Abradability and erosion resistance of seals in turbine engine air-gas channel

Farafonov D.P., Migunov V.P., Saraev A.A., Leschev N.E.
Farafonov D.P., Migunov V.P., Saraev A.A., Leschev N.E. Abradability and erosion resistance of seals in turbine engine air-gas channel // Proceedings of VIAM. 2018. No. 8. DOI: 10.18577/2307-6046-2018-0-8-70-80. URL: https://www.viam-works.ru/en/journal/2018/8/7
Keywords
abradability, erosion resistance, gas-turbine engine, sealing material, wear, wear debris.
Abstract

The main properties of abraded sealing materials defining efficiency of their application in flowing part of gas turbine engines, are abradability which can be provided by relative wear of sealing material and material of rotor details, and its erosion resistance, which has to be rather high to guarantee engine operation during the set resource. Abradability and erosion resistance are defined by strength properties of materials and are inversely proportional sizes therefore creation of effective abraded sealing materials is one of the most complex and actual challenges of aviation materials science. Results of researches of abradability and erosion resistance of modern aircraft engines of sealing materials applied in designs are given in article, and also the pilot materials developed by VIAM Federal State Unitary Enterprise

Reference list
  1. Wilson S. Overview of Sulzer Metco compressor and turbine abradable technology // 8th International Charles Parsons Turbine Conference. 2011. University of Portsmouth. Available at: http://www.iom3.org/sites/default/files/iom3-corp/wed%200940%20s%20Wilson.pdf (accessed: June 14, 2018).
  2. Smarsly W., Zheng N., Buchheim C.S. et al. Advanced High Temperature Turbine Seals Materials and Designs // Material Science Forum. 2005. Vol. 492–493 P. 21–26.
  3. Farafonov D.P., Migunov V.P., Degovets M.L., Aleshina R.Sh. Perspektivy razvitiya i primeneniya istiraemyh uplotnitelnyh materialov iz metallicheskih volokon v protochnom trakte turbiny aviacionnyh dvigatelej [Development prospects of abradable sealing materials made from metal fibers for application in flow duct of aircraft engine turbine] //Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 51–59. DOI: 10.18577/2071-9140-2015-0-3-51-59.
  4. Farafonov D.P., Degovets M.L., Aleshina R.SH. Metallicheskie volokna iz zharostojkikh splavov, legirovannykh metallami platinovoj gruppy [The metal fibers of heat-resistant alloys alloyed by platinum group metals] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 44–52. DOI: 10.18577/2071-9140-2016-0-1-44-52.
  5. Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Vysokotemperaturnye intermetallidnye splavy dlya detaley GTD [The high-temperature intermetallic alloys for parts of gas-turbine engines] // Aviacionnye materialy i tehnologii. 2013. №3. S. 26–31.
  6. Simms N.J., Norton J.F., McColvin G. Performance of candidate gas turbine abradeable seal materials in high temperature combustion atmospheres // Materials and Corrosion. 2005. Vol. 56. P. 765–777.
  7. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  9. Migunov V.P., Farafonov D.P. Issledovanie osnovnyh ekspluatacionnyh svojstv novogo klassa uplotnitelnyh materialov dlya protochnogo trakta GTD [Research of the main operational properties of new class of sealing materials for flowing path of GTE] // Aviacionnye materialy i tehnologii. 2011. №3. S. 15–20.
  10. Serov M.M., Borisov B.V. Poluchenie metallicheskikh volokon i poristykh materialov iz nikh metodom ekstraktsii visyashchej kapli rasplava [Receiving metal fibers and porous materials from them method of extraction of hanging drop melt] // Tekhnologiya legkikh splavov. 2007. №3. C. 62–65.
  11. Kablov E.N., Solntsev S.S., Rozenenkova V.A., Mironova N.A. Sovremennye polifunktsionalnye vysokotemperaturnye pokrytiya dlya nikelevykh splavov, uplotnitelnykh metallicheskikh voloknistykh materialov i berillievykh splavov [Modern multifunctional high temperature coatings for nickel alloys, sealing metal fibrous materials and beryllium alloys] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2013. №1. St. 05. Available at: http://www.materialsnews.ru (accessed: June 18, 2018).
  12. Solntsev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Vysokotemperaturnye tonkoplenochnye pokrytiya dlya uplotnitelnyh materialov iz metallicheskih volokon [High-temperature thin-film coverings for sealing materials from metal fibers] // Aviacionnye materialy i tehnologii. 2012. №1. S. 30–36.
  13. Afanasev-Khodykin A.N., Rylnikov V.S., Farafonov D.P. Tekhnologiya pajki poristo-voloknistogo materiala iz splava tipa «fekhral» dlya uplotneniya protochnoj chasti GTD [Technology soldering porous fibrous material of the alloy of the «fehral» to seal the flow part of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №1. St. 02. Available at: http://www.viam-works.ru (accessed: June 15, 2018). DOI: 10.18577/2307-6046-2014-0-1-2-2.
  14. Fei W., Kuiry S.C., Seal S. Inhibition of Metastable Alumina Formation on Fe–Cr–Al–Y Alloy Fibers at High Temperature Using Titania Coating // Oxidation of Metals. 2004. Vol. 62. Issue 1–2. P. 29–44.
  15. Sporer D., Refke A., Dratwinski M. et al. Increased Efficiency of Gas Turbines // Sulzer Technical Review. Available at: http://www.sulzer.com/-/media/files/about-us/sulzer-technical-review/str-archive/2008/_2_4_sporer_e.ashx (accessed: June 25, 2018).