Wrought intermetallic titanium ortho alloy doped with yttrium

Part 1. Research on ingot microstructure and rheological curves plotting
Alexeev E.B., Nochovnaya N.A., Novak A.V., Panin P.V.
Alexeev E.B., Nochovnaya N.A., Novak A.V., Panin P.V. Wrought intermetallic titanium ortho alloy doped with yttrium. Part 1. Research on ingot microstructure and rheological curves plotting // Proceedings of VIAM. 2018. No. 6. DOI: 10.18577/2307-6046-2018-0-6-12-21. URL: https://www.viam-works.ru/en/journal/2018/6/2
Keywords
intermetallic titanium alloy, ortho phase Ti2AlNb, rare-earth elements (REE), yttrium, microstructure, deformation treatment, differential scanning calorimetry curves (DSC), rheological curves.
Abstract

The article contains the results of microstructure investigations in the cross section of an ingot from wrought intermetallic titanium ortho alloy doped with yttrium. The effect of heat treatment in a two-phase (b/В2+α2)-area on microstructure of the yttrium doped ortho alloy ingot has been studied. Thermal analysis has been performed with differential scanning calorimetry (DSC) curves plotting which specify phase transformation temperatures of the alloy in focus. Rheological curves for the upset cylindrical samples have been plotted, which revealed deformation strain reduction with upsetting temperature increase from 850 to 1050°C. It has been shown that doping of ortho alloys with rare-earth elements (REE) results in rolling temperature increase.

Reference list
  1. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tekhnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  2. Titanium and Titanium Alloys: Fundamental Applications / ed. by С. Leyens, M. Peters. KGaA, Weinheim: Wiley-VCH Verlag GmbH&Co., 2003. 513 p.
  3. Chen W., Li J.W., Xu L., Lu B. Development of Ti2AlNb Alloys: Opportunities and Challenges // Advanced Materials and Processes. 2014. Vol. 172. No. 5. P. 23–27.
  4. Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  5. Splav na osnove titana i izdelie, vypolnennoe iz nego: pat. 2210612 Ros. Federaciya [Titanium-based alloy and the product which has been executed of it: pat. 2210612 Rus. Federation]; zayavl. 24.09.01; opubl. 20.08.03.
  6. Intermetallidnyj splav na osnove titana: pat. 2405849 Ros. Federaciya [Intermetallic titanium-based alloy: pat. 2405849 Rus. Federation]; zayavl. 28.10.09; opubl. 10.12.10.
  7. Novak A.V., Alekseev E.B., Ivanov V.I., Dzunovich D.A. Izuchenie vliyaniya parametrov zakalki na strukturu i tverdost intermetallidnogo titanovogo orto-splava VTI-4 [The study of the quenching parameters influence on structure and hardness of orthorhombic titanium aluminide alloy VТI-4] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №2. St. 05. Available at: http://www.viam-works.ru (accessed: May 4, 2018). DOI: 10.18577/2307-6046-2018-0-2-5-5.
  8. Alekseev E.B., Nochovnaya N.A., Ivanov V.I., Panin P.V., Novak A.V. Issledovanie vliyaniya alyuminiya na fazovyj sostav i termomekhanicheskij rezhim izotermicheskoj shtampovki intermetallidnogo splava VTI-4 [Research of influence of aluminum on phase structure and thermomechanical mode of isothermal punching of intermetallic alloy VTI-4] // Tekhnologiya legkikh splavov. 2015. №1. S. 57–61.
  9. Zhang S.Z. et al. Phase transformation and microstructure evolution of differently processed Ti–45Al–9Nb–Y alloy // Intermetallics. 2012. Vol. 31. P. 208–216.
  10. Liu Z.G., Chai L.H., Chen Y. Microstructure evolution in rapidly solidified Y added TiAl ribbons // Intermetallic. 2011. Vol. 19. P. 160–164.
  11. Zhao L.L., Li G.Y., Zhang L.Q. Influence of Y addition on the long time oxidation behaviors of high Nb containing TiAl alloys at 900°C // Intermetallics. 2010. Vol. 18. P. 1586–1596.
  12. Chen Y., Si Y., Kong F. Effects of yttrium on microstructures and properties of Ti–17Al–27Nb alloy // Transactions of Nonferrous Metals Society of China. 2006. Vol. 16. Issue 2. P. 316–320.
  13. Li B., Kong F., Chen Y. Effect of yttrium addition on microstructures and room temperature tensile properties of Ti–47 Al alloy // Journal of Rare Earths. 2006. Vol. 24. Issue 3. P. 352–356.
  14. Chen Y., Li B., Kong F. Microstructural refinement and mechanical properties of Y-bearing TiAl alloys // Journal of Alloys and Compounds. 2008. Vol. 457. Issues 1–2. P. 265–269.
  15. Chen Y., Li B., Kong F. Effects of minor yttrium addition on hot deformability of lamellar Ti–45Al–5Nb alloy // Transactions of Nonferrous Metals Society of China. 2007. Vol. 17. P. 58–63.
  16. Si Y., Chen Y., Liu Z., Kong F. Influence of yttrium on microstructure and properties of Ti–23Al–25Nb alloy after heat treatment // Transactions of Nonferrous Metals Society of China. 2006. Vol. 16. P. 849–853.
  17. Chang X., Si J., Gao F., Jing Y., Zhang J. Effect of Gd аddition on heat treatment microstructure of wrought TiAl // Journal of Iron and Steel Research, International. 2007. Vol. 14. P. 26–29.
  18. Lia W., Inksonb B., Horitac Z., Xiaa K. Microstructure observations in rare earth element Gd-modified Ti–44 at% Al // Intermetallics. 2000. Vol. 8. P. 519–523.
  19. Shiriaev A.A., Antashev V.G. Osobennosti razrabotki vysokoprochnogo samozakalivaiushchegosia vysokotekhnologichnogo psevdo-β-titanovogo splava [Peculiarities of development of advanced high-strength self-hardening high-processable pseudo-β-titanium alloys] // Aviatsionnye materialy i tekhnologii. 2014. №4. S. 23–30. DOI: 10.18577/2071-9140-2014-0-4-23-30.
  20. Nochovnaya N.A., Alekseev E.B., Panin P.V., Novak A.V. Issledovanie struktury i mekhanicheskikh svojstv deformiruemogo intermetallidnogo titanovogo splava VIT5, legirovannogo gadoliniem [Research of structure and mechanical properties of the deformable intermetallic VIT5 titanium alloy alloyed by gadolinium] // Titan. 2017. №2. S. 21–29.
  21. Kablov E.N., Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Issledovanie struktury i svojstv zharoprochnykh splavov na osnove alyuminidov titana s mikrodobavkami gadoliniya [Research of structure and properties of hot strength alloys on the basis of titanium aluminides with gadolinium microadditives] // Materialovedenie. 2017. №3. S. 3–10.
  22. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskikh napravlenij razvitiya materialov i tekhnologij ikh pererabotki na period do 2030 goda» // Aviacionnye materialy i tekhnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  23. Antipov V.V. Strategiya razvitiya titanovykh, magnievykh, berillievykh i alyuminievykh splavov // Aviacionnye materialy i tekhnologii. 2012. №S. S. 157–167.
  24. Kablov E.N. Bez novykh materialov – net budushchego // Metallurg. 2013. №12. S. 4–8.
  25. Bazyleva O.A., Arginbaeva E.G., Fesenko T.V., Kolodochkina V.G. Issledovanie vliyaniya likvacionnoj neodnorodnosti na strukturu i dolgovechnost intermetallidnykh splavov na osnove nikelya // Materialy budushchego. 2014. №6. S. 7–12.
  26. Bazyleva O.A., Arginbaeva E.G., Fesenko T.V., Kolodochkina V.G. Study of the effect of liquation on structure and durability of intermetallic alloys based on nickel // Inorganic Materials: Applied Research. 2015. Vol. 6. No. 1. P. 5–10.
  27. Bazyleva O.A., Bondarenko Yu.A., Morozova G.I., Timofeeva O.B. Struktura, khimicheskij i fazovyj sostavy intermetallidnogo splava VKNA-1V posle vysokotemperaturnykh obrabotok i tekhnologicheskikh nagrevov // Zharoprochnye splavy. 2014. №5. S. 3–6.
  28. Povarova K.B., Drozdov A.A., Bazyleva O.A., Bondarenko Yu.A., Bulakhtina M.A., Arginbaeva E.G., Antonova A.V., Morozov A.E., Nefedov D.G. Vliyanie sposobov polucheniya monokristallov splavov na osnove Ni3Al na makro- i mikroodnorodnost raspredeleniya komponentov, strukturu, svojstva // Metally. 2014. №3. S. 40–51.