Biomorphic composites: a promising class of materials (review)

Part 1. History of creation, methods of the production
Sevastyanov D.V., Daskovskiy M.I., Doriomedov M.S., Skripachyov S.Yu.
Sevastyanov D.V., Daskovskiy M.I., Doriomedov M.S., Skripachyov S.Yu. Biomorphic composites: a promising class of materials (review). Part 1. History of creation, methods of the production // Proceedings of VIAM. 2018. No. 8. DOI: 10.18577/2307-6046-2018-0-8-47-60. URL: https://www.viam-works.ru/en/journal/2018/8/5
Keywords
biomorphic composites, mechanical properties, application area of biomorphic composites, silicon carbide.
Abstract

Overview and history for biomorphic composites (a wood-based promising class of mate-rials) were presented. Methods for the preparation of such composites (liquid silicon infiltration, gaseous Si or SiO infiltration, SiO2 precursor infiltration with subsequent carbothermal reduction) were introduced. In all cases wood pyrolysis with strict control of operating tempe-rature ensuring preparation of crack-free monoliths is used as the initial stage of the process.

Reference list
  1. Ershov A.E. Poluchenie prostranstvenno-uporyadochennykh biomorfnykh kompozitov, ikh svojstva i primenenie: avtoref. dis. … kand. tekhn. nauk [Receiving the space arranged biomorphic composites, their properties and application: thesis abstract, Cand. Sc. (Tech.)]. Chernogolovka, 2016. 22 s.
  2. Singh M., Martinez-Fernandez J., De Arellano-Lopez A.R. Environmentally conscious ceramics (ecoceramics) from natural wood precursors // Current Opinion in Solid State and Materials Science. 2003. Vol. 7. P. 247–254.
  3. De Arellano-Lopez A.R., Martinez-Fernandez J., Gonzalez P. et al. Biomorphic SiC: A new engineering ceramic material // International Journal of Applied Ceramic Technology. 2004. Vol. 1. No. 1. P. 56–67.
  4. Ugolev B.N. Drevesinovedenie i lesnoe tovarovedenie: ucheb. [Wood science and forest merchendizing: textbook]. M.: MGUL, 2007. 351 s.
  5. Ramirez-Rico J., Martinez-Fernandez J., Singh M. Biomorphic ceramics from wood-derived precursors // International Materials Reviews. 2017. Vol. 62. No. 8. P. 465–485.
  6. Ota T., Takahashi M., Hibi T. et al. Biomimetic process for producing SiC «wood» // Journal of American Ceramic Society. 1995. Vol. 78. No. 12. P. 3409–3411.
  7. Byrne C.E., Nagle D.C. Carbonization of wood for advanced materials applications // Carbon. 1997. Vol. 35. No. 2. P. 259–266.
  8. Byrne C.E., Nagle D.C. Carbonized wood monoliths – characterization // Carbon. 1997. Vol. 35. No. 2. P. 267–273.
  9. Byrne C.E., Nagle D.C. Cellulose derived composites – a new method for materials processing // Materials Research Innovations. 1997. Vol. 1. No. 3. P. 137–144.
  10. Greil P., Lifka T., Kaindl A. Biomorphic cellular silicon carbide ceramics from wood: I. Processing and microstructure // Journal of the European Ceramic Society. 1998. Vol. 18. No. 14. P. 1961–1973.
  11. Greil P., Lifka T., Kaindl A. Biomorphic cellular silicon carbide ceramics from wood: II. Mechanical properties // Journal of the European Ceramic Society. 1998. Vol. 18. No. 14. P. 1975–1983.
  12. Shlejzman V.V., Peschanskaya N.N., Orlova T.S., Smirnov B.I. Mikroplastichnost biomorfnogo kompozita SiC/Al pri odnoosnom szhatii [Microplasticity of biomorphic composite of SiC/Al at uniaxial compression] // Fizika tverdogo tela. 2009. T. 51. №12. S. 2315–2319.
  13. Wilkes T.E., Harder B.J., Almer J.D., Faber K.T. Load partitioning in honeycomb-like silicon carbide aluminum alloy composites // Acta Materialia. 2009. Vol. 57. No. 20. P. 6234–6242.
  14. Popovska N., Almeida-Streitwieser D., Xu C. et al. Kinetic analysis of the processing of porous biomorphic titanium carbide ceramics by chemical vapor infiltration // Chemical Vapor Deposition. 2005. Vol. 11. No. 3. P. 153–158.
  15. Rambo C.R., Cao J., Rusina O., Sieber H. Manufacturing of biomorphic (Si, Ti, Zr)-carbide ceramics by sol-gel processing // Carbon. 2005. Vol. 43. No. 6. P. 1174–1183.
  16. Rambo C.R., Cao J., Sieber H. Biomorphic (Si, Ti, Zr)-carbide synthesized through sol-gel process. // Ceramic Transactions. 2005. Vol. 166. P. 49–55.
  17. Greil P., Vogli E., Fey T. et al. Effect of microstructure on the fracture behavior of biomorphous silicon carbide ceramics // Journal of the European Ceramic Society. 2002. Vol. 22. No. 14–15. P. 2697–2707.
  18. Munoz A., Martinez-Fernandez J., Singh M. High temperature compressive mechanical behavior of joined biomorphic silicon carbide ceramics // Journal of the European Ceramic Society. 2002. Vоl. 22. No. 14–15. P. 2727–2733.
  19. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  20. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  21. Daskovskij M.I., Doriomedov M.S., Skripachev S.Yu. Sistematizaciya bazisnyh faktorov, prepyatstvuyushhih vnedreniyu polimernyh kompozicionnyh materialov v Rossii (obzor) [Underlying factors preventing the introduction of polymer composite materials in Russia (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5 St. 06. Available at: http://www.viam-works.ru (accessed: July 31, 2018). DOI: 10.18577/2307-6046-2016-0-5-6-6.
  22. Sevastjanov D.V., Doriomedov M.S., Daskovskij M.I., Skripachev S.Ju. Samoarmirovannye po-limernye kompozity – klassifikacija, poluchenie, mehanicheskie svojstva i primenenie (obzor) [Single-polymer composites – classification, synthesis, mechanical properties and application (re-view)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4 (52). St. 12. Available at: http://www.viam-works.ru (accessed: July 31, 2018). DOI: 10.18577/2307-6046-2017-0-4-12-12.
  23. 23 Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 05. Available at: http://www.viam-works.ru (accessed: July 31, 2018).
  24. Ospennikova O.G., Kablov E.N., Shunkin V.N. Razrabotka i issledovanie plastifikatora dlya modelnykh kompozitsij na osnove prirodnykh voskov [Development and plasticizer research for model compositions on the basis of natural waxes] // Aviacionnye materialy i tehnologii. 2002. №3. S. 68–70.