Influence of the coating type on the damping ability

Gorlov D.S., Shchepilov A.V., Zaklyakova O.V., Gadzhikhalilova S.I.
Gorlov D.S., Shchepilov A.V., Zaklyakova O.V., Gadzhikhalilova S.I. Influence of the coating type on the damping ability // Proceedings of VIAM. 2018. No. 8. DOI: 10.18577/2307-6046-2018-0-8-120-129. URL: https://www.viam-works.ru/en/journal/2018/8/12
Keywords
ion-plasma coating, solid-lubricant coating, damping ability, blade root damping, q-factor, tribological characteristics, fretting, fretting-wear.
Abstract

In this research we investigated the possibility of reducing the vibration amplitude of the free end of a flat sample during vibration tests on the first bending form due to the application of different types of surfaces on the sample shank when it is fixed in the technological capture on the equipment for the vibrodynamic stand. The dependence of the q-factor of the oscillating system on different types of coatings, the thickness of which is ~30 microns, and the tribological characteristics of the coatings are

investigated. It is shown that the solid-lubricant coating VFP-5 increases damping, reducing the amplitude of the free end of the sample during vibration tests on the first bending form. The coating based on the aluminum alloy VSDP-28, does not significantly reduce the amplitude of the free end of the sample and the ion-plasma coatings of the TiN/CrN, Ti–TiN and SDP-2 systems reduce the damping properties of samples from the titanium alloy VT6.

Reference list
  1. Nozhnitskij Yu.A. Razrabotka klyuchevykh (kriticheskikh) tekhnologij dlya sozdaniya novogo pokoleniya gazoturbinnykh dvigatelej [Development of key (critical) technologies for creation of new generation of gas turbine engines] // Novye tekhnologicheskie protsessy i nadezhnost GTD: nauch.-tekhnich. sb. 2000. Vyp. 1: Bliski i blingi turbomashin. S. 5–34.
  2. Matveev V.V. Dempfirovanie kolebanij deformiruemykh tel [Vibration damping of deformable bodies]. Kiev: Naukova dumka, 1985. 264 s.
  3. Adamenko A.Ya. Dempfiruyushchaya sposobnost parnykh rabochikh lopatok gazoturbinnykh dvigatelej v usloviyakh vozdejstviya tsentrobezhnykh sil i temperatury: dis. … kand. tekhn. nauk [Damping capacity of pair working blades of gas turbine engines in the conditions of influence of centrifugal forces and temperature: thesis, Cand. Sc. (Tech.)]. Kiev, 1984. 238 s.
  4. Pisarenko G.S., Yakovlev A.P., Matveev V.V. Vibropogloshchayushchie svojstva konstruktsionnykh materialov: sprav. [Vibe absorbing properties of constructional materials: directory]. Kiev: Naukova dumka, 1971. 376 s.
  5. Pisarenko G.S., Kaminer A.A. Aerodinamicheskoe dempfirovanie kolebanij lopatok turbomashin [Aerodynamic vibration damping of blades of turbomachines]. Kiev: Naukova dumka, 1991. 302 s.
  6. Repetskij O.V. Kompyuternyj analiz dinamiki i prochnosti turbomashin [Computer analysis of dynamics and durability of turbomachines]. Irkutsk: Izd-vo IrGTU, 1999. 301 s.
  7. Matveev V.V., Yakovlev A.P., Balyuk A.D., Rzhavin L.N. Issledovanie dempfiruyushchikh svojstv zamkovogo soedineniya kompressornykh lopatok pri povyshennoj temperature [Research of damp properties of lock connection of compressor blades at elevated temperature] // Termoprochnost materialov i konstruktivnykh elementov. Kiev: Naukova dumka, 1967. Vyp. 4. S. 396–401.
  8. Ospennikova O.G., Muboyadzhyan S.A., Doronin O.N., Gorlov D.S. Issledovanie dempfiruyushchej sposobnosti ploskikh obraztsov iz titanovogo splava VT6 s pokrytiem [Research of damping capacity of flat samples from BT6 titanium alloy with covering] // Metally. 2018. №2. S. 11–20.
  9. Tokar I.G., Zinkovskij A.P., Matveev V.V. K voprosu o vozmozhnostyakh povysheniya dempfiruyushchej sposobnosti rabochikh lopatok sovremennykh gazoturbinnykh dvigatelej [To question of opportunities of increase of damping capacity of working blades of modern gas turbine engines] // Problemy prochnosti. 2003. №4. S. 58–68.
  10. Gorlov D.S., Shchepilov A.V. Issledovanie dempfiruyushchej sposobnosti kompozitsii «splav–pokrytie» posle ispytanij na zharostojkost i korrozionnuyu stojkost [Study of the damping capacity of the «alloy–coating» composition after tests on heat resistance and corrosion resistance] // Aviacionnye materialy i tehnologii. 2017. №4 (49). S. 62–69. DOI: 10.18577/2071-9140-2017-0-4-62-69.
  11. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Pomelov YA.A. Ionno-plazmennye zashchitnye pokrytiya dlya lopatok gazoturbinnykh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] // Konversiya v mashinostroenii. 1999. №2. S. 42–47.
  12. Muboyadzhyan S.A., Budinovskij S.A. Ionno-plazmennaya tehnologiya: perspektivnye protsessy, pokrytiya, oborudovanie [Ion-plasma technology: prospective processes, coatings, equipment] // Aviacionnye materialy i tehnologii. 2017. №S. S. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  13. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokonagruzhennykh detalej gazoturbinnykh dvigatelej [Materials for the high-loaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 13–19.
  14. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  15. Sibileva S.V., Karimova S.A. Obrabotka poverhnosti titanovyh splavov s celyu obespecheniya adgezionnyh svojstv [Surface treatment of titanium alloys to provide adhesion properties] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 25–35.
  16. Aleksandrov D.A., Muboyadzhyan S.A., Lutsenko A.N., Zhuravleva P.L. Uprochnenie poverkhnosti titanovykh splavov metodom ionnoj implantatsii i ionnogo modifitsirovaniya [Hardening of the surface of titanium alloys by ion implantation method and ionic modification] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 33–39. DOI: 10.18577/2071-9140-2018-0-2-33-39.