Glue binders and glue prepregs for alumopolymeric composite materials

Antipov V.V., Kotova E.V., Serebrennikova N.Yu., Petrova A.P.
Antipov V.V., Kotova E.V., Serebrennikova N.Yu., Petrova A.P. Glue binders and glue prepregs for alumopolymeric composite materials // Proceedings of VIAM. 2018. No. 5. DOI: 10.18577/2307-6046-2018-0-5-44-54. URL: https://www.viam-works.ru/en/journal/2018/5/6
Keywords
glue binder, glue prepreg, binder content, shear viscosity, glue bond, tensile strength, layered alumopolymeric composite materials, GLARE.
Abstract

Multilayer composite materials of GLARE type with metallic and polymeric layers of GLARE type regarding to sheet constructions for additional weight reduce and resource characteristics increase of aviation parts are shown in this paper. GLARE is a constructive aluminum glassfiber, where a combination of thin aluminum sheets and glue prepregs based on glassfiber provides a unique combination of properties: high strength and crack resistance with low density. It is shown that strength increase in GLARE type materials is provided by new filler material usage. A melt-type VSK-14-2mR glue compound based on a mix of defined structural epoxide olygomers and polyacrylsulfones has a low dynamic viscosity and good viscosity properties and was developed as a glass filler for RVMPN-10-400 roving with increased filament packing density and helps to reach maximum strength of polymeric composite material. Properties of fiberglass with KMKS-1.80.T60.37, KMKS-2.120.T60.37 and KMKS-2mR.120.RVMPN.30 g

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Anikhovskaya L.I., Minakov V.T. Klei i kleevye prepregi dlya perspektivnykh izdelij aviakosmicheskoj tekhniki [Glues and glue prepregs for perspective products of aerospace equipment] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubil. nauch.-tekhnich. sb. M.: MISIS–VIAM, 2002. S. 315–326.
  3. Khrychev Yu.I., Shkodina E.P., Magin N.A. i dr. Razrabotka tekhnologicheskogo processa izgotovleniya radioprozrachnogo obtekatelya iz kleevykh prepregov tipa KMKS-2m.120 [Development of technological process of manufacturing of radio transparent fairing from glue prepregs of the KMKS-2M.120 type] // Klei. Germetiki. Tekhnologii. 2013. №2. S. 27–30.
  4. Krotov A.S., Starcev O.V., Repin A.V. i dr. Sorbciya i diffuziya vlagi v metallopolimernykh sloistykh sistemakh [Sorption and moisture diffusion in metalpolymeric layered systems] // Sb. tr. Mezhdunar. konf. «Sloistye kompozicionnye materialy – 98». Volgograd, 1998. S. 170–171.
  5. Kobec L.P., Deev I.S. Strukturoobrazovanie v termoreaktivnykh svyazuyushchikh i matricakh kompozicionnykh materialov na ikh osnove [Structurization in thermosetting binding and matrixes of composite materials on their basis] // Rossijskij khimicheskij zhurnal. 2010. №1. S. 67–78.
  6. Dementeva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [Adhesive prepregs and layered materials on their basis] // Aviacionnye materialy i tehnologii. 2013. №2. S. 19–21.
  7. Senatorova O.G., Antipov V.V., Lukina N.F., Sidelnikov V.V., Kotova E.V. Vysokoprochnye treshchinostojkie legkie sloistye alyumostekloplastiki klassa SIAL – perspektivnye materialy dlya aviacionnykh konstrukcij [High-strength cracker resistance lungs layered aluminum fiber glasses class SIAL – perspective materials for aviation designs] // Tekhnologiya legkikh splavov. 2010. №1. S. 28–31.
  8. Fridlyander I.N., Anikhovskaya L.I., Senatorova O.G., Sidelnikov V.V. i dr. Kleenye metallicheskie i sloistye metallopolimernye kompozity [Glued metal and layered metalpolymeric composites] // Mashinostroenie: enciklopediya v 40 t. M.: Mashinostroenie, 2001. T. II-3: Cvetnye metally i splavy. Kompozicionnye metallicheskie materialy / pod red. I.N. Fridlyandera, E.N. Kablova i dr. S. 814–832.
  9. Fridlyander I.N., Senatorova O.G., Anikhovskaya L.I., Sidelnikov V.V., Dementeva L.A. Sloistye metallopolimernye kompozity [Layered metalpolymeric composites] // Mashinostroenie: enciklopediya v 40 t. M.: Mashinostroenie, 2001. T. II-3: Cvetnye metally i splavy. Kompozicionnye metallicheskie materialy / pod red. I.N. Fridlyandera, E.N. Kablova i dr. S. 185–195.
  10. Kablov E.N., Antipov V.V., Senatorova O.G., Lukina N.F. Novyj klass sloistykh alyumostekloplastikov na osnove alyuminij-litievogo splava 1441 s ponizhennoj plotnostyu [New class layered aluminum fiber glasses on basis aluminum - lithium alloy 1441 with lowered density] // Vestnik MGTU im. N.E. Baumana. 2011. Special'nyj vypusk: Perspektivnye konstrukcionnye materialy i tekhnologii. S. 174–184.
  11. Kablov E.N., Antipov V.V., Senatorova O.G. Sloistye alyumostekloplastiki SIAL-1441 i sotrudnichestvo s Airbus i Tu Delft [Layered aluminum fiber glasses SIAL-1441 and cooperation with Airbus and Tu Delft] // Cvetnye metally. 2013. №9 (849). S. 50–53.
  12. Kablov E.N., Minakov V.T., Anikhovskaya L.I. Klei i materialy na ikh osnove dlya remonta konstrukcij aviacionnoj tekhniki [Glues and materials on their basis for repair of designs of aviation engineering] // Aviacionnye materialy i tehnologii. 2002. №1. S. 61–65.
  13. Dementeva L.A., Serezhenkov A.A., Lukina N.F., Kutsevich K.E. Svoistva i naznachenie kompozitsionnyh maerialov na osnove kleevyh prepregov [Properties and appointment of composite materials based on adhesive prepregs] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №8. St. 06. Available at: http://www.viam-works.ru (accessed: February 5, 2018). DOI: 10.18577/2307-6046-2014-0-8-6-6.
  14. Dementeva L.A., Serezhenkov A.A., Bocharova L.I., Lukina N.F., Kucevich K.E., Petrova A.P. Svojstva kompozicionnykh materialov na osnove kleevykh prepregov [Properties of composite materials on the basis of glue prepregs] // Klei. Germetiki. Tekhnologii. 2012. №6. S. 19–24.
  15. Lukina N.F., Dement’eva L.A., Serezhenkov A.A., Kotova E.V. et al. Adhesive prepregs and composite materials on their basis // Russian Journal of General Chemistry. 2011. Vol. 81. No. 5. P. 1022–1024.
  16. Serebrennikova N.Yu., Antipov V.V., Senatorova O.G., Erasov V.S., Kashirin V.V. Gibridnye sloistye materialy na baze alyuminij-litievyh splavov primenitelno k panelyam kryla samoleta [Hybrid multilayer materials based on aluminum-lithium alloys applied to panels of plane wing] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 3–8. DOI: 10.18577/2071-9140-2016-0-3-3-8.
  17. Oreshko E.I., Erasov V.S., Podjivotov N.Yu. Vybor shemy raspolozheniya vysokomodulnyh sloev v mnogoslojnoj gibridnoj plastine dlya ee naibolshego soprotivleniya potere ustojchivosti [Arrangement of high-modular layers in a multilayer hybrid plate for its greatest resistance to stability loss] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 109–117. DOI: 10.18577/2071-9140-2014-0-S4-109-117.
  18. Leshchiner L.N., Kishkina S.I., Starova E.N., Fedorenko T.P., Bulgakova E.N. Svojstva neplakirovannykh i plakirovannykh listov iz splava 1441 [Properties of not plated and plated sheets from alloy 1441] // Cvetnye metally. 1994. №4. S. 56–59.
  19. Oreshko E.I., Erasov V.S., Podzhivotov N.Yu., Lutsenko A.N. Raschet na prochnost gibridnoj paneli kryla na baze listov i profilej iz vysokoprochnogo alyuminijlitievogo splava i sloistogo alyumostekloplastika [Strength calculation of hybrid wing panel on the basis of sheets and profiles from high-strength aluminum lithium alloy and laminated aluminum fiberglass] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 53–61. DOI: 10.18577/2071-9140-2016-0-1-53-61.