Stickiness and possibility of using prepregs for automated technologies (review)

Timoshkov P.N., Usacheva M.N., Khrulkov A.V.
Timoshkov P.N., Usacheva M.N., Khrulkov A.V. Stickiness and possibility of using prepregs for automated technologies (review) // Proceedings of VIAM. 2018. No. 8. DOI: 10.18577/2307-6046-2018-0-8-38-46. URL: https://www.viam-works.ru/en/journal/2018/8/4
Keywords
polymeric composite materials, stickiness, automated calculation, prepreg, method of stickiness determination, composite structures.
Abstract

In this review, the stickiness property of prepregs is considered, which affects the technological parameters in the process of laying out the workpiece parts from polymer composite materials. Various methods for determining stickiness, advantages and disadvantages of these methods are considered. It is shown that stickiness of prepregs depends on the temperature and storage conditions of prepregs. Dependence of the stickiness of prepregs on the temperature makes it possible to ensure easy separation of the prepreg from the substrate and to pass through the belt tape at a reduced temperature without adhering to the rollers, and then good adhesion to the tooling and to the prepreg layers due to heating to the temperature of high tackiness. The material VKU-25 developed in VIAM will allow to carry out the automated technology at manufacturing of preparations of details from polymeric composite materials.

Reference list
  1. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy VIAM 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Gusev Yu.A., Borshhev A.V., Khrulkov A.V. Osobennosti prepregov dlya avtomatizirovannoj vykladki metodami ATL i AFP [Features of prepregs intended for automated laying by ATL and AFP technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 06. Available at: http://www.viam-works.ru (accessed: June 20, 2018). DOI: 10.18577/2307-6046-2015-0-3-6-6.
  6. Timoshkov P.N. Oborudovanie i materialy dlya tekhnologii avtomatizirovannoj vykladki prepregov [Equipment and materials for the technology of automated calculations prepregs] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  7. Sloan J. ATL and AFP: defining the megatrends in composite aerostructures // High performance composites: Garden Business Media Inc., 2008. P. 20–25.
  8. Crossley R.J., Schubel P.J., Warrior N.A. The experimental characterization and Investigate on of prepreg tack // Proceedings of ICCM-18. Edinburgh, 2009. P. 1–11.
  9. Postnov V.I., Nikitin K.E., Petukhov V.I., Burkhan O.L., Orzaev V.G. Metod i ustrojstvo dlya opredeleniya lipkosti prepregov [Method and the device for determination of stickiness of prepregs] // Aviacionnye materialy i tehnologii. 2009. №3. S. 29–33.
  10. Dubois O., Le Cam J.-B., Beakou A. Experimental analysis of prepreg tack // Experimental Mechanics, Society for Experimental Mechanics. 2010. №50. P. 599–606.
  11. Ahn K.J., Seferis J.C., Pelton T., Wihelm M. Analysis and Characterization of Prepreg Tack // Polymer Composites. 1992. Vol. 13. No. 3. P. 197–206.
  12. Gillanders A.M., Kerr S., Martin T.J. Determination of prepreg tack // International Journal Adhesion and Adhesives. 1981. Vol. 1. No. 3. P. 125–134.
  13. Orlov E.V., Gusev Yu.A., Khrulkov A.V., Korotkov I.A. Sravnitelnyj analiz metodov opredeleniya lipkosti preprega [Comparative analysis of stickiness determination methods of prepreg] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 09. Available at: http://www.viam-works.ru (accessed: June 27, 2018). DOI: 10.18577/2307-6046-2016-0-7-9-9.
  14. ChemInstruments. Available at: http://www.cheminstruments.com/ (accessed: June 02, 2018).
  15. Postnov V.I., Burkhan O.L., Mantusova O.Yu. Metodika zamera lipkosti prepregov [Technique of measurement of stickiness of prepregs] // Sb. tez. dokl. Mezhdunar. nauch.-tekhnich. konf. «Sovremennye dostizheniya v oblasti kleev i germetikov. Materialy, syr'e, tekhnologii». N. Novgorod: Gladkova O.V., 2013. 227 s.
  16. Ustrojstvo dlya opredeleniya lipkosti prepregov i klejkikh lent: pat. 1716398 SSSR [The device for determination of stickiness of prepregs and sticky tapes: pat. 1716398 USSR]; zayavl.: 23.01.90; opubl.: 29.02.92.
  17. Pribor dlya izmereniya lipkosti prepregov: pat. 2549469 Ros. Federatsiya [The device for measurement of stickiness of prepregs: pat. 2549469 Rus. Federation]; zayavl.: 20.02.14; opubl.: 27.04.15.
  18. Strelnikov S.V., Petukhov V.I., Postnov V.I., Shvets N.I. Novye resheniya v tekhnologii izgotovleniya prepregov dlya panelej interera [New decisions in manufacturing techniques of prepregs for interior panels] // Izvestiya SamNTS RAN. 2011. T. 13. №4 (2). S. 498–507.
  19. Crossley R.J., Schubel P.J., Warrior N.A. The experimental determination of prepreg tack and dynamic stiffness // Composites: Part A. 2012. No. 43. P. 423–434.