Effect of hydrogen doping on structure and phase composition of sheet semi-products of VT23 titanium alloy

Panin P.V., Lukinа E.A., Alexeev E.B.
Panin P.V., Lukinа E.A., Alexeev E.B. Effect of hydrogen doping on structure and phase composition of sheet semi-products of VT23 titanium alloy // Proceedings of VIAM. 2018. No. 7. DOI: 10.18577/2307-6046-2018-0-7-49-57. URL: https://www.viam-works.ru/en/journal/2018/7/6
Keywords
titanium alloy VT23, hydrogen technology, hydrogen doping, hydrogenating annealing, phase composition, structure.
Abstract

The influence of extra hydrogen doping on phase and structural transformations in high-strength VT23 alloy has been studied. The volume ratios of α- and β-phases have been defined for room temperature state in dependence on hydrogen amount and hydrogenating annealing temperature in the range from 650 to 800°C. A quantitative estimation of β-phase content and α-particles dimensions in VT23 alloy have been evaluated with hydrogenation parameters being in focus. It has been shown that the alloy contains approximately 30% (vol.) of β-phase in initial condition. Doping with 0,1% (wt.) of hydrogen results in β-phase volume fraction increase from 50% after hydrogenation at 650°C to 80% after hydrogenation at 800°C. The dimensions of α-particles within the mentioned conditions change from 0,6–1,2 to 1,8–2,2 µm.

Reference list
  1. Kablov E.N. Iz chego sdelat budushchee? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  2. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsij, tekhnologicheskogo liderstva i natsionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  3. Kablov E.N. Materialy i khimicheskie tekhnologii dlya aviatsionnoj tekhniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Bratukhin A.G. Sovremennye aviatsionnye materialy: tekhnologicheskie i funktsionalnye osobennosti [Modern aviation materials: technological and functional features]. M.: Aviatekhinform, 2003. 440 s.
  5. Vozdvizhenskij V.M., Zhukov A.A., Postnova A.D., Vozdvizhenskaya M.V. Splavy tsvetnykh metallov dlya aviatsionnoj tekhniki [Non-ferrous alloys for aviation engineering]. Rybinsk: RGATA, 2002. 219 s.
  6. Bratukhin A.G., Kolachev B.A., Sadkov V.V. i dr. Tekhnologiya proizvodstva titanovykh samoletnykh konstruktsij [Production technology of titanic aircraft designs]. M.: Mashinostroenie, 1995. 448 s.
  7. Horev A.I. Fundamentalnye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravleniya ih razvitiya [Fundamental and applied works on structural titanium alloys and perspective directions of their development] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 04. Available at: http://www.viam-works.ru (accessed: June 13, 2018).
  8. Ilin A.A., Skvortsova S.V., Spektor V.S., Lukina E.A., Petrov L.M. Nizkotemperaturnoe vakuumnoe ionno-plazmennoe azotirovanie titanovykh splavov raznykh klassov [Low-temperature vacuum ion plasma nitriding of titanium alloys of different classes] // Tekhnologiya legkikh splavov. 2008. №3. S. 103–111.
  9. Lyasotskaya V.S. Termicheskaya obrabotka svarnykh soedinenij titanovykh splavov [Thermal processing of welded compounds of titanium alloys]. M.: Ekomet, 2003. 352 s.
  10. Kollerov M.Yu., Ilin A.A., Filatov A.A., Mamaev V.S. Uprochnyayushchaya termicheskaya obrabotka krupnogabaritnykh polufabrikatov i izdelij iz vysokoprochnykh titanovykh splavov [Strengthening thermal processing of large-size semi-finished products and products from high-strength titanium alloys] // Metallovedenie i termicheskaya obrabotka metallov. 2002. №5. S. 14–17. 11. Kolachev B.A., Polkin I.S., Talalaev V.D. Titanovye splavy raznykh stran [Titanium alloys of the different countries]. M.: VILS, 2000. 318 s.
  11. Novikov I.I. Teoriya termicheskoj obrabotki metallov: uchebnik dlya vuzov. 3-e izd., ispr. i dop. [Theory of thermal processing of metals: the textbook for higher education institutions. 3rd ed., rev. and add.]. M.: Metallurgiya, 1978. 392 s.
  12. Ilin A.A., Kolachev B.A., Nosov V.K., Mamonov A.M. Vodorodnaya tekhnologiya titanovykh splavov / pod obshch. red. A.A. Ilina [Hydrogen technology of titanium alloys / gen. ed. by .A. Ilin]. M: MISiS, 2002. 392 s.
  13. Livanov V.A., Bukhanova A.A., Kolachev B.A. Vodorod v titane [Hydrogen in titanium]. M.: Metallurgiya, 1962. 246 s.
  14. Kolachev B.A. Vodorodnaya khrupkost metallov [Hydrogen embrittlement of metals]. M.: Metallurgiya, 1985. 216 s.
  15. Ilin A.A. Mekhanizm i kinetika fazovykh i strukturnykh prevrashchenij v titanovykh splavakh [The mechanism and kinetics of phase and structural transformations in titanium alloys]. M.: Nauka, 1994. 304 s.
  16. Panin P.V., Manokhin S.S., Dzunovich D.A. Poluchenie i issledovanie submikrokristallicheskoj struktury v titanovykh splavakh pri obratimom legirovanii vodorodom i plasticheskoj deformatsii [Receiving and research of submicrocrystalline structure in titanium alloys at reversible alloying hydrogen and plastic strain] // Voprosy materialovedeniya. 2016. №4 (88). S. 7–17.
  17. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  18. Aviatsionnye materialy: spravochnik v 13 t. 7-e izd., pererab. i dop. / pod obshch. red. E.N. Kablova [Aviation materials: the directory in 13 vol. 7th ed., rev. and add. / gen. ed. by E.N. Kablov]. M.: VIAM, 2010. T. 6: Titanovye splavy. 96 s.
  19. Yakovlev A.L., Filatov A.A., Burkhanova A.A., Popova Yu.A., Nochovnaya N.A Effektivnost primeneniya titanovogo splava VT23 v novykh izdeliyakh «OKB Sukhogo» [Efficiency of application of VT23 titanium alloy in new products of «Sukhoi Design Bureau»] // Titan. 2013. №2 (40). S. 39–42.
  20. Khorev A.I. Kompleksno-legipovannyj titanovyj splav VT23 universalnogo primeneniya [Complex alloyed VT23 titanium alloy of universal application] // Tekhnologiya mashinostpoeniya. 2007. №7. S. 5–11.
  21. Khorev A.I. Titanovyj splav VT23 i ego sravnenie s luchshimi zarubezhnymi splavami [VT23 titanium alloy and its comparison with the best foreign alloys] // Titan. 2006. №1 (18). S. 47–52.
  22. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravochnik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI, 2009. 520 s.
  23. Protsenko O.M., Karachevtsev F.N., Mekhanik E.A. Opyt razrabotki metodiki izmereniya soderzhaniya vodoroda v titanovyh splavah [Experience on development of measurement procedure for determination of hydrogen content in titanium alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 08. Available at: http://www.viam-works.ru (accessed: June 16, 2018). DOI: 10.18577/2307-6046-2014-0-12-8-8.
  24. Kolachev B.A., Betsofen S.Ya., Bunin S.Ya., Volodin V.A. Fiziko-mekhanicheskie svojstva legkikh konstruktsionnykh materialov [Physicomechanical properties of easy constructional materials]. M.: Metallurgiya, 1995. 442 s.
  25. Dzunovich D.A., Panin P.V., Lukina E.A., Shiryaev A.A. Vliyanie rezhimov termicheskoj obrabotki na strukturu i svojstva svarnykh krupnogabaritnykh polufabrikatov iz titanovogo splava VT23 [Heat treatment effect on structure and properties of welded large-dimensioned semi-finished products from VT23 titanium alloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №1 (61). St. 07. Available at: http://www.viam-works.ru (accessed: June 13, 2018). DOI: 10.18577/2307-6046-2018-0-1-7-7.
  26. Ilin A.A., Skvortsova S.V., Popova Yu.A., Kudelina I.M. Vliyanie termicheskoj obrabotki na formirovanie struktury i svojstv krupnogabaritnykh polufabrikatov iz splava VT23 [Influence of thermal processing on forming of structure and properties of large-size semi-finished products from alloy VT23] // Titan. 2010. №4. S. 48–53.
  27. Skvortsova S.V., Popova Yu.A., Panin P.V., Grushin I.A., Kuryshev E.A. Vliyanie termicheskoj obrabotki na strukturu i svojstva svarnykh soedinenij iz titanovogo splava VT23 [Influence of thermal processing on structure and property of welded connections from VT23 titanium alloy] // Titan. 2011. №2. S. 16–21.
  28. Panin P.V., Dzunovich D.A., Alekseev E.B. Sposoby opisaniya fazovogo sostava titanovyh splavov, dopolnitelno legirovannyh vodorodom (obzor) [Ways of phase areas representation in titanium alloys additionally doped with hydrogen (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 03. Available at: http://www.viam-works.ru (accessed: June 13, 2018). DOI: 10.18577/2307-6046-2015-0-3-3-3.
  29. Panin P.V., Shiryaev A.A., Dzunovich D.A. Postroenie temperaturno-kontsentratsionnoj diagrammy fazovogo sostava titanovogo splava VT6, dopolnitelno legirovannogo vodorodom // Tekhnologiya mashinostroeniya. 2014. №3 (141). S. 5–9.
  30. Ilin A.A., Mamonov A.M., Nosov V.K., Majstrov V.M. O vliyanii vodoroda na diffuzionnuyu podvizhnost atomov metallicheskoj podreshetki β-fazy titanovykh splavov [About influence of hydrogen on diffusion mobility of atoms of metal podreshetka β-фазы titanium alloys] // Metally. 1994. №5. S. 99–103.
  31. Ilin A.A., Mikhajlov Yu.V., Nosov V.K., Majstrov V.M. Vliyanie vodoroda na raspredelenie legiruyushchikh elementov mezhdu α- i β-fazami v titanovom splave VT23 [Influence of hydrogen on distribution of doping elements between α-and β-фазами in BT23 titanium alloy] // Fiziko-khimicheskaya mekhanika materialov. 1987. №1. S. 112–114.
  32. Nazimov O.P., Ilin A.A., Kollerov M.Yu. O sostoyanii vodoroda v titane [About condition of hydrogen in titanium] // Zhurnal fizicheskoj khimii. 1980. T. 54. S. 2774–2777.