The phenomenon of formation and low-temperature diffusion transformation of metastable solid solutions with the release of dispersed particles of intragranular widmanstatten alpha phase in heat-resistant titanium alloys

Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Zavodov A.V.
Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Zavodov A.V. The phenomenon of formation and low-temperature diffusion transformation of metastable solid solutions with the release of dispersed particles of intragranular widmanstatten alpha phase in heat-resistant titanium alloys // Proceedings of VIAM. 2018. No. 8. DOI: 10.18577/2307-6046-2018-0-8-3-22. URL: https://www.viam-works.ru/en/journal/2018/8/1
Keywords
titanium alloys, thermal treatment, microstructure, electron microscopy, diffusion transformation, strength, Widmanstetten alpha.
Abstract

In the article discussed the phenomenon of formation and low-temperature diffusion transformation of metastable solid solutions with the release of dispersed particles of intragranular Widmanstatten α in Russian heat-resistant titanium alloys. It is shown that the intragranular Widmanstatten alpha phase can be formed at the final stage of cooling of the semi-finished product after heat treatment to a solid solution, as well as a result of aging. Examples of heterogeneous structures in various semi-finished products and details are given. The change of mechanical properties of heat-resistant titanium alloys in connection with structural dispersion hardening is considered.

Reference list
  1. Anoshkin N.F., Brun M.Ya., Shakhanova G.V. Trebovaniya k bimodalnoj strukture s optimalnym kompleksom mekhanicheskikh svojstv i rezhimy ee polucheniya [Requirements for bimodal structure with optimal complex of mechanical properties and modes of its production] // Titan. 1998. №1 (10). S. 35–41.
  2. Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Zavodov A.V. Vliyanie uslovij okhlazhdeniya krupnykh promyshlennykh pokovok iz zharoprochnogo titanovogo splava VT41 na fazovyj sostav i mekhanicheskie svojstva [Influence of cooling conditions of large industrial forgings made of heat-resistant titanium alloy VT41 on the phase composition and mechanical properties] // Tsvetnye metally. 2018. №2. S. 76–82. DOI: 10.17580/tsm.2018.02.10.
  3. Pavlova T.V., Kashapov O.S., Kondrateva A.R., Kalashnikov V.S. Vozmozhnosti po rasshireniyu oblasti primeneniya splava VT8-1 dlya diskov i rabochih koles kompressora [Opportunities to expand the VT8-1 alloy application for disks and compressor rotor wheels] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №3 (39). St. 05. Available at: http://www.viam-works.ru (accessed: July 31, 2017). DOI: 10.18577/2307-6046-2016-0-3-5-5.
  4. Sauer C., Lutjering G. Influence of layers at grain boundaries on mechanical properties of Ti-alloys // Materials Science and Engineering A. 2001. Vol. 319–321. P. 393–397.
  5. Es-Souni M. Creep behaviour and creep microstructures of a high-temperature titanium alloy Ti–5.8Al–4.0Sn–3.5Zr–0.7Nb–0.35Si–0.06C (Timetal 834). Part I. Primary and steady-state creep // Materials Characterization. 2001. Vol. 46. P. 365–379.
  6. Davies P., Pederson R., Coleman M., Birosca S. The hierarchy of microstructure parameters affecting the tensile ductility in centrifugally cast and forged Ti-834 alloy during high temperature exposure in air // Acta Materialia. 2016. Vol. 117. P. 51–67.
  7. Tong Li, Mansur Ahmed, Gang Sha et al. The influence of partitioning on the growth of intragranular a in near- Ti alloys // Journal of Alloys and Compounds. 2015. Vol. 643. P. 212–222.
  8. Evans D.J., Broderick T.F., Woodhouse J.B., Hoenigman J.R. On the synergism of α2 and sislicides in Ti–6Al–Sn–2Cr–2Zr–2Mo–Si // Titanium`95: Science and Technology. 1995. P. 2413–2420.
  9. Moiseyev V.N. Titanium alloys: Russian Aircraft and Aerospace applications. Taylor & Francis Group, 2006. 214 p.
  10. Monicault J.-M., Guedou J.-Y., Soniak F. Issues and progress in manufacturing of aero titanium parts. 2008. JM de Monicaut / ITA 24.09.2008. 38 pp.
  11. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  12. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. Kablov E.N. Razrabotki VIAM dlya gazoturbinnykh dvigatelej i ustanovok [The achievements of VIAM for gas turbine engines and installations] // Krylya Rodiny. 2010. №4. S. 31–33.
  14. Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Kondrateva A.R. Issledovanie vliyaniya rezhimov termicheskoj obrabotki na strukturu i svojstva opytnykh pokovok iz splava VT41 s melkozernistoj strukturoj [The influence of heat treatment conditions on structure and properties of pilot forgings from VT41 alloy with fine grained structure] // Aviacionnye materialy i tehnologii. 2017. №3 (48). S. 3–7. DOI: 10.18577/2071-9140-2017-0-3-3-7.
  15. Bhattacharyya D., Viswanathan G.B., Denkenberger R. et al. The role of crystallographic and geometrical relationships between a and b phases in an a/b titanium alloy // Acta Materialia. 2003. Vol. 51. P. 4679–4691. DOI: 10.1016/S1359-6454(03)00179-4.
  16. Suwas S., Singh A.K. Textural changes during β→α and α→β→α transformations in a Near-α Titanium Alloy // Metallurgical and materials transactions. 2004. Vol. 35A. P. 925–938. DOI: 10.1007/s11661-004-0017-8.
  17. Scotti L. First-principles study of solute diffusion mechanisms in alpha-Ti: thesis for the degree of PhD. School of Metallurgy and Materials. College of Engineering and Physical Sciences. University of Birmingham. March, 2016. 211 p.
  18. Seishi Ishiyama, Shuji Hanada, Osamu Izumi. Effect of Zr, Sn and Al Additions on Deformation Mode and Beta Phase Stability of Metastable Beta Ti Alloys // ISIJ International. 1991. Vol. 31. No. 8. P. 807–813. DOI: 10.2355/isijinternational.31.807.
  19. Jing R., Liang S.X., Liu C.Y. et al. Structure and mechanical properties of Ti–6Al–4V alloy after zirconium addition // Materials Science and Engineering: A. 2012. Vol. 552. P. 295–300. DOI: 10.1016/j.msea.2012.05.043.
  20. Binguo Fu, Hongwei Wang, Chunming Zou, Zunjie Wei. The influence of Zr content on microstructure and precipitation of silicide in as-cast near α titanium alloys // Materials Characterization. 2015. Vol. 99. P. 17–24. DOI: 10.1016/j.matchar.2014.09.015.
  21. Dolton W.T., Allison J.E., Lasecki J.V. The influence of thermal exposure on properties and microstructure of elevated temperature titanium alloys // Titanium’92 Science and technology. TMS, 1993. P. 295–302.
  22. Popov A.A., Popova M.A. Izotermicheskie diagrammy vydeleniya silitsidnykh i alyuminidnykh faz v zharoprochnykh titanovykh splavakh [Isothermal diagrams of silicide and aluminide phases in heat-resistant titanium alloys] // Metallovedenie i termicheskaya obrabotka metallov. 2016. №11. S. 23–28.
  23. Ahmed T., Rack H.J. Phase transformations during cooling in a+b titanium alloys // Materials Science and Engineering A. 1998. Vol. 243. P. 206–211. DOI: 10.1016/j.matchar.2016.05.020.
  24. Zhichao Sun, Xuanshuang Li, Huili Wu, He Yang. Morphology evolution and growth mechanism of the secondary Widmanstatten α phase in the TA15 Ti-alloy // Materials Characterization. 2016. Vol. 118. P. 167–174.
  25. Zhang X.D., Evans D.J., Baeslack W.A., Fraser H.L. Effect of long term aging on the microstructural stability and mechanical properties of Ti–6Al–2Cr–2Mo–2Sn–2Zr alloy // Materials Science and Engineering. 2003. A344. P. 300–311.
  26. Da Costa Teixeira J., Appolaire B., Aeby-Gautier E. et al. Transformation kinetics and microstructures of Ti17 titanium alloy during continuous cooling // Materials Science and Engineering A. 2007. Vol. 448. P. 135–145. DOI: 10.1016/j.msea.2006.10.024.