Influence of hardener OS-17 on exploiting properties of the varnish covering UR-231
Kuznetsova V.A., Zheleznyak V.G., Baranova N.V., Lebedeva N.N. Influence of hardener OS-17 on exploiting properties of the varnish covering UR-231 // Proceedings of VIAM. 2018. No. 6. DOI: 10.18577/2307-6046-2018-0-6-68-76. URL: https://www.viam-works.ru/en/journal/2018/6/8
Keywords
lacquer coatings, moisture-protective and electro-isolative varnishes, printed-circuit boards, electronics elements, isocyanate hardeners, polyurethane paints.
Abstract
In the study operational properties of coverings on the basis of varnish UR-231 are investigated. Comparison tests of varnish UR-231 with hardeners OS-17 and diethylene glycol urethane (DGU), and also coverings on their basis are carried out. Varnish UR-231 put on samples of alloy D16-AT and samples of printed circuit boards according to specifications 6-21-14–90. Comparing analysis of the received results was carried for the purpose to define possibility of replacement of DGU hardener on hardener OS-17 in interests of reduction of technological process of painting of varnish coatings at the expense of reduction of time of varnish filmforming.
Reference list
- Istoriya aviatsionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshch. red. E.N. Kablova [History of aviation materials science. VIAM is 80: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. S. 319–329.
- Kablov E.N. Materialy i khimicheskie tekhnologii dlya aviatsionnoj tekhniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
- Kablov E.N. Rol khimii v sozdanii materialov novogo pokoleniya dlya slozhnykh tekhnicheskikh system [Chemistry role in creation of materials of new generation for complex technical systems] // XX Mendeleevskij szd po obshchej i prikladnoj khimii: tez. dokl. v 5 t. UrO RAN, 2016. S. 25–26.
- Kablov E.N. Khimiya v aviatsionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij khimicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Kablov E.N. Materialy novogo pokoleniya – osnova innovatsij, tekhnologicheskogo liderstva i natsionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
- Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A., Malova N.E. Razvitie aviatsionnykh lakokrasochnykh materialov [Development of aviation paint and varnish materials] // Vse materialy. Entsiklopedicheskij spravochnik. 2012. №5. S. 49–54.
- Kiping D. Otsenka effektivnosti i stoimosti novykh vidov vlagozashchitnykh pokrytij (iz materialov simpoziuma SMTA Pan Pac, yanvar 2008 g.) [Assessment of efficiency and cost of new types of vlagozashchitny coverings (from materials of symposium of SMTA Pan Pac, January, 2008)] // Tekhnologii v elektronnoj promyshlennosti. 2008. №6. S. 66–71.
- Urazaev V. Vlagozashchitnye polimernye pokrytiya: kakie byvayut [Vlagozashchitnye polymer coatings: which being] // Tekhnologii v elektronnoj promyshlennosti. 2005. №5. S. 52–55.
- Kuznetsova V.A., Semenova L.V., Kondrashov E.K., Lebedeva T.A. Lakokrasochnye materialy s ponizhennym soderzhaniem vrednyh i toksichnyh komponentov dlya okraski agregatov i konstrukcij iz PKM [Paint-and-lacquer materials with a low content of harmful and design of polymer composite materials] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2013. №8. St. 05. Available at: http://www.viam-works.ru (accessed: June 09, 2018).
- Kondrashov E.K., Kuznetsova V.A., Lebedeva T.A., Semenova L.V. Osnovnye napravleniya povysheniya ekspluatatsionnykh, tekhnologicheskikh i ekologicheskikh kharakteristik lakokrasochnykh pokrytij dlya aviatsionnoj tekhniki [The main directions of increase of utilization, technical and ecological properties of paint coatings for aviation engineering] // Rossijskij khimicheskij zhurnal. 2010. T. LIV. №1. S. 96–102.
- Nefyodov N.I., Semyonova L.V. Tendencii razvitiya v oblasti konformnyh pokrytij dlya vlagozashhity i elektroizolyacii plat pechatnogo montazha i jelementov radiojelektronnoj apparatury [Development tendencies in the field on conformal coating for the moisture protection and electrical insulation of printed-circuit boards and electronic elements] // Aviacionnye materialy i tehnologii. 2013. №1. S. 50–52.
- Medgyes B.K., Ripka G. Qualifying methods of conformal coatings used on assembled printed circuit boards Electronics Technology Journal // 30-th International Spring Seminar, 9–13 May. 2007. Budapest Univ. of technol. & Econ. Budapest, 2007. P. 429–433.
- Solntsev S.St., Soloveva G.A., Denisova V.S. Elektroizolyatsionnye emalevye pokrytiya dlya sovremennoj elektronnoj tekhniki [Insulating enamel coatings for modern electronics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №9. St. 08. Available at: http://www.viam-works.ru (accessed: June 09, 2018). DOI: 10.18577/2307-6046-2014-0-9-8-8.
- Nefedov N.I., Salikhov T.R., Melnikov D.A. Issledovanie protsessov otverzhdeniya elektroizolyatsionnykh lakov [Study of the curing processes of electroinsulating varnishes] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №6. St. 09. Available at: http://www.viam-works.ru (accessed: June 09, 2018). DOI: 10.18577/2307-6046-2016-0-6-9-9.
- Papaj Douglas E.A., Mills Sina J., Jamali S. Effect of hardener variation on protective properties of polyurethane coating // Progress in Organic Coatings. 2014. Vol. 77. Part B. P. 2086–2090.
- Avar G., Meier-Westhues U., Casselmann H., Achten D. Polyurethanes // Polymer Science: A Comprehensive Reference. 2012. Vol. 10. P. 411–441.