Influence of the large-scale factor on level of properties of foamed polyacrylimide

Petrova G.N., Perfilova D.N., Malyshenok S.V., Kuznetsova K.R.
Petrova G.N., Perfilova D.N., Malyshenok S.V., Kuznetsova K.R. Influence of the large-scale factor on level of properties of foamed polyacrylimide // Proceedings of VIAM. 2018. No. 6. DOI: 10.18577/2307-6046-2018-0-6-39-47. URL: https://www.viam-works.ru/en/journal/2018/6/5
Keywords
thermoplastics, cellular foam, foamed polyacrylimide, rigid, foaming, dimensions, properties, forecasting.
Abstract

In article results of researches on impact assessment of large-scale factor on level of the physical and mechanical properties rigid foamed polyacrylimide sheet brands VPP-5, made of sheet prepolymer on basis acrylimide are given.

Dependences of values of apparent density, durability are considered at stretching and factors of their variation from overall dimensions foam concrete block. It is established that the factor of variation has values less than 10%, and extent of dispersion of the obtained data is insignificant.

Results of the carried-out work will allow to predict properties of blocks foamed polyacrylimide different dimensions.

Reference list
  1. Kablov E.N., Bejder E.Ya., Petrova G.N., Stolyankov Yu.V., Rumyanceva T.V. Penopoliimidy [Foamed polyimides] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 09. Available at: http://viam-works.ru (accessed: May 17, 2018). DOI: 10.18577/2307-6046-2015-0-4-9-9.
  2. Popov Yu.O., Kolokol’tseva T.V., Khrulkov A.V. Novoe pokolenie materialov i tehnologij dlya izgotovleniya lonzheronov lopastej vertoleta [The new generation of materials and technologies for helicopter blade spars] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 5–9.
  3. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  4. Beider E.Ya., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Thermoplastic composite materials and foam polyimides] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 01. Available at: http://www.viam-works.ru (accessed: May 17, 2018).
  5. Doroshenko N.I., Chursova L.V. Evolyuciya materialov dlya lopastej vertoletov [Evolution of materials for blades of helicopters] // Aviacionnye materialy i tehnologii. 2012. №2. S. 16–18.
  6. Bejder E.Ya., Gureeva E.V., Petrova G.N. Penopoliimidy [Foamed ployimidies] // Vse materialy. Entsiklopedicheskij spravochnik. 2012. №6. S. 2–8.
  7. Poliimidnye kompozitsionnye materialy: struktura, svojstva, tekhnologii / pod obshch. red. A.A. Berlina [Polyimide composite materials: structure, properties, technologies / gen. ed. by A.A. Berlin]. SPb.: Professiya, 2008. 512 s.
  8. Shuldeshov E.M., Kraev I.D., Platonov M.M. Polimernaya kompozicionnaya zvukopogloshhayushhaya panel [Polymeric composition sound absorbing panel] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №5 (53). St. 07. Available at: http://www.viam-works.ru (accessed: May 17, 2018). DOI: 10.18577/2307-6046-2017-0-5-7-7.
  9. Shuldeshov E.M., Kraev I.D., Petrova A.P. Polimernyj zvukopogloshchayushchij material-konstruktsiya dlya snizheniya shuma na mestnosti aviatsionnykh dvigatelej [Polymeric sound-absorbing material design for environmental noise abatement of aircraft engines] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №2 (62). St. 06. Available at: http://www.viam-works.ru (accessed: May 17, 2018). DOI: 10.18577/2307-6046-2018-0-2-6-6.
  10. Shashkeev K.A., Shuldeshov E.M., Popkov O.V., Kraev I.D., Yurkov G.Yu. Poristye zvukopogloshhayushhie materialy (obzor) [Porous sound-absorbing materials (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №6. St. 06. Available at: http://www.viam-works.ru (accessed: May 17, 2018). DOI: 10.18577/2307-6046-2016-0-6-6-6.
  11. PMI – peny s isklyuchitelnymi kharakteristikami [PMI – foams with exclusive characteristics] // Plastiks. 2007. №10. S. 1–2.
  12. Mikhajlin Yu.A. Termoustojchivye polimery i polimernye materialy [Thermo resistance polymers and polymeric materials]. SPb.: Professiya, 2006. 623 s.
  13. Kablov E.N. Sovremennye materialy – osnova innovatsionnoj modernizatsii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  14. Kablov E.N. Khimiya v aviatsionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij khimicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  15. Gryaznov V.I., Petrova G.N., Yurkov G.Yu., Buznik V.M. Smesevye termojelastoplasty so specialnymi svojstvami [Thermoplastic mixtures with special properties] // Aviacionnye materialy i tehnologii. 2014. №1. S. 25–29. DOI: 10.18577/2071-9140-2014-0-1-25-29.
  16. Kravchenko T.P., Ermakov S.N., Kerber M.L., Kostyagina V.A. Nauchno-tekhnicheskie problemy polucheniya kompozitsionnykh materialov na osnove konstruktsionnykh termoplastov [Scientific and technical problems of receiving composite materials on the basis of constructional thermoplastics] // Plasticheskie massy. №10. 2010. S. 32–34
  17. Kerber M.L., Vinogradov V.M., Golovkin G.S. i dr. Polimernye kompozitsionnye materialy: struktura, svojstva, tekhnologiya [Polymeric composite materials: structure, properties, technology]. SPb.: Professiya, 2011. S. 32–33.
  18. Kryzhanovskij V.K., Burlov V.V., Panimatchenko A.D., Kryzhanovskaya YU.V. Tekhnicheskie svojstva polimernykh materialov [Engineering properties of polymeric materials]. SPb.: Professiya, 2005. 240 c.
  19. Petrova G.N., Bejder E.YA., Starostina I.V. Lit'evye termoplasty dlya izdelij aviatsionnoj tekhniki [Molding thermoplastics for products of aviation engineering] // Vse materialy. Entsiklopedicheskij spravochnik. 2016. №6. S. 10–15.
  20. Petrova G.N., Starostina I.V., Rumyantseva T.V, Sapego YU.A. Effektivnost' povysheniya kachestva izdelij iz polikarbonata termoobrabotkoj // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №9. St. 06. URL: http://www.viam-works.ru (data obrashcheniya: 17.05.2018). DOI: 10.18577/2307-6046-2017-0-9-6-6.
  21. Trostyanskaya E.B., Stepanova M.I., Rassokhin G.I. Teplostojkie linejnye polimery. Rostov n/D: RGASKHM, 2002. S. 3–22.
  22. Petrova G.N., Starostina I.V., Rumyanceva T.V., Sapego Yu.A. Effektivnost povysheniya kachestva izdelij iz polikarbonata termoobrabotkoj [Efficiency of improvement of quality of products from polycarbonate heat treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №9 (57). St. 06. Available at: http://www.viam-works.ru (accessed: May 17, 2018). DOI: 10.18577/2307-6046-2017-0-9-6-6.
  23. Berlin A.A., Shutov F.A. Khimiya i tekhnologiya gazonapolnennykh vysokopolimerov [Chemistry and technology of gas-filled high polymers]. M.: Nauka, 1980. 504 s.
  24. Parahin I.V., Tumanov A.S. Fenolokauchukovyj penoplast povyshennoj plastichnosti [Phenolic-rubber foamed plastic of higher plasticity] // Aviacionnye materialy i tehnologii. 2014. №4 (33). C. 65–67. DOI: 10.18577/2071-9140-2014-0-4-65-67.
  25. Parahin I.V., Tumanov A.S. Fenolno-kauchukovyj penoplast marki VRP-4 [Phenolic-rubber foam the grade of VPP-4] // Aviacionnye materialy i tehnologii. 2014. №1 (30). C. 42–46. DOI: 10.18577/2071-9140-2014-0-1-42-46.
  26. Klempner D., Sedzharevich V. Polimernye peny i tekhnologii vspenivaniya [Polymeric foams and technologies of foaming]. SPb.: Professiya, 2009. 604 s.
  27. Krutko E.T., Prokopchuk N.R. Perspektivnye puti sozdaniya novykh termostojkikh materialov na osnove poliimidov [Perspective ways of creation of new heat-resistant materials on the basis of polyimide] // Trudy BGTU. 2013. №4. Khimiya, tekhnologiya organicheskikh veshchestv i biotekhnologii. S. 145–149.
  28. Dobrokhotova M.L. i dr. Poliimidy: spravochnik po plasticheskim massam [Polyimide: directory on plastics]. M.: Khimiya, 1969. S. 317–325.
  29. Kornienko P.V., Gorelov YU.P., Shirshin K.V. Poluchenie i svojstva vspenennykh materialov na osnove sopolimerov akrilonitrila i metakrilovoj kisloty [Receiving and properties of frothed materials on the basis of copolymers acryl nitrile and methacrylic acid] // Zhurnal prikladnoj khimii. 2013. T. 86. №1. S. 96–100.
  30. Kornienko P.V., Gorelov Yu.P., Shirshin K.V. Poluchenie konstruktsionnykh penopolimetakrilimidov na osnove sshitykh sopolimerov akrilonitrila i metakrilovoj kisloty [Receiving constructional penopolimetakrilimidov on the basis of the sewed copolymers acryl nitrile and methacrylic acid] // Zhurnal prikladnoj khimii. 2012. T. 85. №11. S. 1842–1846.
  31. Kornienko P.V., Shirshin K.V. i dr. Poluchenie vspenennykh poliimidnykh materialov na osnove akrilonitrila i metakrilovoj kisloty [Receiving frothed polyimide materials on basis acryl nitrile and methacrylic acid] // Plasticheskie massy. 2013. №6. S. 4–17.
  32. Sorokin A.E., Platonov M.M., Malyshenok S.V. Osobennosti vspenivaniya poliimidnykh smol pri ponizhennom davlenii [Features of foaming of polyimide pitches with reduced pressure] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4. St. 07. Available at: http://www.viam-works.ru (accessed: May 17, 2018). DOI: 10.18577/2307-6046-2017-0-4-7-7.
  33. Davydova I.F., Kavun N.S. Poliimidnyj steklotekstolit s ponizhennoj temperaturoj otverzhdeniya [Polyimide fiberglass plastic with lower curing temperature] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 09. Available at: http://www.viam-works.ru (accessed: May 17, 2018). DOI: 10.18577/2307-6046-2015-0-2-8-8.
  34. Yontz D.J., Hsu S.L. A Mass Spectrometry Analysis of Hard Segment Length Distribution in Polyurethanes // Macromolecules. 2000. Vol. 33. P. 8415–8420.
  35. Velankar S., Cooper S.L. Microphase Separation and Rheological Properties of Polyurethane Melts. 3. Effect of Block Incompatibility on the Viscoelastic Properties // Ibid. I. 395–403.
  36. Artemeva V.N., Kudryavtsev V.V. i dr. Elastichnye penomaterialy na osnove poliimidov [Elastic foam materials on the basis of polyimide] // Plasticheskie massy. 1990. №4. S. 32–34.
  37. Manzer L.E. North American Catalysis Society, Toronto // Chem. and Eng. News. 200m. September 03. P. 39.
  38. Artemeva V.N., Kudryavtsev V.V. Ob osobennostyakh mekhanizma polucheniya poliimidov pri termicheskoj imidizatsii razlichnykh forpolimerov [About features of the mechanism of receiving polyimide at thermal imidization of different prepolymers] // Zhurnal prikladnoj khimii. 2000. T. 73. №4. S. 639–647.
  39. 39 Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  40. Stolyankov Yu.V., Bejder E.Ya., Platonov M.M., Petrova G.N. Ustrojstvo dlya mehanicheskoj obrabotki vspenennyh polimernyh materialov [A device for machining of foamed polymer materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 08. Available at: http://www.viam-works.ru (accessed: May 17, 2018). DOI: 10.18577/2307-6046-2015-0-5-8-8.