Influence of technological heatings and ways of surface preparation under pasting on mechanical properties of aluminum foil from alloy AMg2N
Antipov V.V., Petrova A.P., Kozlov I.A., Fomina M.A., Volkov I.A. Influence of technological heatings and ways of surface preparation under pasting on mechanical properties of aluminum foil from alloy AMg2N // Proceedings of VIAM. 2018. No. 7. DOI: 10.18577/2307-6046-2018-0-7-10-24. URL: https://www.viam-works.ru/en/journal/2018/7/2
Keywords
aluminum foil, surface preparation, sedimentation titanium oxide, sedimentation of aluminum oxide, MDO-oxidation, chemical oxidation, EP-076
Abstract
Despite keen interest of designers in polymeric composite materials (PСM), aluminum alloys are the base constructional material of the aviation industry. The special attention is given to designs with high specific mechanical properties which treats aluminum cellular fillers. In work will mention question of protection of such materials from corrosion and giving of their surface of special properties with use of different ways of processing (pikling-process, sedimentation titanium oxide, sedimentation of aluminum oxide, MDO (micro-arc oxidation), chemical oxidation). Comprehensive researches of aluminum foil are conducted and the most effective ways of surface preparation are chosen.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
- Kolobova Z.N., Pavlovskaya T.G., Anikhovskaya L.I., Karimova S.A. Razrabotka sposobov podgotovki poverkhnosti pri remonte kleenykh konstruktsij iz alyuminievykh splavov [Development of ways of surface preparation at repair of kleeny designs from aluminum alloys] // Aviacionnye materialy i tehnologii. M.: VIAM, 2002. Vyp.: Remontnye tekhnologii v aviastroenii. S. 73–76.
- Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
- Kablov E.N. Korroziya ili zhizn [Corrosion or life] // Nauka i zhizn. 2012. №11. S. 16–21.
- Anikhovskaya L.I., Pavlovskaya T.G., Dementeva P.A., Petrova A.P. Podgotovka poverkhnosti pod skleivanie [Surface preparation under pasting] // Klei. Germetiki. Tekhnologii. 2008. №7. S. 32–35.
- Pavlovskaya T.G., Volkov I.A., Kozlov I.A., Naprienko S.A. Ekologicheski uluchshennaya tehnologiya obrabotki poverhnosti alyuminievyh splavov [Ecologically improved technology of aluminum alloys surface treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 02 (accessed: June 25, 2018). DOI: 10.18577/2307-6046-2016-0-7-2-2.
- Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Alyuminievye splavy v aviakosmicheskoj tekhnike [Aluminum alloys in aerospace equipment]. M.: Nauka, 2001. 192 s.
- Kulyushina N.V., Kozlov I.A., Kutyrev A.E., Vagramyan T.A. Adhesive coatings on the basis of trialkoxysilanes for aluminum and steel // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 05. Available at: http://viam-works.ru (accessed: June 25, 2018). DOI: 10.18577/2307-6046-2015-0-8-5-5.
- Skopintsev V.D. Oksidirovanie alyuminiya i ego splavov [Oxidation of aluminum and its alloys]. M.: RKhTU im. D.I. Mendeleeva, 2015. 120 s.
- Vojtovich V.A. Sposoby podgotovki poverkhnosti izdelij iz metallov i splavov [Ways of surface preparation of products from metals and alloys] // Klei. Germetiki. Tekhnologii. 2005. №9. S. 19–23.
- Ebnesajjad S. Handbook of adhesives and surface preparation. Technology, Applications and Manufacturing. William Andrew Publishing, 2011. 450 p. DOI: 10.1016/C2010-0-65918-9.
- Ufferman B., Abke T., Barker M. et al. Mechanical properties of joints in 5052 aluminum made with adhesive bonding and mechanical fasteners // International Journal of Adhesion and Adhesives. 2018. Vol. 83. P. 96–102.
- Chuang Gao, Long Li, Xin Chen et al. The effect of surface preparation on the bond strength of Al–St strips in CRB process // Materials & Design. 2016. Vol. 107. P. 205–211.
- Keisuke Nagato, Takumu Yamaguchi, Masayuki Nakao. Anchoring and chemical-bonding effects of anodic alumina microstructure on adhesion strength // CIRP Annals. Available at: http://www.cirp.net (accessed: June 25, 2018).
- Karimova S.A., Kutyrev A.E., Pavlovskaya T.G., Zaharov K.E. Nizkotemperaturnoe uplotnenie anodno-oksidnyh pokrytij na detalyah iz alyuminievyh splavov [Low temperature sealing of anodic oxide coatings on parts of aluminum alloys] // Aviacionnye materialy i tehnologii. 2014. №4. S. 9–17. DOI: 10.18577/2071-9140-2014-0-4-9-17.
- DeMejo L.P., Rimai D.S., Sharpe L.H. Fundamentals of Adhesion and Interfaces. London: Taylor & Francis, 1999. 201 p.
- Kozlov I.A., Pavlovskaya T.G., Zakharov K.E., Volkov I.A. Ekologicheski uluchshennye tekhnologii podgotovki poverkhnosti alyuminievykh splavov [Ecologically improved technologies of surface preparation of aluminum alloys] // Adgezionnye materialy: sb. dokl. nauch.-tekhnich. konf. M.: VIAM. 2016. S. 13 (CD).