Influence of diameter of fibers of silicon carbide on mechanical properties of the metal-matrix composite (review)

Grishina O.I., Serpova V.M.
Grishina O.I., Serpova V.M. Influence of diameter of fibers of silicon carbide on mechanical properties of the metal-matrix composite (review) // Proceedings of VIAM. 2018. No. 5. DOI: 10.18577/2307-6046-2018-0-5-55-63. URL: https://www.viam-works.ru/en/journal/2018/5/7
Keywords
metal-matrix composite, titanium-matrix composites, titanium intermetallic, silicon carbide, SiC fiber, mechanical properties.
Abstract

The article is a review of foreign studies in the field of the influence of the diameter of reinforcing fibers of silicon carbide in metal matrix composite based on titanium alloys on mechanical behavior. The article consists of four parts. The introduction refers to the need to create composite materials based on high-temperature titanium alloys reinforced with carbide fibers for the creation of new generation aircraft. Within the framework of the implementation of the complex direction 12 Metal-matrix and poly-matrix composite materials reviewed foreign scientific and technical literature in the field of research, materials for the development of metal composite materials based on titanium alloys, fiber-reinforced refractory compounds of various diameters. At the beginning of the article, a detailed description of two types of silicon carbide fibers and methods for their production is given. The features of the structure and composition of the coating of core fibers considered in

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  3. Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviatsionnoj tekhniki [The main results and the directions of development of materials for perspective aviation engineering] // 75 let. Aviatsionnye materialy. M.: VIAM, 2007. S. 20–26.
  4. Ospennikova O.G. Itogi realizacii strategicheskih napravlenij po sozdaniyu novogo pokoleniya zharoprochnyh litejnyh i deformiruemyh splavov i stalej za 2012–2016 gg. [Implementation results of the strategic directions on creation of new generation of heat-resisting cast and wrought alloys and steels for 2012–2016] // Aviacionnye materialy i tehnologii. 2017. №S. S. 17–23. DOI: 10.18577/2071-9140-2017-0-S-17-23.
  5. Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  6. Grashchenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  7. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. Vysokotemperaturnye metallomatrichnye kompozicionnye materialy, armirovannye chasticami i voloknami tugoplavkih soedinenij [High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds] // Aviacionnye materialy i tehnologii. 2017. №S. S. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  8. Izotova A.YU., Grishina O.I., SHavnev A.A. Kompozitsionnye materialy na osnove titana, armirovannye voloknami (obzor) [Fiber-reinforced titanium based composites (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №5 (53). St. 05. URL: http://www.viam-works.ru (accessed: April 23, 2018). DOI: 10.18577/2307-6046-2017-0-5-5-5.
  9. Grishina O.I., Kochetov V.N., Shavnev A.A., Serpova V.M. Aspecty primeneniya vysokoprochnyh i vysokomodulnyh voloknistyh metallicheskih kompozitsionnyh materialov aviatsionnogo naznacheniya (obzor) [Aspects of application of high-strength and high-modulus fiber metal composite materials for aeronautical purpose (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2014. №10. St. 05. URL: http://www.viam-works.ru (accessed: April 23, 2018). DOI: 10.18577/2307-6046-2014-0-10-5-5.
  10. Silicon Carbide Filaments and Мethod: pat. US 4127659; filed 26.01.77; publ. 28.11.78.
  11. Andreeva A.V. Osnovy fizikokhimii i tekhnologii kompozitov [Bases of the physicchemistry and technology of composites]. M.: Radiotekhnika, 2001. 191 s.
  12. Peters P.W.M. Mono filament reinforced metals (MFRM) in MMC-ASSESS // MMC VIII-Metallic Composites and Foams. (London, UK, November 26–27, 2001). URL: https://www.yumpu.com/en/document/view/37676872/kein-folientitel-the-world-of-mmc-assess-metal-matrix-composites.html (accessed: April 23, 2018).
  13. Budiansky B., Hutchinson J.W., Evans A.G. Matrix fracture in fiber-reinforced ceramic // Journal of the Mechanics and Physics of Solids. 1986. No. 34. P. 167–189.
  14. Curtin W.A. Theory of mechanical properties of ceramic-matrix composite // Journal of the American Ceramic Society. 1991. No. 74. P. 2837–2845.
  15. Shuqi Guo. Fiber size effects on mechanical behaviours of SiC fibres-reinforced Ti3AlC2 matrix composites // Journal of the European Ceramic Society. 2017. Vol. 37. No. 15. P. 5099–5104. DOI: 10.1016/j.jeurceramsoc.2017.07.023.
  16. Bermejo R., Torres Y., Sanchez-Herencia A.J. et al. Residual stresses, strength and toughness of laminates with different layer thickness ratios // Acta materialia. 2006. No. 54. P. 4745–4757.
  17. Juhong Lou, Yanqing Yang, Shenquan Liu. Effect of properties of SiC fibers on longitudinal tensile behavior of SiCf/Ti-6Al-4V composites // Journal of Wuhan University of Technology-Materials Science Edition. 2017. Vol. 32. No. 2. P. 278–283.
  18. Guo S.Q., Hu C.F., Gao H. et al. SiC (SCS-6) fibre-reinforced Ti3AlC2 matrix composites: interfacial characterization and mechanical behavior // Journal of the European Ceramic Society. 2015. No. 35. P. 1375–1384.
  19. John A. McElman. Continuous silicon carbide fibre MMCs // Engineered Materials Handbook. Ohio: ASM International, Metal Park, 1987. Vol. 1: Composites. P. 858–866.