Heat-reflective coating for protection of expandable structure on against influence of the heat transfer rate

Kozlova A.A., Kondrashov E.K., Barbotko S.L., Vereninova N.P.
Kozlova A.A., Kondrashov E.K., Barbotko S.L., Vereninova N.P. Heat-reflective coating for protection of expandable structure on against influence of the heat transfer rate // Proceedings of VIAM. 2018. No. 4. DOI: 10.18577/2307-6046-2018-0-4-75-83. URL: https://www.viam-works.ru/en/journal/2018/4/9
Keywords
membranous tissue material, heat-reflective coating, thermal impulse, inflatable life designs, enamel, reflection power.
Abstract

Passenger evacuation in the event of a flight accident is often carried out using of inflatable life designs, and in the event of a fire it is important to save the air-tightness and efficiency of the life rafts. In defence of the membranous tissue materials, whereof inflatable life designs are manufacture, heat-reflecting enamel VE-72 is developed from influence of thermal radiation. Research has shown that the heat-reflecting coating of the VE-72 has high technical charac-teristics and also has proved the high efficiency of the heat-reflecting properties of the coating: the duration of the preset overpressure preservation of 20 kPa from exposure of an external heat current of 1,7 W/c2 is 15 minutes even with glue seams, which is 5 times higher than the requirements of the standard TSO-C69c and 3 times higher than the foreign equivalent of art. M-11673 (Air Cruisers Company, USA). Tests of materials on the preservation of leakage under the influence of radiant heat current were carr

Reference list
  1. Kablov E.N. Materialy dlya aviakosmicheskoj tehniki [Materials for aerospace equipment] // Vse materialy. Enciklopedicheskij spravochnik. 2007. №5. S. 7–27.
  2. Technical Standard Order TSO-C69c, Emergency Evacuation Slides, Ramps, Ramp/Slides, And Slide/Rafts. Department of Transportation Federal Aviation Administration Aircraft Certification Service. Washington, DC. 1999. 47 p.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Sposob izgotovleniya ognestojkogo materiala: pat. 2210648 Ros. Federaciya [Way of manufacturing of fire-resistant material: stalemate. 2210648 Rus. Federation]; zayavl. 29.04.02; opubl. 20.08.03.
  5. Aqueous epoxy modified acrylic heat-reflecting thermo-insulating coating: pat. CN1434063; filed. 13.02.03; publ. 06.08.03.
  6. Escape device for aircraft: pat. US5542629; filed. 31.05.94; publ. 06.08.96.
  7. Platonov M.M., Nazarov I.A., Nesterova T.A., Bejder E.Ya. Tkaneplenochnyj material VRT-9 dlya naduvnoj obolochki aviacionnyh spasatelnyh trapov [Membranous tissue material VRT-9 for inflatable shell of rescue ladders] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №5. St. 05. Available at: http://viam-works.ru (accessed: March 22, 2018).
  8. Platonov M.M., Nesterova T.A., Nazarov I.A., Bejder E.Ya. Pozharobezopasnyj material na tekstilnoj osnove s poliuretanovym pokrytiem dlya naduvnoj obolochki spasatelnogo trapa [Fabric-based fireproof material with polyurethane coating for inflatable shell of rescue ladder] // Aviacionnye materialy i tehnologii. 2013. №2. S. 50–54.
  9. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  10. Barbotko S.L. Pozharobezopasnost aviacionnyh materialov [Fire safety of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  11. Barbotko S.L. Razvitie metodov ocenki pozharobezopasnosti materialov aviacionnogo naznacheniya [Development of the fire safety test methods for aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  12. Aircraft Materials Fire Test Handbook: Technical Document DOT/FAA/AR-00/12. U.S. Department of Transportation Federal Aviation Administration. 2000. 235 p.
  13. Marker T.R. Refinement of the Radiant Heat Test for Evacuation Slide Materials // International Aircraft Materials Fire Test Working Group (Savannah, GA, US. March 4, 2014). 2014. 12 p.
  14. Marker T.R. Evacuation Slide Test Method: Comparison Test Results // International Aircraft Materials Fire Test Working Group Meeting (Solothurn, Switzerland. June 25–26, 2014). 2014. 10 p.
  15. Marker T.R. Evacuation Slide Test Method: Comparison of HFG and Power Controller Calibration Methods // International Aircraft Materials Fire Test Working Group (Atlantic City, NJ, US. October 27, 2014). 2014. 12 p.
  16. Marker T.R. Slide Evacuation Test Method: Standardization of power control for electrical furnace // International Aircraft Materials Fire Test Working Group Meeting (February 24, 2015). 2015. 13 p.
  17. Marker T.R. Evacuation SlideTest Method: Round Robin 4 // International Aircraft Materials Fire Test Working Group Meeting (Bremen, Germany. June 3–4, 2015). 2015. 16 p.
  18. Marker T.R. Evacuation Slide Test Method: Standardization of the Power Required for Proper Heat Output of the Furnace; Elimination of the Heat Flux Transducer for Calibration // International Aircraft Materials Fire Test Working Group Meeting (Atlantic City, NJ, US. October 19–20, 2015). 2015. 14 p.
  19. Marker T.R. Evacuation Slide Test Method: Update on Recent Tests // International Aircraft Materials Fire Test Working Group (Bordeaux, France. March 16–17, 2016). 2016. 18 p.
  20. Marker T.R. Development of a New Test Method for Evacuation Slide Materials: Updated to New Test Method // International Aircraft Materials Fire Test Working Group Meeting (Kansas City, MO, US. June 7, 2016). 2016. 13 p.
  21. Marker T.R. Evacuation Slide Materials Test Method: Round Robin 5 // International Aircraft Materials Fire Test Working Group (Mobile, AL. March 7, 2017). 2017. 18 p.
  22. Marker T.R. Evacuation Slide Test Method: Comparison of Radiant Heaters Used for Revised Evacuation Slide Test Method // International Aircraft Materials Fire Test Working Group (Cologne, Germany. June 7–8, 2017). 2017. 13 p.
  23. Do D. Evacuation Slide Test Method: The Revised Test Method used for The Evacuation Slide Test // International Aircraft Materials Fire Test Working Group (Atlantic City, NJ, US. October 30–31, 2017). 2017. 14 p.
  24. Zhelezina G.F., Gulyaev I.N., Soloveva N.A. Aramidnye organoplastiki novogo pokoleniya dlya aviacionnyh konstrukcij [Aramide organic plastics of new generation for aviation designs] // Aviacionnye materialy i tehnologii. 2017. №S. S. 368–378. DOI: 10.18577/2071-9140-2017-0-S-368-378.
  25. Polimernaya teplootrazhayushhaya kompoziciya dlya pokrytiya: pat. 2467042 Ros. Federaciya [Polymeric heatreflecting composition for coating: pat. 2467042 Rus. Federation]; zayavl. 07.06.11; opubl. 20.11.12.