Biomorphic composites: a promising class of materials (review)

Part 2. Mechanical properties, application
Sevastyanov D.V., Doriomedov M.S., Daskovskiy M.I., Skripachyov S.Yu.
Sevastyanov D.V., Doriomedov M.S., Daskovskiy M.I., Skripachyov S.Yu. Biomorphic composites: a promising class of materials (review). Part 2. Mechanical properties, application // Proceedings of VIAM. 2018. No. 8. DOI: 10.18577/2307-6046-2018-0-8-61-69. URL: https://www.viam-works.ru/en/journal/2018/8/6
Keywords
biomorphic composites, mechanical properties, application area of biomorphic composites, silicon carbide.
Abstract

Analysis of mechanical properties for biomorphic composites was performed. It was shown that properties in axial direction exceeded the ones in radial and tangential directions. This fact can be explained by the preservation of microstructure on going from a piece of wood to a biomorphic composite. Prospects for application of biomorphic composites in various industrial fields (as catalyst support, high-temperature gas filtration materials, armor materials as well as in medicine, radio electronics, and power engineering) were discussed.

Reference list
  1. Greil P., Lifka T., Kaindl A. Biomorphic cellular silicon carbide ceramics from wood: II. Mechanical properties // Journal of the European Ceramic Society. 1998. Vol. 18. No. 14. P. 1975–1983
  2. Ramirez-Rico J., Martinez-Fernandez J., Singh M. Biomorphic ceramics from wood-derived precursors // International Materials Reviews. 2017. Vol. 62. No. 8. P. 465–485.
  3. Qiao G., Ma R., Cai N., Zhang C., Jin. Z. Mechanical properties and microstructure of Si/SiC materials derived from native wood. // Materials Science and Engineering A. 2002. Vol. 323. No. 1–2. P. 301–305.
  4. Presas M., Pastor J.Y., Llorca J. et al. Mechanical behavior of biomorphic Si/SiC porous composites. // Scripta Materialia. 2005. Vol. 53. No. 10. P. 1175–1180.
  5. Kaul V.S., Faber K.T., Sepulveda R. et al. Precursor selection and its role in the mechanical properties of porous SiC derived from wood // Materials Science and Engineering A. 2006. Vol. 428. No. 1–2. P. 225–232.
  6. Singh M., Martinez-Fernandez J., De Arellano-Lopez A.R. Environmentally conscious ceramics (ecoceramics) from natural wood precursors // Current Opinion in Solid State and Materials Science. 2003. Vol. 7. P. 247–254.
  7. Presas M., Pastor J.Y., Llorca J. et al. Microstructure and fracture properties of biomorphic SiC // International Journal of Refractory Metals & Hard Materials. 2006. Vol. 24. No. 1–2. P. 49–54.
  8. Singh M., Salem J.A. Mechanical properties and microstructure of biomorphic silicon carbide ceramics fabricated from wood precursors // Journal of the European Ceramic Society. 2002. Vol. 22. No. 14–15. P. 2709–2717.
  9. Sieber H., Hoffmann C., Kaindl A., Greil P. Biomorphic cellular ceramics // Advanced Engineering Materials. 2000. Vol. 2. No. 3. P. 105–109.
  10. Park H.S., Jang J.J., Lee K.H. et al. Effects of microstructure on flexural strength of biomorphic C/SiC composites // International Journal of Fracture. 2008. Vol. 151. P. 233–245.
  11. Kardashev B.K., Nefagin A.S., Smirnov B.I. i dr. Uprugie i neuprugie svojstva biomorfnykh kompozitov SiC/Si i biomorfnykh SiC na osnove duba i evkalipta [Elastic and not elastic properties of biomorphic composites of SiC/Si and biomorphic SiC on the basis of oak and eucalyptus] // Fizika tverdogo tela, 2006. T. 48. №9. C. 1617–1621.
  12. Kardashev B.K., Orlova T.S., Smirnov B.I. i dr. Modul Yunga i vnutrennee trenie biomorfnogo kompozita SiC/Si na osnove biomatritsy dereva sapeli [The elasticity modulus and internal friction of biomorphic composite of SiC/Si on the basis of biomatrix of tree snuffled] // Fizika tverdogo tela. 2009. T. 51. №4. S. 709–712.
  13. Kardashev B.K., Orlova T.S., Smirnov B.I. i dr. Uprugost i neuprugost biomorfnykh ugleroda, karbida kremniya i kompozita SiC/Si, poluchennykh na osnove mikrodrevesnoj fibry MDF [Elasticity and not elasticity of biomorphic carbon, silicon carbide and composite of SiC/Si received on the basis of microwood fiber of MDF] // Fizika tverdogo tela. 2010. T. 52. №10. S. 1937–1942.
  14. Bautista M.A., Quispe Cancapa J., Martinez-Fernandez J. et al. Microstructural and mechanical evaluation of porous biomorphic silicon carbide for high temperature filtering applications // Journal of the European Ceramic Society. 2011. Vol. 31. No. 7. P. 1325–1332.
  15. Gordic M.V., Babic B.M., Static J.M. et al. Mechanical properties of biomorphic silicon carbide ceramics // Science of Sintering. 2011. Vol. 43. No. 2. P. 215–223.
  16. Yan Z., Liu J., Zhang J. et al. Biomorphic silicon/silicon carbide ceramics from birch powder // Ceramics International. 2011. Vol. 37. No. 3. P. 725–730.
  17. Lee D.J., Jang J.J., Park H.S. et al. Fabrication of biomorphic SiC composites using wood preforms with different structures // Ceramics International. 2012. Vol. 38. No. 4. P. 3089–3095.
  18. Wang Q., Sun W.-Z., Jin G.-Q. et al. Biomorphic SiC pellets as catalyst support for partial oxidation of methane to syngas // Applied Catalysis B: Environmental. 2008. Vol. 79. No. 4. P. 307–312.
  19. Church T.L., Fallani S., Liu J. et al. Novel biomorphic Ni/SiC catalysts that enhance cellulose conversion to hydrogen // Catalysis Today. 2012. Vol. 190. No. 1. P. 98–106.
  20. Arzac G.M., Rico-Ramirez J., Gutierrez-Pardo A. et al. Monolithic supports based on biomorphic SiC for the catalytic combustion of hydrogen // RSC Advances. 2016.Vol. 6. P. 66373–66384.
  21. Zampieri A., Sieber H., Selvam T. Biomorphic cellular SiSiC/Zeolite ceramic composites: from rattan palm to bioinspired structured monoliths for catalysis and sorption // Advanced Materials. 2005. Vol. 17. No. 3. P. 344–349.
  22. Zampieri A., Kullmann S., Selvam T. et al. Bioinspired rattan-derived SiSiC/Zeolite monoliths: preparation and characterization // Microporous and Mesoporous Materials. 2006. Vol. 90. No. 1–3. P. 162–174.
  23. Rambo C.R., Junkes J., Sieber H., Hotza D. Biomorphic ceramics as porous supports for zeolite coating // Advances in Science and Technology. 2006. Vol. 45. P. 819–828
  24. Wang Y.-Y., Jin G.-Q., Guo X.-Y. Growth of ZSM-5 coating on biomorphic porous silicon carbide derived from durra // Microporous and Mesoporous Materials. 2009. Vol. 118. No. 1–3. P. 302–306.
  25. Gomez-Martin A., Orihuela M.P., Becerra J.A. et al. Permeability and mechanical integrity of porous biomorphic SiC ceramics for application as hot-gas filters // Materials and Design. 2016. Vol. 107. No. 5. P. 450–460.
  26. Bautista M.A., Quispe Cancapa J., Martinez-Fernandez J. et al. Microstructural and mechanical evaluation of porous biomorphic silicon carbide for high temperature filtering applications // Journal of the European Ceramic Society. 2011. Vol. 31. No. 7. P. 1325–1332.
  27. Alonso-Farinas B., Lupion M., Rodriguez-Galan M., Martinez-Fernandez J. New candle prototype for hot gas filtration industrial applications // Fuel. 2013. Vol. 114. P. 120–127.
  28. Gonzalez P., Borrajo J.P., Serra J. et al. A new generation of bio-derived ceramic materials for medical applications // Journal of Biomedical Materials Research Part A. 2009. Vol. 88A. No. 3. P. 807–813.
  29. Gonzalez P., Borrajo J.P., Serra J. et al. Extensive studies on biomorphic SiC ceramics properties for 9medical applications // Key Engineering Materials. 2004. Vol. 254–256. P. 1029–1032.
  30. Borrajo J.P., Serra J., Liste S. et al. Pulsed laser deposition of hydroxylapatite thin films on biomorphic silicon carbide ceramics // Applied Surface Science. 2005. Vol. 248. No. 1–4. P. 355–359.
  31. Will J., Hoppe A., Muller F.A. et al. Bioactivation of biomorphous silicon carbide bone implants // Acta Biomaterialia. 2010. Vol. 6. No. 12. P. 4488–4494.
  32. Mahmoodi M., Ghazanfari L. Fundamentals of biomedical applications of biomorphic SiC // Properties and Applications of Silicon Carbide. 2011. P. 297–344.
  33. Heidenreich B., Krenkel W., Lexow B. Development of CMC-materials for lightweight armor // Ceramic Engineering and Science Proceedings. 2003. Vol. 24. P. 375–381.
  34. Heidenreich B., Crippa M., Voggenreiter H. Development of biomorphic SiSiC- and C/SiSiC-materials for lightweight armor // Advances in Ceramics Armor VI. 2010. Vol. 31. Issue 5. P. 207–220.
  35. Heidenreich B., Gahr M., Medvedovski E. Biomorphic reaction bonded silicon carbide ceramics for armor applications // Ceramic Transactions. 2006. Vol. 178. P. 45–53.
  36. Zaenchkovskij P.V., Makarov O.Yu. Perspektivy primeneniya keramicheskikh materialov v radioelektronnoj promyshlennosti [Perspectives of application of ceramic materials in the radio-electronic industry] // Vestnik VGTU. 2009. T. 5. №7. S. 47–50.
  37. Ershov A.E. Poluchenie prostranstvenno-uporyadochennykh biomorfnykh kompozitov, ikh svojstva i primenenie: avtoref. dis. … kand. tekhn. nauk [Receiving the space arranged biomorphic composites, their properties and application: thesis abstract, Cand. Sc. (Tech.)]. Chernogolovka, 2016. 22 s.
  38. Heidenreich B., Schmidt J., Denis S. et al. CMC materials and biomorphic SiSiC for energy applications // Ceramic Transactions. 2010. Vol. 210. P. 115–123.
  39. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  40. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  41. Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 05. Available at: http://www.viam-works.ru (accessed: July 31, 2018).
  42. Ospennikova O.G., Kablov E.N., Shunkin V.N. Razrabotka i issledovanie plastifikatora dlya modelnykh kompozitsij na osnove prirodnykh voskov [Development and plasticizer research for model compositions on the basis of natural waxes] // Aviacionnye materialy i tehnologii. 2002. №3. S. 68–70.
  43. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. Vysokotemperaturnye metallomatrichnye kompozicionnye materialy, armirovannye chasticami i voloknami tugoplavkih soedinenij [High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds] // Aviacionnye materialy i tehnologii. 2017. №S. S. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  44. Kablov D.E., Simonov V.N., Alekseeva M.S. Issledovanie stroeniya filtra i osobennostej filtracii primesej poristoj keramikoj iz oksida alyuminiya Al2O3 [Research of structure of the filter and features of impurity filtering by porous ceramics from Al2O3 aluminum oxide] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 47–53. DOI: 10.18577/2071-9140-2016-0-4-47-53.