Investigations of the influence of quality of the consumed electrode on the process of electroslag remelting under pressure of high-nitrogen steels

Krylov S.А., Makarov А.А., Tonysheva О.А., Mosolov A.N.
Krylov S.А., Makarov А.А., Tonysheva О.А., Mosolov A.N. Investigations of the influence of quality of the consumed electrode on the process of electroslag remelting under pressure of high-nitrogen steels // Proceedings of VIAM. 2018. No. 9. DOI: 10.18577/2307-6046-2018-0-9-3-11. URL: https://www.viam-works.ru/en/journal/2018/9/1
Keywords
metallurgy under pressure, electroslag remelting, induction melting, high-nitrogen steel, gas pores.
Abstract

A new breakthrough in the creation of new materials and technologies for producing high-nitrogen steels (HNS) in Russia was made after the installation of an electroslag remelting unit under pressure (ESRP) and the development of FGUP “VIAM” of ESRP technologies. Due to the high demands placed on semi-finished products of HNS, high requirements are also imposed on ingots of ESRP and on consumable HNS electrodes. Investigations of metal used as consumable electrodes of the ingot are conducted, and requirements for its smelting are formulated.

Reference list
  1. Tonysheva O.A., Voznesenskaya I.M., Eliseev E.A., Shalkevich A.B. Novaya vysokoprochnaya ekonomnolegirovannaya azotsoderzhashchaya stal povyshennoj nadezhnosti [The new high-strength containing steel of increased reliability economically alloyed nitrogen] // Aviacionnye materialy i tehnologii. 2012. №S. S. 84–88.
  2. Rashev TS. Vysokoazotistye stali. Metallurgiya pod davleniem [High-nitrogen steels. Metallurgy under pressure]. Sofiya: Prof. Marin Drinov, 1995. 272 s.
  3. Energietechnik Еssen. Сronidur30. Available at: http://www.energietechnik-essen.de (accrssed: August 21, 2018).
  4. Berns H. High Interstitial Stainless Austenitic Steels, Part I: Constitution, Heat Treatment, Properties, Applications // Proceedings of 10th International Conference on High Nitrogen Steels. 2009. P. 129–139.
  5. Stein G., Hucklenbroich I., Wagner M. P200 – a new austenitic nitrogen steel for power generating equipment// Material Science Forum. 1999. Vol. 318–320. Р. 167–174.
  6. Krylov S.A., Evgenov A.G., Shherbakov A.I., Makarov A.A. Novaya elektroshlakovaya pech pod davleniem DEShP-0,1: osvoenie i perspektivy razvitiya [New pressure electroslag remelting furnace PESR-0,1: development and prospects for improvement] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5. St. 04. Available at: http://www.viam-works.ru (accessed: May 03, 2018). DOI: 10.18577/2307-6046-2016-0-5-4-4.
  7. Krylov S.A., Shcherbakov A.I., Makarov A.A., Tonysheva O.A. Snizhenie soderzhaniya nemetallicheskikh vklyuchenij v korrozionnostojkoj azotsoderzhashchej stali [Reduction of non-metallic inclusions in the nitrogen-containing corrosion-resistant steels] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №5 (53). St. 01. Available at: http://www.viam-works.ru (accessed: May 08, 2018). DOI: 10.18577/2307-6046-2017-0-5-1-1.
  8. Krylov S.A., Evgenov A.G., Makarov A.A., Tonysheva O.A. Slitok elektroshlakovogo pereplava pod davleniem [The ingot PESR] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №3 (51). St. 03. Available at: http://www.viam-works.ru (accessed: May 10, 2018). DOI: 10.18577/2307-6046-2017-0-3-3-3.
  9. Rigina L.G., Vasilev Ya.M., Dub V.S., Kolpishon E.Yu., Afanasev S.Yu. Legirovanie stali azotom [The alloying of steel with nitrogen] // Spetselektrometallurgiya. 2005. №2. S. 14–21.
  10. Lysenkova E.V. Povyshenie tochnosti raschetov rastvorimostej azota i nitrida titana v rasplavakh na osnove zheleza. Primenenie k stalyam, legirovannym azotom i titanom: dis. … kand. tekhn. nauk [Increase the accuracy of calculations of the solubilities of nitrogen and titanium nitride in iron-based melts. Application to steels doped with nitrogen and titanium: thesis, Cand. Sc. (Tech.)]. M., 2015. S. 19–20.
  11. Kablov E.N. Innovatsionnye razrabotki FGUP «VIAM» GNTS RF po realizatsii «Strategicheskikh napravlenij razvitiya materialov i tekhnologij ikh pererabotki na period do 2030 goda» // Aviatsionnye materialy i tekhnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Kablov E.N. Sovremennye materialy – osnova innovatsionnoj modernizatsii Rossii [Modern materials are the basis of Russia's innovative modernization] // Metally Evrazii. 2012. №3. S. 10–15.
  13. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Russia needs materials of a new generation] // Redkie zemli. 2014. №3. S. 8–13.
  14. Potak Ya.M. Vysokoprochnye stali. Ser.: Uspekhi sovremennogo metallovedeniya [High-strength steels. Ser.: Advances in modern metal science]. M.: Metallurgiya, 1972. S. 142.
  15. Shved F.I. Slitok vakuumnogo dugovogo pereplava [Ingot vacuum arc remelting]. Chelyabinsk: Izd-vo Tatyany Lure, 2009. S. 289–295.