.Y. Research of process of out-of-autoclave formation semi-pregs on the basis of carbon fillers (review) // Proceedings of VIAM. 2018. No. 9. DOI: 10.18577/2307-6046-2018-0-9-21-31. URL: https://www.viam-works.ru/en/journal/2018/9/3
Keywords
semi-pregs, prepregs, fiber, impregnation, permeability, porosity.
Abstract

The increase in let-out volumes and especially dimensions оf products from composite, has demanded search of cheaper alternatives to avtoklave way of manufacturing of products. Ways of liquid vacuum formation dry preformеs impregnation binding have appeared the cheapest. The arisen problems of receiving high-quality products vacuum formation have led to development semi-pregs, representing fabrics or cordlike fillers which are duplicated with film of the binding. Many manufacturing firms of materials include in the nomenclature of the materials wide ruler semi-pregs. In work researches of processes of receiving polymeric composite materials (PСM) on the basis of developed semi-pregs by means of their formation by means of atmospheric pressure instead of autoclave for manufacturing of load bearing structures are considered. The interrelation of porosity of plastics, permeability, and some other parameters for the purpose of receiving PCM with minimal porosity and properties, approximate to avtoklave formation is investigated PСM.

 

Reference list
  1. Terebenin B.P. Tekhnologicheskie osobennosti izgotovleniya krupnogabaritnykh izdelij iz stekloplastika [Technological features of manufacturing large-sized products made of fiberglass] // Steklotekstolity i drugie konstruktsionnye plastiki. M.: Oborongiz, 1960. 168 s.
  2. Dushin M.I., Khrulkov A.V., Mukhametov R.R. Issledovanie tekhnologicheskikh parametrov avtoklavnogo formovaniya detalej iz polimernykh kompozitsionnykh materialov [Research of technological parameters of autoclave molding of parts from polymer composite materials] // Klei. Germetiki. Tekhnologii. 2013. №8. S. 12–15.
  3. Dushin M.I., Chursova L.V., Khrulkov A.V., Kogan D.I. Osobennosti izgotovleniya PKM metodom vakuumnoj infuzii [Peculiarities of manufacturing PCM by the method of vacuum infusion] // Voprosy materialovedeniya. 2013. №3. S. 33–40.
  4. Dushin M.I., Muhametov R.R., Platonov A.A., Merkulova Yu.I. Issledovanie filtracionnyh harakteristik armiruyushhih napolnitelej i svyazuyushhih pri razrabotke tehnologii bezavtoklavnogo formovaniya polimernyh kompozicionnyh materialov [Study of filtration characteristics of reinforcing fillers and binders in the development of non-out-autoclave technology for polymer composite material] // Aviacionnye materialy i tehnologii. 2013. №2. S. 22–25.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kablov E.N. Materialy novogo pokoleniya [Materials of a new generation] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  7. Kablov E.N. Kompozity: segodnya i zavtra [Composites: Today and Tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  8. Grunenfelder L.K., Nutt S.R. Void formation in composite prepregs – effect of dissolved moisture // Composites Science Technologies. 2010. Vol. 70. P. 2304–2309.
  9. Ridgard C. Out of Autoclave Composite Technology for Aerospace, Defense and Space Structures // International SAMPE Symposium. 2009. P. 134–136.
  10. Thomas S., Bongiovanni C., Nutt S.R. In Situ Estimation of through-Thickness Resin Flow using Ultrasound // Composites Science and Technology. 2008. Vol. 68. No. 15–16. P. 3093–3098.
  11. Donetskiy K.I., Dushin M.I., Mischun M.I., Sevastianov D.V. Nekotorye osobennosti primeneniya semipregov dlya vakuumnogo formovaniya PKM (obzor) [Some features of semi-pregs application for vacuum formation of polymeric composite materials (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №12 (60). St. 08. Available: http://www.viam-works.ru (accessed: July 31, 2018). DOI: 10.18577/2307-6046-2017-0-12-8-8.
  12. Thorfinnson B., Biermann T.F. Production of Void Free Composite Parts without Debulking // International SAMPE Symposium. 1986. P. 71–74.
  13. Thorfinnson B., Biermann T.F. Degree of Impregnation of Prepregs: Effects on Porosity // International SAMPE Symposium. 1987. P. 28–32.
  14. Boyd J. Tutorial: Vacuum Bag Only Composite Part Manufacturing // International SAMPE Symposium. 2003. P. 7–10.
  15. Arafath A.R.A., Fernlund G., Poursartip A. Gas Transport in Prepregs: Model and Permeability Experiments // ICCM-17. 2009. P. 43–47.
  16. Dushin M.I., Doneckij K.I., Karavaev R.Yu. Ustanovlenie prichin obrazovaniya poristosti pri izgotovlenii PKM [Identification of the reasons of porosity formation when manufacturing composites] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №6 (42). St. 08. Available at: http://www.viam-works.ru (accessed: July 31, 2018). DOI: 10.18577/2307-6046-2016-0-6-8-8.
  17. Campbell F.C., Mallow A.R., Browning C.E. Porosity in Carbon Fiber Composites an Overview of Causes // Journal of Advanced Materials. 1995. Vol. 26. No. 4. P. 18–33.
  18. Kardos J.L. Void Growth and Dissolution // Processing of Composites. 2000. Vol. 1. P. 182–206.
  19. Zingraff L. Void Formation and Transport during Liquid Moulding and Forming of Reactive Thermoplastic Composites: PhD Thesis. École polytechnique fédérale de Lausanne (EPFL), 2004. 231 p.
  20. Lykov A.V. Yavleniya perenosa v kapillyarno-poristykh telakh [Transport phenomena in capillary-porous bodies]. M.: Gos. izd-vo tekhniko-teoretich. liter., 1954. 472 s.
  21. Kavkazov Yu.L. Vzaimodejstvie kozhi s vlagoj [Interaction of the skin with moisture]. M.: Gizlegprom, 1952. 320 s.
  22. Rudobashta S.P. Massoperenos v sistemakh s tverdoj fazoj [Mass transfer in systems with a solid phase]. M.: Khimiya, 1980. 248 s.
  23. Putnam J.W., Seferis J.C. Prepreg Gas Permeation as a Function of Fiber Orientation and Aging Time // Journal of Advanced Materials. 1995. Vol. 26. No. 3. P. 35–41.
  24. Gaskell D.R. An Introduction to Transport Phenomena in Materials Engineering. Macmillan Publishing Company, 1992. 143 p.
  25. Civan F. Porous Media Transport Phenomena. John Wiley & Sons, 2011. 448 p.
  26. Gas Transport in Porous Media / Eds. by S.W. Webb, C.K. Ho. Springer, 2006. 303 p.
  27. Louis B., Hsiao K., Fernlund G. Gas Permeability Measurements of Out of Autoclave Prepreg MTM45-1/CF2426A // International SAMPE Symposium. Seatle, 2010. P. 342–354.
  28. Xin C., Li M., Gu Y. et al. Measurement and Analysis on in-Plane and through-Thickness Air Permeation of Fiber/Resin Prepreg // Journal of Reinforced Plastics and Composites. 2011. Vol. 30. No. 17. P. 1467–1479.
  29. Tavares S.S., Michaud V., Mеnson J.A.E. Assessment of semi-impregnated fabrics in honeycomb sandwich structures // Composites Applied Science Manufactory. 2010. Vol. 41. P. 8–15.
  30. Ahn K.J., Seferis J.C., Price J.O., Berg A.J. Permeation Measurements Through Prepreg Laminates // Sampe Journal. 1991. Vol. 27. No. 6. P. 19–25.
  31. Centea T., Hubert P. Measuring the impregnation of an out-of-autoclave prepreg by micro-CT // Composites Science and Technology. 2011. Vol. 71. P. 593–599.
  32. Gutowski T.G., Cai Z., Bauer S. et al. Consolidation experiments for laminate composites // Journal of Composites Materials. 1987. Vol. 21 (7). P. 650–669.
  33. Cender T.A., Simacek P., Advani S.G. Resin film impregnation in fabric prepregs with dual length scale permeability // Composites: Part A. 2013. Vol. 53. P. 118–128.
  34. Simacek P., Neacsu V., Advani S.G. A phenomenological model for fiber tow saturation of dual scale fabrics in liquid composite molding // Polymer Composites. 2010. Vol. 31. P. 1881–1889.
  35. Hwang W.R., Advani S.G. Numerical simulations of Stokes–Brinkman equations for permeability prediction of dual scale fibrous porous media // Physical Fluids. 2010. Vol. 22. P. 113–115.
  36. Zhou F., Alms J., Advani S. A closed form solution for flow in dual scale fibrous porous media under constant injection pressure conditions // Composition Science Technologies. 2008. Vol. 68. P. 699–708.
  37. Zhou F., Kuentzer N., Simacek P. et al. Analytic characterization of the permeability of dual-scale fibrous porous media // Composition Science Technologies. 2006. Vol. 66. P. 2795–2803.
  38. Umemoto Y., Gouke M., Mashima Y. Out of autoclave material «semi-preg». Technical development of resin transfer molding // Proceedings of the 18th International Conference on Composite materials (Korea, August 21–26, 2011). 2011. Paper No. TH05-2.
  39. Out-of-autoclave prepregs: Hype or revolution? // СompositesWorld. Available at: http://www.compositesworld.com/articles/out-of-autoclave-prepregs-hype-or-revolution (accessed: July 31, 2018).