Features and development trends in the field of heat treatment of magnesium alloys (review)
Mostyaev I.V., Akinina M.V. Features and development trends in the field of heat treatment of magnesium alloys (review) // Proceedings of VIAM. 2018. No. 7. DOI: 10.18577/2307-6046-2018-0-7-41-48. URL: https://www.viam-works.ru/en/journal/2018/7/5
Keywords
magnesium alloys, heat treatment, heat-treatable magnesium alloys, quenching, aging, annealing, homogenization, mechanical properties.
Abstract
The paper presents the review of the technical level and development trends in the field of heat treatment of magnesium alloys is presented. It is shown that new magnesium alloys containing elements from the REE group are being developed, and the foundations of new technologies for their manufacture are being created, while the mechanism of the effect of heat treatment on the structure and strength properties of alloys is widely used. The dependence of the increase in the characteristics of magnesium alloys on the composition of a particular alloy with the application of certain heat treatment regimes is given.
Reference list
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Entsiklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
- Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Yu. Perspektivy primeneniya magnievyh i litejnyh alyuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
- Volkova E.F. Analiz i itogi Mezhdunarodnoj konferencii «Magnij–21. Novye gorizonty» (obzor) [The analysis and results of the International conference «Magnesium–21. Broad horizons» (review)] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 86–94. DOI: 10.18577/2071-9140-2016-0-1-86-94.
- Kablov E.N. Materialy i khimicheskie tekhnologii dlya aviatsionnoj tekhniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
- Volkova E.F., Antipov V.V. Magnievye deformiruemye splavy [Magnesium deformable alloys] // Vse materialy. Entsiklopedicheskij spravochnik. 2012. №5. S. 20‒26.
- Volkova E.F. Sovremennye deformiruemye splavy i kompozitsionnye materialy na osnove magniya [Modern deformable alloys and composite materials on the basis of magnesium] // Metallovedenie i termicheskaya obrabotka metallov. 2006. №11. S. 5–9.
- Kablov E.N. Aviatsionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
- Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dinamika razvitiya magnievyh i litejnyh alyuminievyh splavov [Dynamics of the development of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
- Volkova E.F., Duyunova V.A., Ioda E.N., Panteleev M.D. Osobennosti svarivaemosti novogo deformiruemogo magnievogo splava VMD16 [Features of bondability of new deformable VMD16 magnesium alloy] // Svarochnoe proizvodstvo. 2017. №6. S. 3–11.
- Woo W., Feng Z., Wang X.-L., David S.A. Neutron diffraction measurements of residual stresses in friction stir welding: a review // Sci. Tech. Welding and Joining. 2011. Vol. 16 (1). P. 23–32.
- Woo W., Choo H., Prime M.B. et al. Microstructure, texture, and residual stress in a friction stir processed AZ31B Mg alloy // Acta Materialia. 2008. Vol. 56 (8). P. 1701–1711.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Antonov E.G., Arbuzov B.A., Babkin V.M. i dr. Magnievye splavy: spravochnik [Magnesium alloys: directory]. M.: Metallurgiya, 1978. Ch. 2: Tekhnologiya proizvodstva i svojstva otlivok i deformirovannykh polufabrikatov. S. 208–216.
- Elkin F.M. Deformiruemye magnievye splavy: sovremennoe sostoyanie i perspektivy [Deformable magnesium alloys: current state and perspectives] // Tekhnologiya legkikh splavov. 2009. №3. S. 9–20.
- Yin D.D., Wang Q.D., Gao Y. et al. Effects of heat treatments on microstructure and mechanical properties of Mg–11Y–5Gd–2Zn–0,5Zr (wt. %) alloy // Alloys and Compounds. 2011. Vol. 509. No. 5. P. 1696–1704.
- Process for manufacturing hot-forged parts made of a magnesium alloy: pat. FR2904005 (A1); field: 25.01. 08; publ. 25.03.08.
- Mostyaev I.V. RZE – faktor kachestvennogo povysheniya svojstv magnievyh splavov (obzor) [REE – quality factor increase properties of magnesium alloy (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №7. St. 02. Available at: http://www.viam-works.ru (accessed: June11, 2018). DOI: 10.18577/2307-6046-2015-0-7-2-2.
- Rokhlin L.L., Dobatkina T.V., Nikitina N.I., Tarytina I.E. Issledovanie magnievykh splavov s dvumya redkozemelnymi metallami raznykh podgrupp, tserievoj i ittrievoj [Research of magnesium alloys with two rare earth metals of different subgroups, ceric and yttric] // Institut metallurgii i materialovedeniya im. A.A. Bajkova RAN – 70 let: sb. nauch. tr. M.: Interkontakt Nauka, 2008. S. 304–315.
- Volkova E.F., Rokhlin L.L., Betsofen S.YA., Akinina M.V. Issledovanie vliyaniya RZE ittrievoj i tserievoj podgrupp na svojstva magnievykh splavov [Research of influence of RZE of yttric and ceric subgroups on properties of magnesium alloys] // Tekhnologiya legkikh splavov. 2014. №2. S. 42–48.
- Rokhlin L.L., Dobatkina T.V., Nikitina N.I., Tarytina I.E., Lukyanova E.A. Povedenie pri otzhige vysokoprochnogo magnievogo splava IMV7-1 sistemy Mg–Y–Gd–Zr [Behavior when annealing high-strength IMV7-1 magnesium alloy of Mg-Y-Gd-Zr system] // Perspektivnye materialy. 2011. №6. S. 53–58.
- Jian-Chang Xie, Quan-An Li, Xiao-Qiang Wang, Jian-Hong Li. Microstructure and mechanical properties of AZ81 magnesium alloy with Y and Nd elements // Transactions of Nonferrous Metals Society of China. 2008. Vol. 18. Issue 2. P. 303–308.
- Volkova E.F., Sinebryukhov S.L., Gnedenkov S.V., Betsofen S.Ya. Vliyanie deformatsii i termicheskoj obrabotki na strukturu i svojstva magnievogo splava MA5 [Influence of deformation and thermal processing on structure and properties of MA5 magnesium alloy] // Metallovedenie i termicheskaya obrabotka metallov. 2012. №10. S. 55–59.
- Pekguleryuz M.O. Magnesium alloy development for high-temperature automotive applications // Proceedings of the Second Russian International Conference «Magnesium – Broad Horizons». СПб., 2007 (CD).
- Ovsyannikov B.V., Zamyatin V.M. Vliyanie tekhnologicheskikh faktorov na strukturu i mekhanicheskie svojstva slitkov i polufabrikatov iz magnievykh splavov [Influence of technology factors on structure and mechanical properties of ingots and semi-finished products from magnesium alloys] // Proceedings of the Second Russian International Conference «Magnesium – Broad Horizons» SPb., 2007 (CD).
- Sasaki T.T., Ohkubo T., Hono K. Age Hardening Behavior of Mg–l.2Sn–l.7Zn Alloy Containing Al // Magnesium Technology. P. V: Alloy and Microstructural Design. 2012. P. 179–185.
- Sposob temperaturnoj obrabotki splavov magniya: pat. 2454479 Ros. Federatsiya [Way of temperature processing of alloys of magnesium: pat. 2454479 Rus. Federation]; zayavl. 20.06.11; opubl. 27.06.12.
- Merkulova G.A., Bogdanova T.A., Martynova YA.A. Poisk energosberegayushchej tekhnologii pri podgotovke zagotovok dlya shtampovki detalej iz magnievogo splava sistemy magnij-tsink-tsirkonij [Search of energy saving technology by preparation of preparations for punching of details from magnesium alloy of system magnesium-zinc-zirconium] // Materialy konf. «Nauchno-issledovatelskie problemy v oblasti energetiki i energosberezheniya». 2010. S. 114–116.
- Elkin F.M. Osnovnye puti povysheniya plastichnosti deformiruemykh Mg-splavov [Main ways of increase of plasticity of deformable Mg-alloys] // Proceedings of the First Russian International Conference and Exhibition of «Magnesium – Broad Horizons», November 29– December 12, 2005 (CD).
- Volkova E.F. Analiz sostoyaniya i perspektivy razvitiya deformiruemykh magnievykh splavov [Analysis of condition and perspective of development of deformable magnesium alloys] // Proceedings of the First Russian International Conference and Exhibition of «Magnesium – Broad Horizons», November 29 – December 12, 2005 (CD).