Development the set of methods measurements of the chemical composition of nickel-based alloys

Letov A.F., Karachevtsev F.N., Zagvozdkina T.N.
Letov A.F., Karachevtsev F.N., Zagvozdkina T.N. Development the set of methods measurements of the chemical composition of nickel-based alloys // Proceedings of VIAM. 2018. No. 8. DOI: 10.18577/2307-6046-2018-0-8-89-97. URL: https://www.viam-works.ru/en/journal/2018/8/9
Keywords
measurement technique, nickel alloys, the metrological characteristics, mass-spectrometric analysis, optical-emission analysis, X-ray fluorescence analysis.
Abstract

Heat-resistant nickel alloys are materials used to manufacture a wide range of gas turbine engine parts. The level of refractory strength of the heat-resistant nickel alloys is determined by their chemical and phase composition, as well as by the manufacturing techniques used, which ensure the formation of a given material structure. An important factor in the industrial production of the heat-resistant nickel alloys and in the development of new-generation alloys is the ability to control the chemical composition of the cast bar stock and finished products from the heat-resistant nickel alloys by modern methods of spectral analysis. The development of a set of methods for measuring the mass fraction of elements in heat-resistant nickel alloys by mass spectrometry with inductively coupled plasma, optical emission and X-ray fluorescence analysis, makes it possible to control the content of alloying and microalloying elements and various impurities.

Reference list
  1. Karachevtsev F.N., Zagvozdkina T.N., Orlov G.V. Razrabotka i issledovanie metrologicheskih harakteristik ekspress-metodiki analiza zharoprochnyh nikelevyh splavov [Development and research of metrological characteristics of express-analysis of heat-resistant nickel alloys] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2015. №11. St. 09. Available at: http://viam-works.ru (accessed: June 15, 2018). DOI: 10.18577/2307-6046-2015-0-11-9-9.
  2. Zagvozdkina T.N., Karachevtsev F.N., Dvoretskov R.M., Mekhanik E.A. Primenenie optiko-fizicheskikh metodov izmerenij dlya issledovanij sostava novykh aviatsionnykh materialov [Application of optic physical methods of measurements for researches of structure of new aviation materials] // Metrologiya. 2015. №1. S. 60–68.
  3. Kablov E.N., Petrushin N.V., Parfenovich P.I. Konstruirovanie litejnykh zharoprochnykh nikelevykh splavov s polikristallicheskoj strukturoj [Designing of cast heat resisting nickel alloys with polycrystalline structure] // Metallovedenie i termicheskaya obrabotka metallov. 2018. №2 (752). S. 47–55.
  4. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennykh zharoprochnykh materialov i tekhnologij ikh proizvodstva dlya aviatsionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
  5. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  6. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  7. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlya perspektivnykh aviatsionnykh GTD [Cast heat resisting nickel alloys for perspective aviation GTE] // Tekhnologiya legkikh splavov. 2007. №2. S. 6–16.
  8. Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Monokristallicheskij zharoprochnyj nikelevyj splav novogo pokoleniya s nizkoj plotnostyu [Single-crystal nickel-based superalloy of a new generation with low-density] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
  9. Kablov E.N., Ospennikova O.G., Petrushin N.V. Novyj monokristallicheskij intermetallidnyj (na osnove γʹ-fazy) zharoprochnyj splav dlya lopatok GTD [New single crystal heat-resistant intermetallic γʹ-based alloy for GTE blades] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 34–40. DOI: 10.18577/2071-9140-2015-0-1-34-40.
  10. Ovsepyan S.V., Lomberg B.S., Grigoreva T.I., Bakradze M.M. Zharoprochnyj deformiruemyj svarivaemyj splav dlya detalej GTD s nizkim temperaturnym koeffitsientom linejnogo rasshireniya [Heat resisting deformable welded alloy for GTE details with low temperature coefficient of linear dilatation] // Metallurg. 2013. №7. C. 61–65.
  11. Yakimovich P.V., Alekseev A.V. Opredelenie galliya, germaniya, myshyaka i selena v zharoprochnyh nikelevyh splavah, mikrolegirovannyh RZM, metodom ISP-MS [Determination of gallium, germanium, arsenic and selenium contents in heat-resistant nickel alloys microalloyed by REM using ICP-MS] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 09. Available at: http://viam-works.ru (accessed: June 15, 2018). DOI: 10.18577/2307-6046-2015-0-3-9-9.
  12. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. Karachevtsev F.N., Alekseev A.V., Letov A.F., Dvoretskov R.M. Plazmennye metody analiza elementnogo khimicheskogo sostava nikelevykh splavov [Plasma methods of nickel alloys elemental chemical composition analysis] // Aviacionnye materialy i tehnologii. 2017. №S. S. 483–497. DOI: 10.18577/2071-9140-2017-0-S-483-497.
  14. Striganov A.R., Odintsova G.A. Tablitsy spektralnykh linij atomov i ionov: spravochnik [Tables of spectral lines of atoms and ions: directory]. M.: Energoizdat, 1982. 600 c.
  15. Vajnshtejn L.A., Sobelman I.I., Yukov E.A. Vozbuzhdenie atomov i ushirenie spektralnykh linij [Excitation of atoms and broadening of spectral lines]. M.: Nauka, 1979. 320 s.