Researching of mechanical properties of deformed semi-finished products of VT23M and VT43 alloys, assessment of their climatic stability in the arctic climate

Putyrskiy S.V., Arislanov A.A., Yakovlev A.L., Nochovnaya N.A.
Putyrskiy S.V., Arislanov A.A., Yakovlev A.L., Nochovnaya N.A. Researching of mechanical properties of deformed semi-finished products of VT23M and VT43 alloys, assessment of their climatic stability in the arctic climate // Proceedings of VIAM. 2018. No. 4. DOI: 10.18577/2307-6046-2018-0-4-101-110. URL: https://www.viam-works.ru/en/journal/2018/4/12
Keywords
high-strength titanium alloys, deformation, climatic tests, mechanical properties, heat treatment, microstructure, Arctic, corrosion.
Abstract

The studies, showed, that the structure of the manufactured semi-finished products from the alloys VT23M and VT43 is typical for deformable semi-finished of (α+β) titanium alloys. It was noted that the average size of structural components of semi-finished products of VT43 alloy is smaller than that of VT23M semi-finished products. Tensile tests to determine the mechanical properties of samples from sheets and bars of VT23M and VT43 alloys were carried out at room temperature (20°C) and lowered (-60°C) temperatures. Since the sheets of the VT43 alloy were first obtained within the framework of this work, in order to evaluate the anisotropy of the mechanical properties, tensile tests at a temperature of +20°C were carried out in the longitudinal and transverse directions of hot rolling. It is shown that under the same production conditions for the of sheets from the investigated alloys, the alloy VT43 has a 9,6% higher strength, with an equal elongation. The comparison is given for th

Reference list
  1. Tarasov Yu.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehkniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  2. Aviacionnye materialy: spravochnik v 13 t. 7-e izd., pererab. i dop. / pod obshh. red. E.N. Kablova [Aviation materials: directory in 13 vol., rev. and add. / gen. ed. by E.N. Kablov]. M.: VIAM, 2010. T. 6: Titanovye splavy. 96 s.
  3. Shiriaev A.A., Antashev V.G. Osobennosti razrabotki vysokoprochnogo samozakaliva-iushchegosia vysokotekhnologichnogo psevdo-β-titanovogo splava [Peculiarities of de-velopment of advanced high-strength self-hardening high-processable pseudo-β-titanium alloys] // Aviatsionnye materialy i tekhnologii. 2014. №4. S. 23–30. DOI: 10.18577/2071-9140-2014-0-4-23-30.
  4. Yakovlev A.L., Filatov A.A., Burhanova A.A., Popova Yu.A., Nochovnaya N.A Effektivnost primeneniya titanovogo splava VT23 v novyh izdeliyah «OKB Suhogo» [Efficiency of application of VT23 titanium alloy in new products of «Sukhoi Design Bureau»] // Titan. №2 (40). 2013. S. 39–42.
  5. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravochnik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI, 2009. 520 s.
  6. Lopatin N.V., Bubnov M.V., Rogalev A.M., Korobova N.V., Sidorov A.A. Izotermicheskaya shtampovka zagotovok diska iz splava EP741-NP, poluchennyh metodami poroshkovoj metallurgii [Isothermal forging of EP741-NP alloy disc billets produced by powder metallurgy methods] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 31–37. DOI: 10.18577/2071-9140-2014-0-S5-31-37.
  7. Hopev A.I. Kompleksno-legipovannyj titanovyj splav VT23 univepsalnogo ppimeneniya [Complex toughened VT23 titanium alloy of universal application] // Tehnologiya mash-inostpoeniya. 2007. №7. S. 5–11.
  8. Hopev A.I. Pazpabotka titanovyh splavov metodom kompleksnogo legipovaniya [De-velopment of titanium alloys by method of complex alloying] // Fiziko-himicheskaya mehanika matepialov. 2006. T. 42. №5. S. 45–50.
  9. Horev A.I. Fundamentalnye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravleniya ih razvitiya [Fundamental and applied works on structural titanium alloys and perspective directions of their development] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 04. Available at: http://www.viam-works.ru (accessed: March 20, 2018).
  10. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Stra-tegicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tehnologii. 2016. №2 (14). S. 16–21.
  12. Erasov V.S., Grinevich A.V., Senik V.Ya., Konovalov V.V., Trunin Yu.P., Nesterenko G.I. Raschetnye znacheniya harakteristik prochnosti aviacionnyh materialov [Calculated values of characteristics of durability of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №2. S. 14–16.
  13. Yakovlev A.L., Nochovnaya N.A., Putyrskij S.V., Krohina V.A. Titanopolimernye sloistye materialy [Titanium-polymer laminated materials] // Aviacionnye materialy i tehnologii. 2016. №S2 (44). S. 56–62. DOI: 10.18577/2071-9140-2016-0-S2-56-62.
  14. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PCM mechanical properties] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  15. Lukina N.F., Dementeva L.A., Serezhenkov A.A. i dr. Kleevye prepregi i kompozicionnye materialy na ih osnove [Glue prepregs and composite materials on their basis] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 53–56.
  16. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  17. Arislanov A.A., Goncharova L.J., Nochovnaya N.А., Goncharov V.A. Perspektivy ispolzovaniya titanovyh splavov v sloistyh kompozicionnyh materialah [Prospects for the use of titanium alloys in laminated composite materials] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 04. Available at: http://www.viam-works.ru (accessed: March 20, 2018). DOI: 10.18577/2307-6046-2015-0-10-4-4.
  18. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.