The investigation of the influence of ageing temperature on structural and phase transformations in VZh177

Shestakova A.A., Karachevtsev F.N., Zhebelev N.M.
Shestakova A.A., Karachevtsev F.N., Zhebelev N.M. The investigation of the influence of ageing temperature on structural and phase transformations in VZh177 // Proceedings of VIAM. 2018. No. 5. DOI: 10.18577/2307-6046-2018-0-5-3-11. URL: https://www.viam-works.ru/en/journal/2018/5/1
Keywords
nickel-base superalloy, microstructure, carbides, heat treatment, ageing.
Abstract

The investigation results of the formation of strengthen phases (secondary carbides and γ'-phase) in new Ni-base superalloy VZh177 developed for jet-engine disk application are presented in the article. The structural and phase composition of the material after solution treatment and the further evolution of the microstructure during ageing were esteemed. The main carbide formation elements in bulk primary carbides were determined via the method of energy-dispersion spectroscopy. The nucleation dynamic of the fine dispersion carbides at grain boundaries was investigated via he method of scanning electron microscopy. The investigation of the strengthen γ'-phase morphology in the temperature range from 850 to 1000°C was presented. The dispersion range of the maximum volume of γ'-phase was established. The changing of mean diameter and morphology of the phase depending to ageing regime was also shown. The authors of the article suggest to investigate microhardness after various ageing tim

Reference list
  1. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  2. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  3. Kablov E.N., Ospennikova O.G., Lomberg B.S. Sozdanie sovremennykh zharoprochnykh materialov i tekhnologij ikh proizvodstva dlya aviatsionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4 S. 34–38.
  4. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya konstruktsionnykh materialov i tekhnologij ikh pererabotki dlya aviatsionnykh dvigatelej nastoyashchego i budushchego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  5. Razuvaev E.I., Bubnov M.V., Bakradze M.M., Sidorov S.A. GIP i deformatsiia granulirovannykh zharoprochnykh nikelevykh splavov [HIP and deformation of the granulated heat resisting nickel alloys] // Aviatsionnye materialy i tekhnologii. 2016. №S1 (43). S. 80–86. DOI: 10.18577/2071-9140-2016-0-S1-80-86.
  6. Locq D., Caron (Onera) P. On Some Advanced Nickel-Based Superalloys for Disk Applications // High Temperature Materials AL03-01. 2011. Issue 3. P. 1–9.
  7. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvyaz struktury i svojstv vysokozharoprochnykh nikelevykh splavov dlya diskov gazoturbinnykh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines] // Aviacionnye materialy i tekhnologii. 2011. №2. S. 25–30.
  8. Gabb T.P., Gayda J., Johnson D.F. et al. Comparison of γ-γ′ Phase Coarsening Responses of Three Powder Metal Disk Superalloys // NASA/TM–2016-218936. February, 2016.
  9. Ovsepyan S.V., Lomberg B.S., Bakradze M.M., Letnikov M.N. Termicheskaya obrabotka deformiruemykh zharoprochnykh nikelevykh splavov dlya diskov GTD [Thermal processing of deformable heat resisting nickel alloys for disks GTE] // Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Mashinostroenie. 2011. № SP2. S. 122–130.
  10. Sims Ch.T., Stoloff N.S., Khagel U.K. Supersplavy II: Zharoprochnye materialy dlya aerokosmicheskikh i promyshlennykh energoustanovok v 2 kn. Per. s angl. / pod red. R.E. Shalina [Superalloys of II: Heat resisting materials for space and industrial power installations in 2 books. Trans from Eng. / ed. by R.E. Shalin]. M: Metallurgiya, 1995. Kn. 1. 384 s.
  11. Zharoprochnyj deformiruemyj splav na osnove nikelya i izdelie, vypolnennoe iz etogo splava: pat. 2280091 Ros. Federatsiya. № 2004137299/02 [Heat resisting deformable alloy on the basis of nickel and the product executed from this alloy: pat. 2280091 Rus. Federation. No. 2004137299/02]; zayavl. 21.12.04; opubl. 20.07.06.
  12. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
  13. Buyakina A.A., Letnikov M.N., Bakradze M.M., Shugaev S.A. Vliyanie termomekhanicheskoj i termicheskoj obrabotki na strukturu i svojstva splava VZH177 [The effect of thermomechanical and heat treatment parameters on structure and mechanical properties of superalloy VZH177] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №10. St. 02. Available at: http://www.viam-works.ru (accessed: April 13, 2018). DOI: 10.18577/2307-6046-2016-0-10-2-2.
  14. Filonova E.V., Bakradze M.M., Kochubey A.Ya., Vavilin N.L. Issledovanie izmenenij strukturno-fazovogo sostoyaniya splava VZh175 v processe goryachej deformacii i termicheskoj obrabotki [Structural-phase evolution of VZH175-alloy during hot deformation and heat treatment] // Aviacionnye materialy i tehnologii. 2014. №3. S. 10–13. DOI: 10.18577/2071-9140-2014-0-3-10-13.
  15. Gaofeng Tian, Jinwen Zou, Yu Wang, Wuxiang Wang. Hot Deformation Behaviors and Microstructure Evolution in a New PM Nickel-Base Superalloy // Advanced Materials Research. 2011. Vol. 278. P. 411–416.
  16. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. Primenenie novyh deformiruemyh nikelevyh splavov dlja perspektivnyh gazoturbinnyh dvigatelej [The application of new wrought nickel alloys for advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.