The graphite grades lubrication effect on tribotechnical properties of the metallic composite material

Bolsunovskaya T.A., Efimochkin I.Yu., Sevostyanov N.V., Burkovskaya N.P.
Bolsunovskaya T.A., Efimochkin I.Yu., Sevostyanov N.V., Burkovskaya N.P. The graphite grades lubrication effect on tribotechnical properties of the metallic composite material // Proceedings of VIAM. 2018. No. 7. DOI: 10.18577/2307-6046-2018-0-7-69-77. URL: https://www.viam-works.ru/en/journal/2018/7/8
Keywords
graphite, grain fineness, coarse-grained, finely-crystalline, synthetic, antifrictional, friction, wear, friction coefficient.
Abstract

The effect of different graphite grades in the copper-based metallic composite material on its tribotechnical properties is considered. Graphites were used as a solid lubricant with different crystal structure: synthetic, coarse-grained and fine-crystalline sintered, and finely dispersed colloidal. Tribotechnical tests data, according to the «finger–disk» testing scheme, have determined the influence of various sliding speeds and contact loading on the wear and friction coefficient depending on the graphite grades in composite material. It was shown that the tested graphite grades possess different tribotechnical properties associated with its manufacturing, dispersion and grain fineness.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Solomentseva A.V., Fadeeva V.M., Zhelezina G.F. Antifriktsionnye organoplastiki dlya tyazhelonagruzhennykh uzlov treniya skolzheniya aviatsionnykh konstruktsij [Antifriction organoplastics for heavy loaded sliding friction units of aircraft structures] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 30–34. DOI: 10.18577/2071-9140-2016-0-2-30-34.
  3. Farafonov D.P., Migunov V.P., Aleshina R.SH. Issledovanie tribotekhnicheskikh kharakteristik materialov, primenyaemykh dlya uprochneniya bandazhnykh polok rabochikh lopatok turbin GTD // Aviatsionnye materialy i tekhnologii. 2016. №S1 (43). S. 24–30. DOI: 10.18577/2071-9140-2016-0-S1-24-30.
  4. Ivanov E.V. Sozdanie iznosostojkih i antifrikcionnyh materialov i pokrytij dlja kosmicheskogo korablja «Buran» [Creation of wearproof and antifriction materials and coverings for the «Buran» spacecraft] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 142–151.
  5. Frolov K.V. Metody sovershenstvovaniya mashin i sovremennye problemy mashinovedeniya [Methods of improvement of machines and modern problems of mashinovedeniye]. M.: Mashinostroenie, 1984. 224 s.
  6. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsij, tekhnologicheskogo liderstva i natsionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  7. Kablov E.N. Sovremennye materialy – osnova innovatsionnoj modernizatsii Rossii [Modern materials – basis of innovative modernization of Russia] // Materialy Evrazii. 2012. №3. S. 10–15.
  8. Kablov E.N. Bez novykh materialov – net budushchego [Without new materials – there is no future] // Metallurg. 2013. №12. S. 4–8.
  9. Braun E.D., Bushe N.A., Buyakovskij I.A. Osnovy tribologii (trenie, iznos, smazka) [Tribology bases (friction, wear, lubricant)]. M.: Nauka i tekhnika, 2001. 778 s.
  10. Kragelskij I.V., Vinogradova I.E. Koeffitsienty treniya [Friction coefficients]. M.: Mashgiz, 1962. 219 s.
  11. Fedorchenko I.M., Pugina L.I. Kompozitsionnye spechennye antifriktsionnye materialy [The composite sintered antifriction materials]. Kiev: Naukova dumka, 1980. 404 s.
  12. Belogorskij V.D. Antifriktsionnyj grafit i ego primenenie v promyshlennosti [Antifriction graphite and its application in the industry]. M.: Znanie, 1974. 154 s.
  13. Ostrovskij V.S. Iskusstvennyj grafit [Artificial graphite]. M.: Metallurgiya, 1986. 272 s.
  14. Brejtuejt E.R. Tverdye smazochnye materialy i antifriktsionnye pokrytiya [Firm lubricants and anti friction coatings]. M.: Khimiya, 1967. 320 s.
  15. Fialkov A.S. Uglegrafitovye materialy [Carbon graphite materials]. M.: Energiya, 1979. 319 s.
  16. GOST 17022–81. Grafit. Tipy, marki i obshchie tekhnicheskie trebovaniya [State Standard 17022–81. Graphite. Types, brands and general technical requirements]. M.: Standartinform, 2010. 8 s.
  17. Kuksenova L.I., Lapteva V.G., Kolmakov A.G., Rybakova L.M. Metody ispytaniya na trenie i iznos [Test methods on friction and wear]. M.: Intermet Inzhiniring, 2001. 152 s.